Physical Properties | Metric | English | Comments |
---|---|---|---|
Environmental Stress Crack Resistance | >= 500 hour | >= 500 hour | ISO 22088 |
Polimeri Europa Eraclene® BC 86 High Density Polyethylene - Blow Molding Eraclene BC 86 is a high density polyethylene resin (HDPE) with antioxidants, suitable for blow molding application. It is especially recommended for the production of containers up to 20 liters.Er.. |
|||
Environmental Stress Crack Resistance | >= 500 hour | >= 500 hour | F50, Condition A, ASTM D1693, 100% Igepal |
NOVA Chemicals Novapol® HB-W355-A HDPE Blow Molding Resin Molded Plaque Properties.Applications: drums, large industrial parts.Data provided by the manufacturer. |
|||
Environmental Stress Crack Resistance | >= 500 hour | >= 500 hour | F<sub>0</sub>; ASTM D1693/B |
Reliance Industries Relene S42005 Polyethylene Wire and cable High Density Polyethylene grade. Characteristics: excellent processing, superior physical/electrical properties, good environmental stress crack resistance. Applications: recommended .. |
|||
Environmental Stress Crack Resistance | >= 500 hour | >= 500 hour | (10% Igepal), F<sub>50</sub>; ASTM D1693 |
Formosa Plastics Formolene® L64220UT1 Rotational Molding LLDPE
(discontinued **) Hexene CopolymerApplications: Large tanks, material handling equipment and industrial rotational molding applications.Formolene L64220U is fully heat and UV stabilized.Meets all requirements of the .. |
|||
Environmental Stress Crack Resistance | 500 - 1000 hour | 500 - 1000 hour | Average value: 667 hour Grade Count:6 |
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate; Molded/Extruded". Each property range of values reported is minimum and maximum .. |
|||
Environmental Stress Crack Resistance | >= 500 hour | >= 500 hour | F50, Condition A; ASTM D1693 |
ExxonMobil Escorene® LD-721 High EVA Coextrusion Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A high vinyl acetate copolymer specialty film resin providing outstanding heat sealability along with excellent strength, properties and clarity.App.. |
|||
Environmental Stress Crack Resistance | >= 500 hour | >= 500 hour | F50, Condition A; ASTM D1693 |
ExxonMobil Escorene® LD-723 High EVA Extrusion Coating Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A high vinyl acetate extrusion coating resin which provides outstanding heat sealability and high clarity. It has a good balance of drawability and.. |
|||
Environmental Stress Crack Resistance | >= 500 hour | >= 500 hour | F50, Condition A; ASTM D1693 |
ExxonMobil Escorene® LD-725 High EVA Film and Compounding Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.An 18% vinyl acetate copolymer designed for specialty film and compounding applications. Outstanding sealability and low modulus are key attributes.. |
|||
Environmental Stress Crack Resistance | >= 500 hour | >= 500 hour | F50, Condition A; ASTM D1693 |
ExxonMobil Escorene® LD-781 High EVA Compounding Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 33% vinyl acetate copolymer for specialty compounding applications. The resin provides excellent stress cracking and flexibility, and allows outs.. |
|||
Environmental Stress Crack Resistance | >= 500 hour | >= 500 hour | F50, Condition B; ASTM D1693 |
ExxonMobil Escorene® LL-8461 LMDPE Rotational Molding Grade
(discontinued **) Data provided by the manufacturer, Exxon Chemical.LL-8400 series are linear medium density polyethylene resins that provide outstanding environmental stress crack resistance. LL-8461 is fully formu.. |
|||
Environmental Stress Crack Resistance | >= 500 hour | >= 500 hour | |
Kazanorgsintez 102-03K Cable Composition Based on Low Density Polyethylene Production Method: Produced in the form of pellets (natural or black colored) on the bases of basic 10204-003, 15303-003, 15313-003. Application: Designed to apply isolation, cable covers and ca.. |
|||
Environmental Stress Crack Resistance | >= 500 hour | >= 500 hour | |
Kazanorgsintez 102-05K Cable Composition Based on Low Density Polyethylene Production Method: Produced in the form of pellets (natural or black colored) on the bases of basic 10204-003, 15303-003, 15313-003. Application: Designed to apply isolation, cable covers and ca.. |
|||
Environmental Stress Crack Resistance | >= 500 hour | >= 500 hour | |
Kazanorgsintez 102-11K Cable Composition Based on Low Density Polyethylene Production Method: Produced in the form of pellets (natural or black colored) on the bases of basic 10204-003, 15303-003, 15313-003. Application: Designed to apply isolation, cable covers and ca.. |
|||
Environmental Stress Crack Resistance | >= 500 hour | >= 500 hour | |
Kazanorgsintez 153-05K Cable Composition Based on Low Density Polyethylene Production Method: Produced in the form of pellets (natural or black colored) on the bases of basic 10204-003, 15303-003, 15313-003. Application: Designed to apply isolation, cable covers and ca.. |
|||
Environmental Stress Crack Resistance | >= 500 hour | >= 500 hour | F50; ASTM D1693 |
LG Chemical LUTENE BB0808 LDPE Blown Film Grade Description: LUTENE BB0808 is mainly intended for the extrusion of blown film with high mechanical property for the manufacture of shrink film and pallet shrink covers. LUTENE BB0808 have the balanc.. |
|||
Environmental Stress Crack Resistance | >= 500 hour | >= 500 hour | ASTM D1693A |
Ineos K50-10-136 HDPE Ineos K50-10-136 is a high molecular weight, high density polyethylene copolymer. This product was developed for blowmolding automotive fuel tanks and other large parts, where the finished produc.. |
|||
Environmental Stress Crack Resistance | >= 500 hour | >= 500 hour | F50; ASTM D1693 |
LG Chemical SEETEC PF150 HDPE Features: Characteristics: Good impact & tear strength, High speed & superior heat sealing propertiesAdditives: Anti-oxidants, LubricantsApplication: Shopping bags, Thin films, Trash bags, Multiwall.. |
|||
Environmental Stress Crack Resistance | 500 hour | 500 hour | |
JPJ Technologies 7300M HDPE Extrusion Information provided by JPJ Technologies |
|||
Environmental Stress Crack Resistance | 500 hour | 500 hour | |
JPJ Technologies 7800M HDPE Extrusion Information provided by JPJ Technologies |
|||
Environmental Stress Crack Resistance | >= 500 hour @Temperature 50.0 °C |
>= 500 hour @Temperature 122 °F |
F50, 25% Igepal; ASTM D1693 |
SCG Chemicals EL-Proâ„¢ P400S Polypropylene Flat Yarn/Sheet Key Characteristics:High outputGood mechanical propertiesRecommended Applications:Stretched tapeMonofilament for woven bag, woven sheet, rope, strap and sheetInformation provided by SCG Chemicals |
|||
Environmental Stress Crack Resistance | 500 hour | 500 hour | Condition B (10% Igepal), F<sub>50</sub>; ASTM D1693 |
Formosa Plastics Formolene® HB4903 Blow Molding HDPE Hexene CopolymerApplications: High performance blow molding applications, fuel tanks, seating, garbage cans, sheet, large industrial containers.Formolene HB4903 is a high performance copolymer that .. |
|||
Environmental Stress Crack Resistance | 500 hour | 500 hour | Antarox 10%, F50; ASTM D1693-A |
Borealis BS2541 High Density Polyethylene BS2541 is a high density polyethylene with very high ESCR This product is intended for blow molding. Applications: household and chemical containers such as detergents, cleaners, and motor oils, an.. |
|||
Environmental Stress Crack Resistance | >= 500 hour | >= 500 hour | F50; ASTM D2561 |
CPC - Vycom SEABOARD™ GRIP-X™ Slip Resistant High Density Polyethylene (HDPE) Grip-X is a UV stabilized high density polyethylene (HDPE) sheet formulated to meet demanding conditions of the marine industry. Grip-X is manufactured with a special surface treatment and stipulate.. |
|||
Environmental Stress Crack Resistance | 500 hour | 500 hour | Condition A (100% Igepal), F<sub>50</sub>; ASTM D1693 |
Formosa Plastics Formolene® HB4903 Sheet and Thermoforming HDPE
(discontinued **) High Density Hexene CopolymerApplications: Fuel tanks, seating, garbage cans, sheet, large industrial containers.Formolene HB4903 is a high performance copolymer that is designed for the most demand.. |
|||
Environmental Stress Crack Resistance | 500 hour | 500 hour | Condition B (10% Igepal), F<sub>50</sub>; ASTM D1693 |
Formosa Plastics Formolene® HB4903 Sheet and Thermoforming HDPE
(discontinued **) High Density Hexene CopolymerApplications: Fuel tanks, seating, garbage cans, sheet, large industrial containers.Formolene HB4903 is a high performance copolymer that is designed for the most demand.. |
|||
Environmental Stress Crack Resistance | >= 500 hour | >= 500 hour | F50, Condition A; ASTM D1693 |
ExxonMobil Escorene® LD-702 High EVA Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A fractional melt index, 13.3% vinyl acetate copolymer specialty film resin for applications requiring outstanding heat sealability, strength, and t.. |
|||
Environmental Stress Crack Resistance | >= 500 hour | >= 500 hour | F50, Condition A; ASTM D1693 |
ExxonMobil Escorene® LD-728 High EVA Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A high vinyl acetate copolymer with a low melting temperature and excellent strength properties and toughness.Applications: Injection molding; Foams.. |
|||
Environmental Stress Crack Resistance | >= 500 hour | >= 500 hour | F50, Condition B; ASTM D1693 |
ExxonMobil Escorene® LL-8302 LMDPE Rotational Molding Grade
(discontinued **) Data provided by the manufacturer, Exxon Chemical.LL-8300 series are linear medium density polyethylene resins that provide outstanding environmental stress crack resistance. LL-8302 is the base re.. |
|||
Environmental Stress Crack Resistance | >= 500 hour | >= 500 hour | F50, Condition A; ASTM D1693 |
ExxonMobil Escorene® LD-724 High EVA Compounding Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A high vinyl acetate copolymer resin for specialty compounding applications. Outstanding heat sealability along with excellent strength properties .. |
|||
Environmental Stress Crack Resistance | >= 500 hour | >= 500 hour | |
Kazanorgsintez 153-11K Cable Composition Based on Low Density Polyethylene Production Method: Produced in the form of pellets (natural or black colored) on the bases of basic 10204-003, 15303-003, 15313-003. Application: Designed to apply isolation, cable covers and ca.. |