Physical Properties | Metric | English | Comments |
---|---|---|---|
Environmental Stress Crack Resistance | >= 1000 hour | >= 1000 hour | ASTM D1693 |
NIZHNEKAMSKNEFTEKHIM PE 6948C (486H3) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Environmental Stress Crack Resistance | 1000 hour | 1000 hour | Average value: 1000 hour Grade Count:4 |
Overview of materials for Thermoplastic Olefinic Elastomer (TPO) This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Olefinic Elastomer (TPO)". Each property range of values reported is minimum and maximum v.. |
|||
Environmental Stress Crack Resistance | >= 1000 hour | >= 1000 hour | Condition A (100% Igepal), F<sub>50</sub>; ASTM D1693 |
Formosa Plastics Formolene® L43840U Rotational Molding LLDPE
(discontinued **) Butene CopolymerApplications: Toys and other non-tank rotational molding applications.Formolene L43840U is a Butene Copolymer of linear low density polyethylene for toys and other non-tank rotationa.. |
|||
Environmental Stress Crack Resistance | >= 1000 hour | >= 1000 hour | Condition A (100% Igepal), F<sub>50</sub>; ASTM D1693 |
Formosa Plastics Formolene® L63550U Rotational Molding LLDPE
(discontinued **) Hexene CopolymerApplications: Toys, medium tanks, material handling equipment and flat surface rotational molding applications.Formolene L63550 is fully heat and UV stabilized.Meets all requirements.. |
|||
Environmental Stress Crack Resistance | >= 1000 hour | >= 1000 hour | (100% Igepal), F<sub>50</sub>; ASTM D1693 |
Formosa Plastics Formolene® L63565 Rotational Molding LLDPE
(discontinued **) Hexene CopolymerApplications: Toys, medium tanks, material handling equipment and flat surface rotational molding applications.Meets all requirements of the U.S. Food and Drug Administration as spec.. |
|||
Environmental Stress Crack Resistance | >= 1000 hour | >= 1000 hour | (100% Igepal), F<sub>50</sub>; ASTM D1693 |
Formosa Plastics Formolene® L63565U Rotational Molding LLDPE
(discontinued **) Hexene CopolymerApplications: Toys, medium tanks, material handling equipment and flat surface rotational molding applications.Formolene L63565U is fully heat and UV stabilized.Meets all requirement.. |
|||
Environmental Stress Crack Resistance | >= 1000 hour | >= 1000 hour | (100% Igepal), F<sub>50</sub>; ASTM D1693 |
Formosa Plastics Formolene® L63935 Rotational Molding LLDPE
(discontinued **) Hexene CopolymerApplications: Tanks, toys and other non-tank rotational molding applicationsMeets all requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520, covering .. |
|||
Environmental Stress Crack Resistance | 1000 hour | 1000 hour | |
NOVA Chemicals Sclair® 35BP HDPE Extrusion Resin, 2.2% Carbon Black Filled
(discontinued **) Features: Excellent ESCR, medium molecular weight, good processability, excellent long term thermal stability, good chemical resistance, excellent UV stability.Applications: Extrusion on to metal pi.. |
|||
Environmental Stress Crack Resistance | >= 1000 hour | >= 1000 hour | F0, ASTM D1693 |
NOVA Chemicals Sclair® 96A HDPE Extrusion Resin
(discontinued **) Features: Excellent processability, excellent stretchability, superior strength, gel free.Applications: Oriented tapes for industrial woven bags and tarpaulins, monoaxial oriented films.Data provide.. |
|||
Environmental Stress Crack Resistance | >= 1000 hour | >= 1000 hour | ASTM D1693 |
ExxonMobil HD 9856BA Blow Molding Resin
(discontinued **) HD 9856BA is a HDPE blow molding resin designed for high performance packaging applications. Containers made from HD 9856BA exhibit a unique combination of stiffness and environmental stress cracki.. |
|||
Environmental Stress Crack Resistance | >= 1000 hour | >= 1000 hour | 10% Igepal®; ASTM D1693 |
LyondellBasell Petrothene® GA837091 Medium Density Polyethylene
(Unverified Data**) ApplicationsPETROTHENE GA 837-091 is a broad molecular weight, medium density resin designed for use as a base resin in wire and cable jacketing. An antioxidant has been added to ensure thermal st.. |
|||
Environmental Stress Crack Resistance | >= 1000 hour | >= 1000 hour | No failures, compressed ring, 25% Igepal; ASTM F 1248 |
Total Finathene® 3407B Black HDPE pipe grade
(discontinued **) Applications: industrial and mining gas distribution, potable water, sewer and sewer relining, gas and oil gathering, fiber optic innerduct, general pipe reliningInformation provided provided by To.. |
|||
Environmental Stress Crack Resistance | >= 1000 hour | >= 1000 hour | F50, Condition C; ASTM D1693 |
ExxonMobil Escorene® LD-612 EVA Injection Molding Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 5.8% vinyl acetate copolymer resin designed for molding and extrusion applications requiring low temperatures, flexibility and toughness. This re.. |
|||
Environmental Stress Crack Resistance | >= 1000 hour | >= 1000 hour | F50, Condition C; ASTM D1693 |
ExxonMobil Escorene® LD-613 EVA Injection Molding Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.An 8.8% vinyl acetate copolymer resin designed for molding and extrusion applications requiring low temperatures, flexibility and toughness. This r.. |
|||
Environmental Stress Crack Resistance | >= 1000 hour | >= 1000 hour | F50, Condition A; ASTM D1693 |
ExxonMobil Escorene® LD-401 EVA for Electrical Insulation
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A crosslinkable, 9.9% vinyl acetate copolymer designed for electrical applications.Applications: Base resin for fully formulated low voltage cable i.. |
|||
Environmental Stress Crack Resistance | >= 1000 hour | >= 1000 hour | F<sub>50</sub>; ASTM D1693 |
LyondellBasell Petrothene® LP5002 High Density Polyethylene (Blow Molding Grade) ApplicationsThe PETROTHENE LP series of polyethylene resins exhibits excellent environmental stress crack resistance and is especially designed for bottles containing aggressive agricultural and hou.. |
|||
Environmental Stress Crack Resistance | >= 1000 hour | >= 1000 hour | F<sub>50</sub>; ASTM D1693 |
LyondellBasell Petrothene® LP500200 High Density Polyethylene (Sheet & Profile Grade) ApplicationsThe PETROTHENE LP 5002 series of polyethylene resins exhibits excellent environmental stress crack resistance.Regulatory StatusThe LP 5002 base resin meets the requirements of Food and D.. |
|||
Environmental Stress Crack Resistance | >= 1000 hour | >= 1000 hour | Condition A - 10% Igepal®; ASTM D1693 |
LyondellBasell Petrothene® PR92735 Linear Low Density Polyethylene ApplicationsPETROTHENE PR 92735 is a high molecular weight, linear low density-based compound designed for cable jacketing. PR 92735 contains a nominal carbon black content of 2.6% and antioxidant .. |
|||
Environmental Stress Crack Resistance | >= 1000 hour | >= 1000 hour | Condition B, F50; ASTM D1693 |
IRPC Polimaxx Polene GG3245 High Density Polyethylene CHARACTERISTICS: EXCELLENT ENVIRONMENTAL STRESS CRACKING RESISTANCE (ESCR) EXCELLENT IMPACT STRENGTH, GOOD PROCESSABILITY, HIGH TOUGHNESSAPPLICATIONS: BLOW MOLDING/ SHEET/ THERMOFORMING EXTRUSION CO.. |
|||
Environmental Stress Crack Resistance | >= 1000 hour @Temperature 50.0 °C |
>= 1000 hour @Temperature 122 °F |
F50, 25% Igepal; ASTM D1639 |
SCG Chemicals EL-Leneâ„¢ L1810FI Linear Low Density Polyethylene Film Key Characteristics:High gloss and clarityContains 3200 ppm slip agent and 2400 ppm antiblocking agentRecommended Applications:Water-quench blown film for general purpose bags such as vegetable or f.. |
|||
Environmental Stress Crack Resistance | 1000 hour | 1000 hour | F50; ASTM D1693 |
UBE UMERIT 2500F Metallocene LLDPE Description: UBE Super Polyethylene Umerit® is an ethylene-olefin copolymer made by UBE using the metallocene catalytic method. The metallocene catalytic method results in superior physical propert.. |
|||
Environmental Stress Crack Resistance | 1000 hour | 1000 hour | F50; ASTM D1693 |
UBE UMERIT 2525F Metallocene LLDPE Description: UBE Super Polyethylene Umerit® is an ethylene-olefin copolymer made by UBE using the metallocene catalytic method. The metallocene catalytic method results in superior physical propert.. |
|||
Environmental Stress Crack Resistance | >= 1000 hour | >= 1000 hour | ASTM D1693 cond. B |
Total 3802 B HDPE, cable, sheet, pipe, injection molding FINATHENE® 3802 B is a polyethylene copolymer based on C6 hexene as co-monomer and is produced by a continuous low-pressure slurry polymerization process. FINATHENE® 3802 B is a black polyethylene.. |
|||
Environmental Stress Crack Resistance | >= 1000 hour | >= 1000 hour | ASTM D1693 cond. B 100% lgepal |
Total 54050 HDPE, blow molding Applications: 55-gallon shipping containers, open-top drums, industrial tanks, agricultural chemical tanks. Blow Molding Stock Temperature 380 – 450 ºF Extrusion melt temperature 400 - 480ºFInfor.. |
|||
Environmental Stress Crack Resistance | >= 1000 hour @Temperature 80.0 °C |
>= 1000 hour @Temperature 176 °F |
At 9.2 bar; ISO 13479 |
Borealis Borstar® HE3492-LS Yellow-Orange High Density Polyethylene for Natural Gas Pipes Borstar HE3492-LS is a yellow-orange, cadmium free, high density polyethylene compound classified as a MRS 10.0 material (PE100) produced with the advanced Borstar technology. It includes a combina.. |
|||
Environmental Stress Crack Resistance | 1000 hour | 1000 hour | F50; ASTM D1693 |
UBE UMERIT 1500F Metallocene LLDPE Description: UBE Super Polyethylene Umerit® is an ethylene-olefin copolymer made by UBE using the metallocene catalytic method. The metallocene catalytic method results in superior physical propert.. |
|||
Environmental Stress Crack Resistance | >= 1000 hour @Temperature 50.0 °C |
>= 1000 hour @Temperature 122 °F |
Condition B; ASTM D 1693 |
Chevron Phillips Marlex® HXB TR-512 Extra high molecular weight polyethylene Benefits: outstanding impact and creep resistance, excellent ESCR, excellent chemical resistanceCharacteristics: ESCR > 700 at Condition A, at 50°C; ASTM D 1693Applications: 55-gallon drums, indust.. |
|||
Environmental Stress Crack Resistance | 1000 - 5000 hour | 1000 - 5000 hour | Average value: 2290 hour Grade Count:10 |
Overview of materials for Medium Density Polyethylene (MDPE), Extruded This property data is a summary of similar materials in the MatWeb database for the category "Medium Density Polyethylene (MDPE), Extruded". Each property range of values reported is minimum and max.. |
|||
Environmental Stress Crack Resistance | >= 1000 hour @Thickness 3.00 mm, Temperature 50.0 °C |
>= 1000 hour @Thickness 0.118 in, Temperature 122 °F |
Condition A, Compression Molded, 10% Igepal; ASTM D1693 |
Solvay Specialty Polymers Cogegum® AFR/960 Polyolefin Cogegum® HFFR -Halogen Free Fire Retardant compound. Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties withou.. |
|||
Environmental Stress Crack Resistance | >= 1000 hour @Temperature 50.0 - 50.0 °C |
>= 1000 hour @Temperature 122 - 122 °F |
Average value: 1000 hour Grade Count:3 |
Overview of materials for High Density Polyethylene (HDPE), Crosslinkable This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Crosslinkable". Each property range of values reported is minimum and .. |