Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.0019 cm/cm @Time 86400 sec |
0.0019 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP STAT-KON DE0029 PC LNP* STAT-KON* DE0029 is a compound based on Polycarbonate resin containing 10% Carbon Fiber. Added features of this material include: Electrically Conductive, Flame Retardant. |
|||
Linear Mold Shrinkage, Flow | 0.0019 cm/cm @Time 86400 sec |
0.0019 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP STAT-KON DE0029 PC (Asia Pacific) LNP* Stat-kon* DE0029 is a compound based on Polycarbonate resin containing Flame Retardant, Carbon Fiber. Added features of this material include: Electrically Conductive, Flame Retardant. |
|||
Linear Mold Shrinkage, Flow | 0.0019 cm/cm @Time 86400 sec |
0.0019 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP STAT-KON DEP42E PC LNP STAT-KON* DEP42E is a compound based on Polycarbonate resin containing 10% Carbon Fiber, 20% PTFE/Silicone. Added features of this material include: Easy Molding. Electrically Conductive, Wear.. |
|||
Linear Mold Shrinkage, Flow | 0.0019 cm/cm @Time 86400 sec |
0.0019 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP STAT-KON DEP42E PC (Asia Pacific) LNP STAT-KON* DEP42E is a compound based on Polycarbonate resin containing Silicone, PTFE, Carbon Fiber. Added features of this material include: Easy Molding. |
|||
Linear Mold Shrinkage, Flow | 0.0019 cm/cm @Time 86400 sec |
0.0019 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP THERMOCOMP DE004ERP PC LNP* Thermocomp* DE004ERP is a compound based on Polycarbonate resin containing 20% Carbon Fiber. Added features include: Electrically Conductive, Easy Molding, Mold Release. |
|||
Linear Mold Shrinkage, Flow | 0.0019 cm/cm @Time 86400 sec |
0.0019 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP THERMOCOMP DE004ERP PC (Asia Pacific) LNP* Thermocomp* DE004ERP is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Electrically Conductive, Easy Molding, Mold Release. |