Ineos G50-100 HDPE

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE
Manufacturer Ineos Olefins & Polymers USA
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ineos G50-100 HDPE.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Ineos G50-100 is a high molecular weight, high density polyethylene copolymer developed for sheet extrusion, thermoforming and large part blowmolding where the finished product demands outstanding physical performance. This material meets the Food and Drug Administration requirements of 21CFR 177.1520.
Physical Properties Metric English Comments
Density 0.950 g/cc
0.0343 lb/in³
ASTM D4883
High Load Melt Index 10 g/10 min
10 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 65
65
ASTM D2240
Tensile Strength at Break 30.3 MPa
4400 psi
2 in/min.; ASTM D638
Tensile Strength, Yield 26.2 MPa
3800 psi
2 in/min (50 mm/min); ASTM D-638
Elongation at Break >= 800 %
>= 800 %
2 in/min (50 mm/min); ASTM D-638
Modulus of Elasticity 0.931 GPa
135 ksi
ASTM D638
Flexural Modulus 1.205 GPa
174.8 ksi
Tangent-Method 1; ASTM D790
Tensile Impact Strength 525 kJ/m²
250 ft-lb/in²
Type L, ASTM D1822
Thermal Properties Metric English Comments
CTE, linear 120 µm/m-°C

@Temperature 20.0 °C
66.7 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 70.0 °C
158 °F
ASTM D648
Vicat Softening Point 130 °C
266 °F
ASTM D1525
Brittleness Temperature <= -75.0 °C
<= -103 °F
ASTM D746
Descriptive Properties Value Comments
Process Blow Molding
Sheet Extrusion
Region US & Canada
Bamberger Polymers Distribution