Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.0022 cm/cm @Time 86400 sec |
0.0022 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP LUBRICOMP OX90351 PPS LNP LUBRICOMP* OX90351 is a compound based on Polyphenylene Sulfide resin containing Proprietary Filler(s). Added feature of this material is: Wear Resistant. |
|||
Linear Mold Shrinkage, Flow | 0.0022 cm/cm @Time 86400 sec |
0.0022 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP THERMOCOMP GF006 PSU LNP THERMOCOMP* GF006 is a compound based on Polysulfone resin containing 30% Glass Fiber. |
|||
Linear Mold Shrinkage, Flow | 0.0022 cm/cm @Time 86400 sec |
0.0022 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP THERMOCOMP GF006XXZ PSU LNP THERMOCOMP* GF006XXZ is a compound based on Polysulfone resin containing 30% Glass Fiber. |
|||
Linear Mold Shrinkage, Flow | 0.0022 cm/cm @Time 86400 sec |
0.0022 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP THERMOCOMP UF0069S PPA LNP THERMOCOMP* UF0069S is a compound based on Polyphthalamide resin containing 30% Glass Fiber. Added features of this material include: Flame Retardant, Heat Stabilized. |
|||
Linear Mold Shrinkage, Flow | 0.0022 cm/cm @Time 86400 sec |
0.0022 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP Thermocomp YF006 TPEE LNP THERMOCOMP* YF006 is a compound based on TPEE resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |