Physical Properties | Metric | English | Comments |
---|---|---|---|
High Load Melt Index | 30 g/10 min @Load 21.6 kg, Temperature 190 °C |
30 g/10 min @Load 47.6 lb, Temperature 374 °F |
High Load Melt Index; ASTM D 1238 |
Chevron Phillips HiD® 9606 HDPE Blown Film and Sheet
(discontinued **) Resin Type: ASTM D 4976 Classification: PE 235, A 54502Applications:General Purpose Films and Sheet, Coextruded Film Structures, Deli and Tissue Films, Sheet Thermoforming Applications with Good Str.. |
|||
High Load Melt Index | 30 g/10 min | 30 g/10 min | ASTM D1238 |
Ineos K44-24-122 HDPE K44-24-122 is a high density polyethylene copolymer designed specifically for pipe coating and extrusion. It complies with the virgin polyethylene resin requirements in CZA Z245-21.Natural resin; s.. |
|||
High Load Melt Index | 30 g/10 min @Load 21.6 kg |
30 g/10 min @Load 47.6 lb |
ASTM D 1238 |
Total 5202 HDPE, blow molding Applications: Bleach and detergents, industrial chemicals, industrial parts, packaging aggressive liquids, food packaging. Blow molding stock temperature 360 - 400°F Extrusion melt temperature 380 .. |
|||
High Load Melt Index | 30 g/10 min @Load 21.6 kg |
30 g/10 min @Load 47.6 lb |
ASTM D 1238 |
Total 5202LD HDPE, blow molding Applications: Bleach and detergents, industrial chemicals, industrial parts, packaging aggressive liquids, food packaging. Blow molding stock temperature 360 - 400°F Extrusion melt temperature 380 .. |
|||
High Load Melt Index | 30 g/10 min @Load 21.6 kg |
30 g/10 min @Load 47.6 lb |
ASTM D 1238 |
Total 5502 BZ HDPE injection blow molding Applications: Cosmetics and toiletries, pharmaceuticals, specialty containers, food packagingInformation provided provided by Total Petrochemicals.Total Petrochemicals acquired former Fina and Atof.. |
|||
High Load Melt Index | 30 g/10 min @Load 21.6 kg, Temperature 190 °C |
30 g/10 min @Load 47.6 lb, Temperature 374 °F |
ASTM D 1238 |
Total 5502 HDPE, blow molding, pipe Drug Master File listed; USP Class VI approved; FDA compliant; UL 94HB/746 certified |
|||
High Load Melt Index | 30 g/10 min @Load 21.6 kg, Temperature 190 °C |
30 g/10 min @Load 47.6 lb, Temperature 374 °F |
ASTM D1238 |
Total Lumicene® mPE M 3410 EP HDPE Film Outstanding clarity and gloss; excellent bubble stability; excellent tear strength; high puncture resistance; good stiffness; excellent heat sealing properties; excellent compatibility with LDPE and.. |
|||
High Load Melt Index | 30 g/10 min @Load 21.6 kg, Temperature 190 °C |
30 g/10 min @Load 47.6 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil HD 7845.30 MMW Blown Film Resin Product Description: HD 7845.30 can be processed on high stalk, pocket extrusion or cast lines. Films made from HD 7845.30 exhibit an excellent stiffness balance. High thermal stability provides exc.. |
|||
High Load Melt Index | 30 g/10 min @Load 21.6 kg, Temperature 190 °C |
30 g/10 min @Load 47.6 lb, Temperature 374 °F |
ASTM D1238 |
Dow FLEXOMER™ DFDA-1098 NT Very Low Density Polyethylene (VLDPE) Resin FLEXOMER™ DFDA-1098 NT is an ethylene-butene copolymer with a unique olefinic composition for improved process-ability and material handling. This product is produced via gas phase polymerization .. |
|||
High Load Melt Index | 30 g/10 min @Load 21.6 kg, Temperature 190 °C |
30 g/10 min @Load 47.6 lb, Temperature 374 °F |
ASTM D1238 |
Dow UNIVAL™ DMDF-6200 NT 7 High Density Polyethylene Resin (HDPE) Excellent extrusion characteristics Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a UNIVAL™ DMDF-6200 NT 7 is specifically designed for use in either intermittent or continuous blow molding equipme.. |
|||
High Load Melt Index | 30 g/10 min @Load 21.6 kg, Temperature 250 °C |
30 g/10 min @Load 47.6 lb, Temperature 482 °F |
|
BASF Luranyl® KR 2402 Polyphenylene Ether + Styrene-Butadiene Blend, Impact Grade Base grade with a balanced combination of impact strength and stiffness for parts calling for good heat deformation resistance (e.g. warm-air vents, coil formers, sheet and wheel covers).Data was co.. |