Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity Test | 56 cm³/g | 56 cm³/g | Limiting Viscosity Number; ISO 1628-4 |
Mitsubishi Xantar® 25 R Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Viscosity Test | 56 cm³/g | 56 cm³/g | Limiting Viscosity Number; ISO 1628-4 |
Mitsubishi Xantar® 25 SR FD Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Viscosity Test | 56 cm³/g | 56 cm³/g | Limiting Viscosity Number; ISO 1628-4 |
Mitsubishi Xantar® 25 UR Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Viscosity Test | 56 cm³/g | 56 cm³/g | Limiting Viscosity Number; ISO 1628-4 |
Mitsubishi Xantar® F 25 R Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Viscosity Test | 56 cm³/g | 56 cm³/g | Limiting Viscosity Number; ISO 1628-4 |
Mitsubishi Xantar® FC 25 R Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Viscosity Test | 56 cm³/g | 56 cm³/g | Limiting Viscosity Number; ISO 1628-4 |
Mitsubishi Xantar® FC 25 UR Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Viscosity Test | 56 cm³/g | 56 cm³/g | Limiting Viscosity Number; ISO 1628-4 |
Mitsubishi Xantar® G4F 25 R Polycarbonate-20% Glass Reinforced Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Viscosity Test | 56 cm³/g | 56 cm³/g | Limiting Viscosity Number; ISO 1628-4 |
Mitsubishi Xantar® G4F 25 UR Polycarbonate-20% Glass Reinforced Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Viscosity Test | 56 cm³/g | 56 cm³/g | Limiting Viscosity Number; ISO 1628-4 |
Mitsubishi Xantar® MX 1081 Polycarbonate-10% Glass Reinforced Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Viscosity Test | 56 cm³/g | 56 cm³/g | Limiting Viscosity Number; ISO 1628-4 |
Mitsubishi Xantar® F 25 UR Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Viscosity Test | 56 cm³/g | 56 cm³/g | Limiting Viscosity Number; ISO 1628-4 |
Mitsubishi Xantar® MX 1082 Polycarbonate-20% Glass Reinforced Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Viscosity Test | 56 cm³/g | 56 cm³/g | Viscosity number |
BASF Ultrason E 2010 G4 20% Glass Filled PES Ultrason E 2010 G4 is a 20% glass reinforced, medium viscosity injection molding PES grade with high rigidity and strength. |
|||
Viscosity Test | 56 cm³/g | 56 cm³/g | Viscosity number |
BASF Ultrason E 2010 G6 30% Glass Filled PES Ultrason E 2010 G6 is a 30% glass reinforced, medium viscosity injection molding PES grade with high rigidity and strength. |
|||
Viscosity Test | 56 cm³/g | 56 cm³/g | Viscosity number |
BASF Ultrason E 2010 PES Ultrason E 2010 is an unreinforced, medium viscosity standard injection molding PES grade. It flows readily and offers outstanding heat resistance and dimensional stability. It conforms to FDA req.. |
|||
Viscosity Test | 56 cm³/g | 56 cm³/g | Viscosity number |
BASF Ultrason E 2020 P PES Ultrason E 2020 P is an unfilled, injection molding PES grade. Polyethersulfone flakes, for solvent based processes; product is soluble e.g. in N-Methylpyrrolidone and N,N-Dimethylacetamide. |