Michelman® Michem® Emulsion 70350 Cationic paraffin emulsion

Category Fluid , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Michelman®
Trade Name Michem® Emulsion
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Michelman® Michem® Emulsion 70350 Cationic paraffin emulsion.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: Cationic paraffin emulsionUsage: Michem® Emulsion 70350 is designed to be a water repellent additive. This product is effectively used for the curing and protection of concrete.We serve many markets through Michem® Emulsion, including: paint & coatings; fiberglass; inks and overprint varnishes; floor care; wood finishes; automotive care products; building products; carpets; die lubricants; fruit and vegetable coatings; textiles and urethane foamInformation provided by Michelman®
Physical Properties Metric English Comments
Specific Gravity 0.940 - 0.960 g/cc
0.940 - 0.960 g/cc
Volatiles 49.5 - 50.5 %
49.5 - 50.5 %
pH 4.5 - 6.5
4.5 - 6.5
<= 7.0
<= 7.0
Recommended pH of system
Brookfield Viscosity <= 500 cP
<= 500 cP
Spindle # 2, rpm 60
Descriptive Properties Value Comments
Appearance White liquid
Emulsifier Charge Cationic
Solids Type Scale
Users viewing this material also viewed the following: