Physical Properties | Metric | English | Comments |
---|---|---|---|
Environmental Stress Crack Resistance | >= 50 hour | >= 50 hour | |
Kazanorgsintez PE2NT26-13 High Density Polyethylene Composite Production Method: Copolymerization of eythylene at low pressure in presence of complex catalysts using gaseous-phase method. Application: Composition is intended for injection molding processin.. |
|||
Environmental Stress Crack Resistance | 50 hour | 50 hour | F<sub>50</sub>; ASTM D1693 |
LyondellBasell Alathon® L5440 High Density Polyethylene ApplicationsALATHON L 5440 is designed for high shear machines. It exhibits excellent color, low odor and excellent processing stability. Typical applications include general purpose, household ch.. |
|||
Environmental Stress Crack Resistance | 50 hour | 50 hour | F50; ASTM D1693 |
LG Chemical LUTENE-H BE0400 HDPE Description: LUTENE - H BE0400 is an excellent materials for blow-molded articles with high density and rigidity. It has good flow characteristics and impact resistance.Applications: Blow molded con.. |
|||
Environmental Stress Crack Resistance | 50 hour @Pressure 4.00 MPa |
50 hour @Pressure 580 psi |
ISO CD 16770 |
Iran Petrochemical (PCC) EX 3 - 80 High Density Polyethylene EX3-80 is a high density polyethylene with 1-Butene as co monomer. It is natural, good ESCR, good impact strength, tough and rigid pipe resin. Applications: pipe extrusion PE 80 class, industrial a.. |
|||
Environmental Stress Crack Resistance | >= 50 hour | >= 50 hour | Condition B, F50; ASTM D1693 |
IRPC Polimaxx Polene GM2865 High Density Polyethylene CHARACTERISTICS: EXCELLENT STIFFNESS, GOOD PROCESSABILITY, HIGH IMPACT STRENGTHAPPLICATIONS: BLOW MOLDING FOR CONTAINERS FROM A FEW ml TO ABOUT 20 LITRES, DAIRY PRODUCT BOTTLES MILK BOTTLES AND GALL.. |
|||
Environmental Stress Crack Resistance | 50 hour @Temperature 23.0 °C |
50 hour @Temperature 73.4 °F |
F<sub>50</sub>; ASTM D1693 |
SIDPEC EGYPTENE® HD 5211 EA HDPE Injection Molding Applications:Paint pailsBottle capsHouse waresToysInformation provided by Interchim s.r.l., official distributor of Sidi Kerir Petrochemicals Co. (SIDPEC) Products |
|||
Environmental Stress Crack Resistance | 50 hour @Temperature 23.0 °C |
50 hour @Temperature 73.4 °F |
F<sub>50</sub>; ASTM D1693 |
SIDPEC EGYPTENE® HD 5813 EA HDPE Injection Molding Applications:CrateAerosol capsHouse waresInformation provided by Interchim s.r.l., official distributor of Sidi Kerir Petrochemicals Co. (SIDPEC) Products |
|||
Environmental Stress Crack Resistance | 50 hour | 50 hour | ASTM D1693 cond. B 10% lgepal |
Total 5202 HDPE, blow molding Applications: Bleach and detergents, industrial chemicals, industrial parts, packaging aggressive liquids, food packaging. Blow molding stock temperature 360 - 400°F Extrusion melt temperature 380 .. |
|||
Environmental Stress Crack Resistance | 50 hour | 50 hour | ASTM D1693 cond. B 10% lgepal |
Total 5202LD HDPE, blow molding Applications: Bleach and detergents, industrial chemicals, industrial parts, packaging aggressive liquids, food packaging. Blow molding stock temperature 360 - 400°F Extrusion melt temperature 380 .. |
|||
Environmental Stress Crack Resistance | 50 hour | 50 hour | ASTM D1693 cond. B 100% lgepal |
Total 5502 BZ HDPE injection blow molding Applications: Cosmetics and toiletries, pharmaceuticals, specialty containers, food packagingInformation provided provided by Total Petrochemicals.Total Petrochemicals acquired former Fina and Atof.. |
|||
Environmental Stress Crack Resistance | 50 hour | 50 hour | Condition B, 100% Igepal, F50; ASTM D1693 |
Total 5502 HDPE, blow molding, pipe Drug Master File listed; USP Class VI approved; FDA compliant; UL 94HB/746 certified |
|||
Environmental Stress Crack Resistance | 50 hour | 50 hour | Condition B, F<sub>50</sub>; ASTM D1693 |
Formosa Plastics Formolene® HB5202A Blow Molding HDPE High Density Polyethylene Hexene Copolymer for Blow Molding – With Antistat Formolene® HB5202A is designed for applications requiring excellent stiffness and stress crack resistance propertiesAppl.. |
|||
Environmental Stress Crack Resistance | 50 hour | 50 hour | Condition A (100% Igepal), F<sub>50</sub>; ASTM D1693 |
Formosa Plastics Formolene® HB5202B2 Sheet and Thermoforming HDPE High Density Polyethylene Hexene CopolymerApplications: Containers for bleach, detergents, chemicals; Molded or formed industrial housings, shrouds and tanks.Formolene HB5202B2 is designed for appli.. |
|||
Environmental Stress Crack Resistance | 50 hour | 50 hour | Condition B, F<sub>50</sub>; ASTM D1693 |
Formosa Plastics Formolene® HB5202B2 Sheet and Thermoforming HDPE High Density Polyethylene Hexene CopolymerApplications: Containers for bleach, detergents, chemicals; Molded or formed industrial housings, shrouds and tanks.Formolene HB5202B2 is designed for appli.. |
|||
Environmental Stress Crack Resistance | 50 hour | 50 hour | F50, Anatarox 100%; ASTM D 1693B |
Total HDPE 5802 High Density Polyethylene - Blow Molding HDPE 5802 is a high density polyethylene with excellent compromise between stiffness and Environmental Stress Crack Resistance. It has been specifically designed for the manufacture of blow molded .. |
|||
Environmental Stress Crack Resistance | 50 hour | 50 hour | Condition A (100% Igepal), F<sub>50</sub>; ASTM D1693 |
Formosa Plastics Formolene® HB5202B Blow Molding HDPE Hexene CopolymerApplications: Bleach, detergent and chemical containers; Molded or formed industrial housings, shrouds, tanksFormolene HB5202B is designed for applications requiring excellent stiffn.. |
|||
Environmental Stress Crack Resistance | 50 hour | 50 hour | Condition B, F<sub>50</sub>; ASTM D1693 |
Formosa Plastics Formolene® HB5202B Blow Molding HDPE Hexene CopolymerApplications: Bleach, detergent and chemical containers; Molded or formed industrial housings, shrouds, tanksFormolene HB5202B is designed for applications requiring excellent stiffn.. |
|||
Environmental Stress Crack Resistance | 50 hour | 50 hour | F50; ASTM D1693 B |
Equate EMDA-6200 HDPE Blow Molding Resin EMDA-6200 grade is a high-density polyethylene copolymer resin designed for blow molding small to medium size bottles. It can be used on intermittent as well as continuous blow molding machines for .. |
|||
Environmental Stress Crack Resistance | 50 hour | 50 hour | Condition B, F<sub>50</sub> |
Chevron Phillips Marlex® HHM 5202-02 BN High Density Ethylene Hexene-1 Copolymer High Density Ethylene Hexene-1 CopolymerCustomer Benefits: For the blow molder who wants to stock one resin that will be suitable for most of his customers' packaging needs. Lightweight containers .. |