Physical Properties | Metric | English | Comments |
---|---|---|---|
High Load Melt Index | 10 g/10 min @Load 21.6 kg, Temperature 240 °C |
10 g/10 min @Load 47.6 lb, Temperature 464 °F |
ISO 1133 |
Premix Thermoplastics PRE-ELEC® PPE 1461
(discontinued **) PRE-ELEC PPE 1461 is a conductive thermoplastic compound based on modified polyphenylene ether (PPE). Conductivity is achieved by using special conductive carbon black. In addition to a low electric.. |
|||
High Load Melt Index | 10 g/10 min @Load 21.6 kg, Temperature 190 °C |
10 g/10 min @Load 47.6 lb, Temperature 374 °F |
High Load; ASTM D1238 |
Chevron Phillips Marlex® HHM TR-480Z/M362 Natural high density ethylene hexene copolymer/black concrete
(disc Benefits: good long term hoop strength performance, very high melt strength, outstanding toughness even at low temperatures, concrete base resinCharacteristics: Pipe Ring ESCR > 2000 h, ASTM F 1248;.. |
|||
High Load Melt Index | 10 g/10 min @Load 21.6 kg, Temperature 190 °C |
10 g/10 min @Load 47.6 lb, Temperature 374 °F |
Condition F; ASTM D1238 |
Formosa Plastics Formolene® HL5010 Sheet and Thermoforming HDPE
(discontinued **) Extra High Molecular Weight Hexene Copolymer Formolene® HL5010 has good melt strength, excellent stress crack resistance, good rigidity, and excellent impact strength even at low temperatures. Thes.. |
|||
High Load Melt Index | 10 g/10 min | 10 g/10 min | ASTM D1238 |
Ineos G36-10-150 HDPE G36-10-150 is a medium density hexene copolymer polyethylene resin designed for the blown geomembrane sheet process. This resin is especially well suited for the production of textured geomembranes... |
|||
High Load Melt Index | 10 g/10 min | 10 g/10 min | ASTM D1238 |
Ineos G50-100 HDPE Ineos G50-100 is a high molecular weight, high density polyethylene copolymer developed for sheet extrusion, thermoforming and large part blowmolding where the finished product demands outstanding p.. |
|||
High Load Melt Index | 10 - 14 g/10 min @Load 21.6 kg, Temperature 190 °C |
10 - 14 g/10 min @Load 47.6 lb, Temperature 374 °F |
ASTM D1238-00 |
Ipiranga Petrochem GM 8260 HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |
|||
High Load Melt Index | 10 g/10 min @Load 21.6 kg |
10 g/10 min @Load 47.6 lb |
at listed melt temp |
Lubrizol Advanced Materials Pearlthane® Clear 15N70 Polyether based TPU PEARLTHANE® CLEAR 15N70 is a polyether copolymer-based TPU with Shore 72 A hardness, free of plasticizer, supplied in form of translucent, colorless pellets with very low yellowness index. PEARLT.. |
|||
High Load Melt Index | 10 g/10 min @Load 21.6 kg, Temperature 190 °C |
10 g/10 min @Load 47.6 lb, Temperature 374 °F |
ISO 1133 |
Borealis BorPEX™ HE1878E High Density Polyethylene Powder for Crosslinked Pipes BorPEX HE1878E is a high molecular weight, high density polyethylene powder specially designed for production of peroxide crosslinked pipes (PEX pipes).Crosslinked (PEX) pipes based on BorPEX HE1878.. |
|||
High Load Melt Index | 10 g/10 min @Load 21.6 kg, Temperature 190 °C |
10 g/10 min @Load 47.6 lb, Temperature 374 °F |
ISO 1133 |
Borealis BorPEX™ ME2592 Medium Density Polyethylene Compound for Crosslinked Pipes (Pex-C (Irradiation)) BorPEXME2592 is a natural, high molecular weight, medium density polyethylene for crosslinkable pipes with excellent flexibility. The compound is especially designed for electron beam irradiation c.. |
|||
High Load Melt Index | 10 g/10 min @Load 21.6 kg |
10 g/10 min @Load 47.6 lb |
ASTM D 1238 |
Total 2287 HDPE Bimodal Film Resin Broad molecular weight distribution. Designed for die build-up sensitive equipmentApplications: T-shirt sacks, trash can liners, merchandise bags, deli wrapInformation provided provided by Total Pe.. |
|||
High Load Melt Index | 10 g/10 min @Load 21.6 kg |
10 g/10 min @Load 47.6 lb |
ISO 1133 |
Total HP 401 MDPE, pipe, cable, sheet FINATHENE® HP 401 is a polyethylene copolymer based on C6 hexene as co-monomer and is produced by a continuous low-pressure slurry polymerization process. FINATHENE® HP 401 is a black high densit.. |
|||
High Load Melt Index | 10 g/10 min @Load 21.6 kg, Temperature 190 °C |
10 g/10 min @Load 47.6 lb, Temperature 374 °F |
ASTM D1238 |
Chevron Phillips Marlex® HXM 50100 Extra high molecular weight hexene copolymer Benefits: excellent balance of stress cracking resistance, good melt strength, excellent stress cracking resistance, good rigidity, excellent impact strength even at low temperaturesApplications: 55.. |
|||
High Load Melt Index | 10 g/10 min @Load 21.6 kg |
10 g/10 min @Load 47.6 lb |
ASTM D1238 |
Equate EGDA-6888 HDPE Film Extrusion Resin EGDA-6888 is a high molecular weight, high density polyethylene copolymer that has been designed specifically for tubular film extrusion. Its broad molecular weight distribution and density have bee.. |
|||
High Load Melt Index | 10 g/10 min @Load 21.0 kg |
10 g/10 min @Load 46.3 lb |
ASTM D1238 |
Equate EPDA-5040 HDPE Non-Pressure Gravity Pipe Resin EPDA-5040 is a high molecular weight high density polyethylene copolymer resin designed for non-pressure gravity pipe applications. It has a good balance of flexibility, ductility, stiffness and tou.. |
|||
High Load Melt Index | 10 g/10 min @Load 21.6 kg, Temperature 190 °C |
10 g/10 min @Load 47.6 lb, Temperature 374 °F |
ASTM D1238 |
Dow UNIVAL™ DMDA-6147 NT 7 High Density Polyethylene Resin (HDPE) Good extrudability/processability Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a UNIVAL™ DMDA-6147 NT 7 is a polymer with broad molecular weight distribution and high molecular weight. This produ.. |
|||
High Load Melt Index | 10 g/10 min @Load 21.6 kg, Temperature 190 °C |
10 g/10 min @Load 47.6 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil HD 7960.13 HMW Blown Film Resin Product Description: HD 7960.13 is a high molecular weight HDPE blown film resin. Films made from HD 7960.13 exhibit excellent impact and toughness properties, as well as high stiffness. HD 7960.13 .. |
|||
High Load Melt Index | 10 g/10 min @Load 21.6 kg, Temperature 190 °C |
10 g/10 min @Load 47.6 lb, Temperature 374 °F |
ASTM D1238 |
Dow UNIPOL™ DGDA-5110 Polyolefin DGDA-5110 UNIPOL™ is designed for the manufacture of thermoformed truck liners and other sheet extrusion applications requiring toughness and good process-ability. Information provided by Dow |
|||
High Load Melt Index | 10 g/10 min @Load 21.6 kg, Temperature 190 °C |
10 g/10 min @Load 47.6 lb, Temperature 374 °F |
ASTM D1238 |
Braskem HF 0150 HDPE Blown Film Extrusion Polyethylene 38µm film gauge, obtained in 75mm extruder, die gap 1.0mm, output 1.75 kg/h-cm with 2:1 BUR. Applications: Grocery and T-shirt bags; merchandise bags; frozen-food bags. Information provided by Bras.. |
|||
High Load Melt Index | 10 g/10 min @Load 21.6 kg, Temperature 190 °C |
10 g/10 min @Load 47.6 lb, Temperature 374 °F |
ISO 1133 |
Borealis BorPEX™ HE2591 High Density Polyethylene Powder for Crosslinked Pipes (Pex-C (Irradiation)) BorPEX HE2591 is a high molecular weight, high density polyethylene powder for crosslinkable pipes, offering excellent processability for peroxide crosslinking. It is a special polymer, stabilized .. |
|||
High Load Melt Index | 10 g/10 min @Load 21.6 kg, Temperature 190 °C |
10 g/10 min @Load 47.6 lb, Temperature 374 °F |
ASTM D1238 |
Formosa Plastics Formolene® HL5010 Blow Molding HDPE Extra High Molecular Weight Hexene CopolymerApplications: Blow Molded 55-gallon shipping containers, gasoline tanks, agricultural chemical tanks; Extruded pallets, cattle feeders, large formed parts.. |
|||
High Load Melt Index | 10 g/10 min @Load 21.6 kg |
10 g/10 min @Load 47.6 lb |
ASTM D 1238 |
Total Finathene® CD 481 HDPE conduit