Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Total 5202LD HDPE, blow molding

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Blow Molding Grade
Manufacturer Total Atofina
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total 5202LD HDPE, blow molding.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Applications: Bleach and detergents, industrial chemicals, industrial parts, packaging aggressive liquids, food packaging. Blow molding stock temperature 360 - 400°F Extrusion melt temperature 380 - 420°FInformation provided provided by Total Petrochemicals.Total Petrochemicals acquired former Fina and Atofina plastics product lines.
Physical Properties Metric English Comments
Density 0.952 g/cc
0.0344 lb/in³
ASTM D 792
Environmental Stress Crack Resistance 50 hour
50 hour
ASTM D1693 cond. B 10% lgepal
100 hour
100 hour
ASTM D1693 cond. B 100% lgepal
Melt Flow 0.35 g/10 min

@Load 2.16 kg
0.35 g/10 min

@Load 4.76 lb
ASTM D 1238
High Load Melt Index 30 g/10 min

@Load 21.6 kg
30 g/10 min

@Load 47.6 lb
ASTM D 1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield >= 26.9 MPa
>= 3900 psi
ASTM D 638 type IV
Elongation at Break 600 %
600 %
ASTM D 638, type IV
Flexural Modulus 1.31 GPa
190 ksi
ASTM D 790
Thermal Properties Metric English Comments
Melting Point 128 °C
263 °F
ASTM D3417