Physical Properties | Metric | English | Comments |
---|---|---|---|
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond CSA-NF Cyanoacrylate Surface Activator Permabond C Surface Activator (CSA-NF) is used in conjunction with Permabond cyanoacrylate adhesives to promote a faster cure and to extend their gap-filling capabilities. It significantly reduces t.. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond ET500 Epoxy Resin PERMABOND ET500 is a two-part fast-setting epoxy adhesive which bonds to a wide variety of substrates such as wood, metal, ceramics and some plastics and composites. It cures rapidly at room tempera.. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond F202 Anaerobic Retainer The unique 'toughening' process incorporated into Permabond® F202 gives this anaerobic adhesive excellent resistance to peel and impact forces. Primarily designed for use on metal surfaces, it is a.. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond HH167 Anaerobic Retainer Permabond® HH167 is a high viscosity gap filling silver paste, which can be used for repairing metal machinery parts. It is ideal for repairing worn shafts, broken threads, damaged keyways and spli.. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond HL126 Anaerobic Threadlocker PERMABOND® HL126 Threadlocker is a water thin product for locking pre-assembled parts through wicking action. PERMABOND® HL126 Threadlocker prevents vibration loosening. Because of the low viscosi.. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond HM129 Anaerobic Threadlocker Permabond® HM129 is a high strength medium viscosity anaerobic threadlocker and sealant. This material cures in the absence of air between tight fitting metal parts. Cure is fast and reliable on st.. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond HM163 Anaerobic Retainer Permabond® HM163 is a medium viscosity, thixotropic anaerobic retaining compound that cures when confined between metal parts to form a tough bond. It has been specifically formulated to provide a .. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond LH050 Anaerobic Threadsealant Permabond® LH050 pipe sealant with PTFE is a general purpose pipe sealant that provides instant air pressure seal up to 1000 psi with limited hand tightening. After cure, the sealing capability is .. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond LH054 Anaerobic Threadsealant Permabond® LH054 is an anaerobic curing, calibrated strength pipe sealant that allows for easier disassembly – especially of larger diameter pipes. It cures anaerobically when in contact with meta.. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond LH150 Anaerobic Threadsealant Permabond® LH150 Pipe Sealant with PTFE is designed for sealing and locking tapered metal pipe threads and fittings. It is ideal for stainless steel and other passive metals. Instant sealing of up .. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond MH196 Anaerobic Gasketmaker Permabond® MH196 is an anaerobic material designed for making “formed in situ” gaskets between metal surfaces. It is capable of replacing a wide range of conventional gaskets, thereby offering po.. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond POP Polyolefin Primer Permabond® Polyolefin Primer has been developed for surface treatment of polyolefins, PTFE and silicones prior to bonding with Permabond® Cyanoacrylate adhesives. Due to their low surface energy, .. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond TA4590 Toughened Acrylic Adhesive Permabond TA4590 is a structural acrylic adhesive designed primarily for bonding metals, ferrites, ceramics and some thermoplastics. This product was specifically designed to be non-corrosive to sen.. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond TA4820 Structural Acrylic Adhesive PERMABOND TA4820 is a 2-part, 1:1 toughened methacrylate adhesive designed for bonding thermoplastics, thermosets, metals and composites. TA4820 has excellent adhesion to as received metal surfac.. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond UV610 UV-curable Adhesive PERMABOND UV610 is a single part, fast setting, UV curable adhesive designed specifically for bonding glass and metal. Its high strength makes it suitable for a wide range of applications including .. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond UV625 UV-curable Adhesive PERMABOND UV625 is a single part, fast curing, UV curable adhesive primarily designed for bonding and sealing glass and metal. The cured adhesive is tough, flexible and has excellent impact resistan.. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond UV648 UV-curable Adhesive PERMABOND UV648 is a UV-curing adhesive developed for use on plastics. It has good adhesion to acrylic and contains a long-wavelength photo initiator to allow it to cure through UV-stabilized plasti.. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond UV649 UV-curable Adhesive PERMABOND UV649 is a single part, fast setting, and UV curable adhesive designed specifically for bonding plastics. This material has excellent adhesion to a variety of plastics including polycarbon.. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Victrex® Vicote® F804 Polyetheretherketone (PEEK) Liquid Dispersion VICOTE F804 has been specifically formulated to provide a resilient coating with high wear and abrasion resistance on ferrous substrates such as carbon and cast steels. These properties are retained.. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Victrex® Vicote® F807 Black Polyetheretherketone (PEEK) Liquid Dispersion Eco-friendly VICOTE Coatings were developed to fill the performance gap found in many existing coating technologies today. Whether applied to industrial, automotive, food processing, semiconductor, .. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond F201 Anaerobic Retainer Permabond® F201 is an anaerobic adhesive which has been developed to give excellent resistance to peel and impact forces. This toughening, combined with good adhesion to aluminum and copper alloys,.. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond MM115P Pure Anaerobic Threadlocker Permabond® MM115 PURE Threadlocker is an excellent general purpose threadlocker and sealant. It is used for locking metal bolts, nuts and screws that may require disassembly for service and mainten.. |
|||
Storage Temperature | 15.0 - 25.0 °C | 59.0 - 77.0 °F | |
Lubrizol Advanced Materials Pearlbond® DIPP-119 Thermoplastic Polyurethane Pearlbond™ DIPP-119 is polycaprolactone copolyester based thermoplastic polyurethane, supplied in form of translucent pellets. Featuring low melting point and excellent transparency, this produ.. |
|||
Storage Temperature | 0.000 - 25.0 °C | 32.0 - 77.0 °F | |
Akzo Nobel Trigonox® C-C75 Polymerization Initiator Initiator for the (co)polymerization of ethylene, styrene, acrylonitrile, acrylates and methacrylates.Chemical Description: tert-Butyl peroxybenzoate, 75% solution in odorless mineral spiritsCAS Num.. |
|||
Storage Temperature | 10.0 - 25.0 °C | 50.0 - 77.0 °F | |
Akzo Nobel Trigonox® C Polymerization Initiator Initiator for the (co)polymerization of ethylene, styrene, acrylonitrile, vinylacetate, acrylates and methacrylates. Trigonox C is a monofunctional peroxide which is used for the crosslinking of pol.. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond A113 Anaerobic Threadlocker Designed for the locking and sealing of metal parts, Permabond® A113 is ideally suited for use on components that need to be dismantled for maintenance. Giving vibration resistance it can be used .. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond A118 Anaerobic Retainer Permabond® A118 is an anaerobic adhesive designed to provide permanent locking and sealing of metal parts such as bearings, gears, studs and other threaded components. It exhibits high strength, ex.. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond A131 Anaerobic Threadsealant Permabond® A131 is an anaerobic adhesive designed to seal threaded metal pipe connections carrying a wide variety of gases and liquids, including potable water. Suitable for use on both parallel an.. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Permabond A136 Anaerobic Gasketmaker Permabond® A136 is an anaerobic material designed for making 'formed in situ' gaskets between metal surfaces. It is capable of replacing a wide range of conventional gaskets thereby offering potent.. |
|||
Storage Temperature | 5.00 - 25.0 °C | 41.0 - 77.0 °F | |
Victrex® Vicote® F810 Black Polyetheretherketone (PEEK) Liquid Dispersion Eco-friendly VICOTE Coatings were developed to fill the performance gap found in many existing coating technologies today. Whether applied to industrial, automotive, food processing, semiconductor, .. |