Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | <= 500 cP | <= 500 cP | #2/20 rpm |
Mallard Creek Polymers ROVENE® 4049 SBR Latex ROVENE® 4049 is a carboxylated styrene-butadiene emulsion that has a medium hand with above average strength properties. This binder has the ability to be cross-linked with external cross-linking.. |
|||
Brookfield Viscosity | <= 500 cP | <= 500 cP | #20/200 |
Mallard Creek Polymers Rovene® 6065 Styrene-Acrylic Emulsion Applications: Rovene® 6065 is a tough, durable nonwoven binder intended to provide improved stiffness and strength. Rovene® 6065 was specifically designed to perform in formaldehyde-free syste.. |
|||
Brookfield Viscosity | 500 - 1800 cP | 500 - 1800 cP | #2/20 rpm |
Mallard Creek Polymers ROVENE® 6101 Styrene-Acrylic Emulsion ROVENE® 6101 is a stiff, non-film forming high-gloss extending vehicle for flexographic and gravure inks and overprint varnishes. It is intended for use primarily on paper and paperboard.APPLICAT.. |
|||
Brookfield Viscosity | <= 500 cP | <= 500 cP | #20/200 |
Mallard Creek Polymers Rovene® 6126 Styrene-Acrylic Emulsion Applications: Rovene® 6126 provides a flexible yet strong cohesive bond for a range of materials and particle surface areas. Rovene® 6126 imparts films with good water resistance properties. F.. |
|||
Brookfield Viscosity | <= 500 cP | <= 500 cP | #2/20 rpm |
Mallard Creek Polymers ROVENE® 8305 SBR Emulsion ROVENE® 8305 is a 50% bound styrene, high gel content hot polymerized styrene – butadiene emulsion. Compatibility with commercial tackifier resin emulsions is excellent, as is filler toleran.. |
|||
Brookfield Viscosity | <= 500 cP | <= 500 cP | #2/20 rpm |
Mallard Creek Polymers ROVENE® 97982 Acrylic Emulsion ROVENE® 97982 is a very soft acrylic latex emulsion suggested as a base resin in flexible packaging laminating adhesives. Rovene® 97982 provides formulations with excellent clarity and UV stab.. |
|||
Brookfield Viscosity | 500 - 1700 cP | 500 - 1700 cP | Spindle # 3, rpm 60 |
Michelman® Hydrosize® U2-01 Nonionic polyurethane emulsion Description: Nonionic polyurethane emulsionUsage: Hydrosize® U2-01 is a high strength sizing for glass and carbon chopped fiber with excellent adhesion.Information provided by Michelman® |
|||
Brookfield Viscosity | 500 - 1700 cP | 500 - 1700 cP | Spindle # 3, rpm 60 |
Michelman® Hydrosize® U2022 Nonionic polyurethane emulsion Description: Nonionic polyurethane emulsionUsage: Hydrosize® U2022 is an APE free, high strength sizing for glass and carbon chopped fiber, with excellent adhesion.Information provided by Michelm.. |
|||
Brookfield Viscosity | <= 500 cP | <= 500 cP | Spindle # 2, rpm 60 |
Michelman® Michem® Emulsion 27720 Nonionic slip and anti-block additive Description: Nonionic slip and anti-block additiveUsage: Michem® Emulsion 27720 is a nonionic, amide emulsion used for anti-blocking, slip and mar resistant properties.We serve many markets throu.. |
|||
Brookfield Viscosity | <= 500 cP | <= 500 cP | Spindle # 3, rpm 60 |
Michelman® Michem® Emulsion 48625M1 Polymer solution Description: Polymer solutionUsage: Michem® Emulsion 48625M1 is a sizing polymer for fiberglass and other fibers serving as reinforcement for various resins.We serve many markets through MichemÂ.. |
|||
Brookfield Viscosity | <= 500 cP | <= 500 cP | Spindle # 2, rpm 60 |
Michelman® Michem® Emulsion 65140 Nonionic polypropylene emulsion Description: Nonionic polypropylene emulsionUsage: Michem® Emulsion 65140 is best used as an additive in floor polish and overprint varnish formulations when a high degree of slip resistance is n.. |
|||
Brookfield Viscosity | <= 500 cP | <= 500 cP | Spindle # 2, rpm 60 |
Michelman® Michem® Emulsion 70350 Cationic paraffin emulsion Description: Cationic paraffin emulsionUsage: Michem® Emulsion 70350 is designed to be a water repellent additive. This product is effectively used for the curing and protection of concrete.We se.. |
|||
Brookfield Viscosity | <= 500 cP | <= 500 cP | Spindle # 3, rpm 60 |
Michelman® Michem® Flex P1801 Water based primer Description: Water based primer for liquids and extrusion coated resins.Usage: Michem®Flex P1801 is a primer for film and paper substrates to promote adhesion to extrusion coated resins resulting.. |
|||
Brookfield Viscosity | <= 500 cP | <= 500 cP | Spindle # 2, rpm 60 |
Michelman® Michem® Guard 1350 Nonionic emulsion of polyethylene wax Description: Nonionic emulsion of polyethylene waxUsage: Michem® Guard 1350 is a water based one micron dispersion which improves rub and abrasion resistance in pigmented coatings and semi-gloss .. |
|||
Brookfield Viscosity | 500 - 1000 cP | 500 - 1000 cP | Spindle # 3, rpm 60 |
Michelman® Michem® Guard 350 Nonionic, Fischer-Tropsch dispersion Description: Nonionic, Fischer-Tropsch dispersionUsage: Michem® Guard 350 is designed to impart abrasion resistance, rub resistance and matting properties to aqueous paints, coatings and inksTypi.. |
|||
Brookfield Viscosity | 500 - 5000 cP | 500 - 5000 cP | Spindle # 4, rpm 60 |
Michelman® Michem® Guard 55 Nonionic polyethylene dispersion Description: Nonionic polyethylene dispersionUsage: Michem® Guard 55 is a dispersion which provides mar and flatting properties when used as an additive in paint, coating, ink and graphic art for.. |
|||
Brookfield Viscosity | <= 500 cP | <= 500 cP | Spindle # 3, rpm 60 |
Michelman® Michem® Guard 7140 Anionic dispersion of polyethylene wax Description: Anionic dispersion of polyethylene waxUsage: Michem® Guard 7140 is a water-based, large particle emulsion which improves rub and abrasion resistance in pigmented coatings and semi-gl.. |
|||
Brookfield Viscosity | <= 500 cP | <= 500 cP | Spindle # 2, rpm 60 |
Michelman® Michem® Wood Coating 70M Anionic paraffin blend emulsion Description: Anionic paraffin blend emulsionUsage: Michem® Wood Coating 70M is a high solids, water resistant topical wood treatment for exterior wood and wood composites. It provides good water .. |
|||
Brookfield Viscosity | 500 - 1600 cP | 500 - 1600 cP | Spindle # 3, rpm 60 |
Michelman® Resisto Coat™ 39AF Abrasion resistance coating Description: Abrasion resistance coatingUsage: Resisto Coat™ 39AF provides excellent, economical abrasion protection. It is used throughout the appliance industry as a protective finish on corn.. |
|||
Brookfield Viscosity | 500 cP @Temperature 25.0 °C |
500 cP @Temperature 77.0 °F |
20 RPM |
KaMin Hydralux® 91 Clay Hydralux® 91 is a high brightness, fine glossing coating clay used in heavy weight coated paper and coated board application. Its fine particle excellent flow properties and size allow for high .. |
|||
Brookfield Viscosity | 500 cP @Temperature 25.0 °C |
500 cP @Temperature 77.0 °F |
20 RPM |
KaMin KaMin® Tek 2001 Clay The uniform, narrow particle size distribution and excellent color makes Kamin® TEK 2001 the preferred extender for gloss latex paints where optimum TiO2 spacing is desired without adverse effect.. |
|||
Brookfield Viscosity | <= 500 cP | <= 500 cP | Spindle # 3, rpm 60 |
Michelman® DigiPrime® 1500LA Primer Description: Primer for digital printing on paper substratesUsage: DigiPrime®1500LA is a product that can be added to size press treatments or pigment coatings to optimize substrates for HP Indig.. |
|||
Brookfield Viscosity | 500 - 1000 cP | 500 - 1000 cP | Spindle # 3, rpm 60 |
Michelman® Michem® Guard 60 Nonionic Fischer-Tropsch dispersion Description: Nonionic Fischer-Tropsch dispersionUsage: Michem® Guard 60 is a dispersion which provides mar resistance properties when used as an additive in paint, coating, ink and graphic art fo.. |
|||
Brookfield Viscosity | 500 - 1100 cP | 500 - 1100 cP | Brookfield RVF sp 3, 20 rpm, Solution 15% MEK (MQSA Nº 55 A); MQSA 40A |
Lubrizol Advanced Materials Pearlstick® D40-70/08 Linear Thermoplastic Polyurethane Pearlstick D40-70/08 is an elastic, linear, aromatic polyurethane, supplied in form of white spherical granules with an extremely high crystallization rate and a very low thermoplasticity level. S.. |
|||
Brookfield Viscosity | 500 cP | 500 cP | 30 rpm |
Solvay RHODOLINE® 581B Surfactant Description: Mineral oil defoamers for high PVC systems Chemical Name: DEFOAMERCAS: 64742-47-8Available in: Asia Pacific, Europe, Latin America and North AmericaSolubility(2% in DI Water): Coarse Di.. |
|||
Brookfield Viscosity | 500 cP @Temperature 25.0 °C |
500 cP @Temperature 77.0 °F |
|
Loctite® 4981 Cyanoacrylate Adhesive Medical Grade BondersLoctite offers the most comprehensive line of adhesives and sealants available to the medical device industry. These USP class VI and/or ISO-10993 compliant products are designe.. |
|||
Brookfield Viscosity | 500 cP | 500 cP | / 1.5 rpm; spindle #2 |
Abatron AboCoat 8204-15/AboCure 8204-15 Epoxy Coating AboCoat 8204-15 is a flammable light-blue liquid resin. AboCure 8204-115 is a flammable clear amber liquid converter. AboCoat 8204-15/AboCure 8204-15 is a dielectric coating for high chemical, solve.. |
|||
Brookfield Viscosity | 500 cP | 500 cP | #1 spindle; 30 rpm. |
DuPont Performance Polymers Neoprene 115 Polychloroprene
(discontinued **) Main feature: Mechanical stability methacrylic acid copolymer reactive. Principal uses include: Coatings, Modifiers, Asphalt, Concrete.Solids content: 47%. Initial pH: 7. Surface tension: 47 dyne.. |
|||
Brookfield Viscosity | <= 500 cP | <= 500 cP | Spindle # 1, rpm 60 |
Michelman® Michem® Coat 1548 Water and grease resistant, gluable coating Description: Water and grease resistant, gluable coatingUsage: Michem® Coat 1548 is a machine ready coating which imparts good water, grease and oil resistance to the substrate. This product has be.. |
|||
Brookfield Viscosity | 500 cP | 500 cP | |
DuPont Performance Polymers AquaStik® AQS-1120 Polychloroprene Latex
(discontinued **) Aquastik™ polychloroprene latexes have been designed for the adhesives industry. They provide an environmentally friendly alternative to solvent-borne systems.This grade features mechanical stabil.. |