Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 500 cP | 500 cP | RVT Spindle 3 @ 20 rpm |
Palm Labs Adhesives TURBO-LOCK SERIES 14 Anaerobic Thread Locking Compound TURBO-LOCK 14 SERIES is a fast curing, high strength, RED, permanent, anaerobic thread-locking compound for bonding and sealing threads. It is highly resistance to heat, vibrations, water, gases, oi.. |
|||
Brookfield Viscosity | 500 cP | 500 cP | One Day Viscosity @ 6rpmGeon® STP 1434 (with provided formulation); Internal Method |
PolyOne Geon™ 170 Series 174 Polyvinyl Chloride Homopolymer (PVC Homopolymer) Geon® 174 is a medium molecular weight, fine particle size homopolymer dispersion resin. It provides a good balance of fused film properties and processing temperatures. It is recommended for appli.. |
|||
Brookfield Viscosity | <= 500 cP | <= 500 cP | #2/20 rpm |
Mallard Creek Polymers PolySaf® 5600 Cationic Polymer PolySaf® 5600 polymer provides exceptional deodorancy performance in personal care products. This non-irritating cationic polymer also enhances the sensory performance of body washes.Markets: Per.. |
|||
Brookfield Viscosity | <= 500 cP | <= 500 cP | #2/20 rpm |
Mallard Creek Polymers ROVENE® 4049 SBR Latex ROVENE® 4049 is a carboxylated styrene-butadiene emulsion that has a medium hand with above average strength properties. This binder has the ability to be cross-linked with external cross-linking.. |
|||
Brookfield Viscosity | <= 500 cP | <= 500 cP | #20/200 |
Mallard Creek Polymers Rovene® 4111 Styrene-Butadiene Emulsion Rovene® 4111 was designed with a specific particle size that greatly improves the spacing between titanium dioxide particles resulting in increased opacity. Additionally, using Rovene® 4111 ma.. |
|||
Brookfield Viscosity | <= 500 cP | <= 500 cP | #20/200 |
Mallard Creek Polymers Rovene® 6065 Styrene-Acrylic Emulsion Applications: Rovene® 6065 is a tough, durable nonwoven binder intended to provide improved stiffness and strength. Rovene® 6065 was specifically designed to perform in formaldehyde-free syste.. |
|||
Brookfield Viscosity | 500 - 1800 cP | 500 - 1800 cP | #2/20 rpm |
Mallard Creek Polymers ROVENE® 6101 Styrene-Acrylic Emulsion ROVENE® 6101 is a stiff, non-film forming high-gloss extending vehicle for flexographic and gravure inks and overprint varnishes. It is intended for use primarily on paper and paperboard.APPLICAT.. |
|||
Brookfield Viscosity | <= 500 cP | <= 500 cP | #20/200 |
Mallard Creek Polymers Rovene® 6126 Styrene-Acrylic Emulsion Applications: Rovene® 6126 provides a flexible yet strong cohesive bond for a range of materials and particle surface areas. Rovene® 6126 imparts films with good water resistance properties. F.. |
|||
Brookfield Viscosity | <= 500 cP | <= 500 cP | #20/200 |
Mallard Creek Polymers Rovene® 6506 Styrene-Acrylic Emulsion Applications: Rovene® 6506 typical applications are across a variety of nonwoven markets and substrates. Rovene® 6506 has demonstrated excellent performance as a binder on a lightweight nonwov.. |
|||
Brookfield Viscosity | <= 500 cP | <= 500 cP | #2/20 rpm |
Mallard Creek Polymers ROVENE® 8305 SBR Emulsion ROVENE® 8305 is a 50% bound styrene, high gel content hot polymerized styrene – butadiene emulsion. Compatibility with commercial tackifier resin emulsions is excellent, as is filler toleran.. |
|||
Brookfield Viscosity | <= 500 cP | <= 500 cP | Spindle # 2, rpm 60 |
Michelman® DigiPrime® 2500 Primer Description: Primer for digital printing suitable for paper substratesUsage: DigiPrime® 2500 is a product that can be added to size press treatments or pigment coatings to optimize substrates for.. |
|||
Brookfield Viscosity | <= 500 cP | <= 500 cP | Spindle # 3, rpm 60 |
Michelman® Michem® Emulsion 48625M1 Polymer solution Description: Polymer solutionUsage: Michem® Emulsion 48625M1 is a sizing polymer for fiberglass and other fibers serving as reinforcement for various resins.We serve many markets through MichemÂ.. |
|||
Brookfield Viscosity | <= 500 cP | <= 500 cP | Spindle # 3, rpm 60 |
Michelman® Michem® Flex P1801 Water based primer Description: Water based primer for liquids and extrusion coated resins.Usage: Michem®Flex P1801 is a primer for film and paper substrates to promote adhesion to extrusion coated resins resulting.. |
|||
Brookfield Viscosity | <= 500 cP | <= 500 cP | Spindle # 2, rpm 60 |
Michelman® Michem® Guard 1350 Nonionic emulsion of polyethylene wax Description: Nonionic emulsion of polyethylene waxUsage: Michem® Guard 1350 is a water based one micron dispersion which improves rub and abrasion resistance in pigmented coatings and semi-gloss .. |
|||
Brookfield Viscosity | 500 - 1000 cP | 500 - 1000 cP | Spindle # 3, rpm 60 |
Michelman® Michem® Guard 350 Nonionic, Fischer-Tropsch dispersion Description: Nonionic, Fischer-Tropsch dispersionUsage: Michem® Guard 350 is designed to impart abrasion resistance, rub resistance and matting properties to aqueous paints, coatings and inksTypi.. |
|||
Brookfield Viscosity | <= 500 cP | <= 500 cP | Spindle # 3, rpm 60 |
Michelman® Michem® Guard 7140 Anionic dispersion of polyethylene wax Description: Anionic dispersion of polyethylene waxUsage: Michem® Guard 7140 is a water-based, large particle emulsion which improves rub and abrasion resistance in pigmented coatings and semi-gl.. |
|||
Brookfield Viscosity | <= 500 cP | <= 500 cP | Spindle # 2, rpm 60 |
Michelman® Michem® Prime 2960 Ethylene acrylic acid dispersion Description: Ethylene acrylic acid dispersionUsage: Michem® Prime 2960 provides outstanding adhesion to both metallic and cellulosic substrates, and enhances the water, grease, oil and solvent re.. |
|||
Brookfield Viscosity | 500 cP @Temperature 25.0 °C |
500 cP @Temperature 77.0 °F |
25% Toluene solution; BAM 922 |
Kraton® D1117 P (SIS) Linear Block Copolymer Description:Kraton D1117 P is a clear, linear triblock copolymer based on styrene and isoprene with a polystyrene content of 17%. It is supplied from North America in the physical form identified: K.. |
|||
Brookfield Viscosity | 500 cP @Temperature 25.0 °C |
500 cP @Temperature 77.0 °F |
20 RPM |
KaMin Hydralux® 91 Clay Hydralux® 91 is a high brightness, fine glossing coating clay used in heavy weight coated paper and coated board application. Its fine particle excellent flow properties and size allow for high .. |
|||
Brookfield Viscosity | 500 cP @Temperature 25.0 °C |
500 cP @Temperature 77.0 °F |
20 RPM |
KaMin KaMin® Tek 2001 Clay The uniform, narrow particle size distribution and excellent color makes Kamin® TEK 2001 the preferred extender for gloss latex paints where optimum TiO2 spacing is desired without adverse effect.. |
|||
Brookfield Viscosity | 500 - 1000 cP | 500 - 1000 cP | Spindle # 3, rpm 60 |
Michelman® Michem® Guard 349 Nonionic, polyethylene dispersion Description: Nonionic, polyethylene dispersionUsage: Michem® Guard 349 is designed to impart rub resistance, block resistance and matting properties to aqueous paints, coatings and inks.Typical u.. |
|||
Brookfield Viscosity | 500 cP @Temperature 25.0 °C |
500 cP @Temperature 77.0 °F |
|
Loctite® 3492 Acrylic Light Cure Adhesive Acrylic Light Cure AdhesivesVersatile Loctite® ultraviolet (UV) and visible light curing adhesives can be used in bonding, encapsulating, coating, tacking, and sealing applications. These single co.. |
|||
Brookfield Viscosity | 500 cP @Temperature 25.0 °C |
500 cP @Temperature 77.0 °F |
|
Loctite® 4013 Cyanoacrylate Adhesive Medical Grade BondersLoctite offers the most comprehensive line of adhesives and sealants available to the medical device industry. These USP class VI and/or ISO-10993 compliant products are designe.. |
|||
Brookfield Viscosity | 500 cP @Temperature 25.0 °C |
500 cP @Temperature 77.0 °F |
|
Loctite® 4981 Cyanoacrylate Adhesive Medical Grade BondersLoctite offers the most comprehensive line of adhesives and sealants available to the medical device industry. These USP class VI and/or ISO-10993 compliant products are designe.. |
|||
Brookfield Viscosity | 500 cP | 500 cP | #5, 100 RPM |
Dow BETAFOAM™ 89120 Water/Amine catalyst BETAFOAM™ 89120 is a component used to make low density, all water blown rigid polyurethane foam.Information provided by Dow |
|||
Brookfield Viscosity | 500 cP | 500 cP | / 1.5 rpm; spindle #2 |
Abatron AboCoat 8204-15/AboCure 8204-15 Epoxy Coating AboCoat 8204-15 is a flammable light-blue liquid resin. AboCure 8204-115 is a flammable clear amber liquid converter. AboCoat 8204-15/AboCure 8204-15 is a dielectric coating for high chemical, solve.. |
|||
Brookfield Viscosity | 500 - 700 cP @Temperature 25.0 °C |
500 - 700 cP @Temperature 77.0 °F |
|
C.O.I.M. EXTER S® S 801 Neopentylic Resin Description: The Exter S product line contains a large number of unsaturated polyester resin products with an array of properties and applications.Specific Notes for ESTER S® S 801: Resin for gel-c.. |
|||
Brookfield Viscosity | 500 - 2500 cP | 500 - 2500 cP | RVF #6 sp. @ 4 rpm |
3M Scotch-Seal™ 1252 Tamper Proof Sealant 3M™ Scotch-Seal™ Tamper Proof Sealant 1252 is a fast drying, anti-tamper sealer which is fire retardant.Features: Can be applied over adjustable or removable parts to indicuate changes in adjustme.. |
|||
Brookfield Viscosity | <= 500 cP | <= 500 cP | Spindle # 1, rpm 60 |
Michelman® Michem® Coat 1548 Water and grease resistant, gluable coating Description: Water and grease resistant, gluable coatingUsage: Michem® Coat 1548 is a machine ready coating which imparts good water, grease and oil resistance to the substrate. This product has be.. |
|||
Brookfield Viscosity | 500 cP | 500 cP | |
DuPont Performance Polymers AquaStik® AQS-1120 Polychloroprene Latex
(discontinued **) Aquastik™ polychloroprene latexes have been designed for the adhesives industry. They provide an environmentally friendly alternative to solvent-borne systems.This grade features mechanical stabil.. |