Physical Properties | Metric | English | Comments |
---|---|---|---|
Environmental Stress Crack Resistance | <= 10 hour | <= 10 hour | F50, Condition A, ASTM D1693, 100% Igepal |
NOVA Chemicals Sclair® 2114 LLDPE Injection Molding Resin Features: High stiffness, high impact strength and low warpage, good top loading capability, high surface gloss.Applications: Container (tub) lids and closures.Data provided by the manufacturer. |
|||
Environmental Stress Crack Resistance | <= 10 hour | <= 10 hour | F50, Condition A, ASTM D1693, 100% Igepal |
NOVA Chemicals Sclair® 2807 HDPE Injection Molding Resin Features: Excellent processability for applications requiring moderate stiffness and toughness, good cold temperature impact properties.Applications: Industrial and lubricant pails.Data provided by .. |
|||
Environmental Stress Crack Resistance | <= 10 hour | <= 10 hour | F50, Condition A, ASTM D1693, 100% Igepal |
NOVA Chemicals Sclair® 2907 HDPE Injection Molding Resin Features: High stiffness, maximum impact strength and toughness, good top loading capability, high surface gloss.Applications: Protective sports equipment, safety helmets, high impact custom molding.. |
|||
Environmental Stress Crack Resistance | <= 10 hour | <= 10 hour | F50, Condition A, ASTM D1693, 100% Igepal |
NOVA Chemicals Sclair® 2908, 2908-UV8A HDPE Injection Molding Resin Features: High stiffness, maximum impact strength and toughness.Applications: Tote boxes, beverage crates.Data provided by the manufacturer. |
|||
Environmental Stress Crack Resistance | <= 10 hour | <= 10 hour | F<sub>50</sub>; Condition A, 100% Igepal; ASTM D1693 |
NOVA Chemicals Sclair® 2908C HDPE Injection Molding Resin High stiffness, Maximum impact strength and toughnessApplications: Tote boxes, Beverage cratesAdditives: AntioxidantInformation provided by NOVA Chemicals. |
|||
Environmental Stress Crack Resistance | <= 10 hour | <= 10 hour | F<sub>50</sub>; Condition A, 100% Igepal; ASTM D1693 |
NOVA Chemicals Sclair® 2909 HDPE Injection Molding Resin High stiffness, Maximum impact strength and toughness, Good top loading capability, High surface glossApplications: Tote boxes, Beverage cratesAdditives: Antioxidant, Ultraviolet light stabilizersIn.. |
|||
Environmental Stress Crack Resistance | <= 10 hour | <= 10 hour | F50, Condition A, ASTM D1693, 100% Igepal |
NOVA Chemicals Sclair® 8111 LLDPE Injection Molding Resin
(discontinued **) Features: Good processability, excellent impact resistance, excellent flexibility and freedom from warpage.Applications: Automotive splash-guards, large containers, closures and lids for food applic.. |
|||
Environmental Stress Crack Resistance | <= 10 hour | <= 10 hour | F50, Condition A, ASTM D1693, 100% Igepal |
NOVA Chemicals Sclair® 69A HDPE Extrusion Resin
(discontinued **) Features: High tensile strength, better moisture barrier, better oil and solvent resistance, lower friction coefficient, lower brittleness temperature, better abrasion resistance, better temperature.. |
|||
Environmental Stress Crack Resistance | 10 hour | 10 hour | Cond. B, 10%; ASTM D1693 |
ExxonMobil HD 6761.17 Injection Molding Resin
(discontinued **) HD 6761 is a narrow molecular weight hexene copolymer designed for good processability and excellent balance of ESCR, Toughness, and Stiffness properties. This resin is ideally suited for a heavy-d.. |
|||
Environmental Stress Crack Resistance | 10 hour | 10 hour | ASTM D1693-70 |
Total Finathene® 6006 HDPE, blow molding, pipe
(discontinued **) Finathene® 6006 is a high density polyethylene produced by the slurry loop low pressure polymerization process. Polymerization is conducted in the absence of any other comonomer. Finathene® 6006 h.. |
|||
Environmental Stress Crack Resistance | <= 10 hour | <= 10 hour | F50, Condition A, ASTM D1693, 100% Igepal |
NOVA Chemicals Sclair® 2709 HDPE Injection Molding Resin Features: Excellent cold temperature toughness, high stiffness.Applications: Housewares, containers, pails, closures.Data provided by the manufacturer. |
|||
Environmental Stress Crack Resistance | <= 10 hour | <= 10 hour | F50, Condition A, ASTM D1693, 100% Igepal |
NOVA Chemicals Sclair® 2710 HDPE Injection Molding Resin Features: Good ESCR, good processability.Applications: Housewares, containers, toys.Data provided by the manufacturer. |
|||
Environmental Stress Crack Resistance | 10 hour | 10 hour | Condition B, 10%; ASTM D1693 |
Ineos B4020N1331 Polyethylene Copolymer This is a unique high density polyethylene copolymer intended for the injection or compression molding of closures for beverages. Because of its high purity and excellent organoleptic properties, t.. |
|||
Environmental Stress Crack Resistance | 10 hour | 10 hour | Condition B, 10%; ASTM D1693 |
Ineos B4020N1332 Polyethylene Copolymer This is a unique high density polyethylene copolymer intended for the injection or compression molding of closures for beverages. Because of its high purity and excellent organoleptic properties, t.. |
|||
Environmental Stress Crack Resistance | 10 hour @Pressure 3.50 MPa |
10 hour @Pressure 508 psi |
ISO CD 16770 |
Iran Petrochemical (PCC) BL2 HF 4750 High Density Polyethylene BL2 is a high density polyethylene with 1-Butene as co monomer. It is high impact strength and slightly, lower stiffness than BL3, outstanding resistance to stress cracking, even in contact with su.. |
|||
Environmental Stress Crack Resistance | 10 hour | 10 hour | F<sub>50</sub>; ASTM D1693 |
Lotte Chemical Titan TITANZEX® HI2000 High density polyethylene HI2000 is a high density polyethylene for injection molding. HI2000 meets the U.S. Food and Drug Administration (FDA) criteria for food contact use as specified in 21 CFR 177.1520 (c) 3.1a & 3.2a. A.. |
|||
Environmental Stress Crack Resistance | 10 hour | 10 hour | F<sub>50</sub>; ASTM D1693 |
Lotte Chemical Titan TITANZEX® HM5001 High density polyethylene HM5001 is a high density polyethylene for yarn extrusion. HM5001 meets the U.S. Food and Drug Administration (FDA) criteria for food contact use as specified in 21 CFR 177.1520 (c) 3.1a & 3.2aApplic.. |
|||
Environmental Stress Crack Resistance | 10 hour | 10 hour | Antarox 10%, F50; ASTM D1693-A |
Borealis BL2631 High Density Polyethylene BL2631 is a high density polyethylene homopolymer intended for blow molding of products requiring high toughness and stiffness. Applications: fresh milk bottles, and juice bottles.Information provi.. |
|||
Environmental Stress Crack Resistance | 10 hour | 10 hour | F50, Anatarox 100%; ASTM D 1693/B |
Total HDPE 2008 SN 60 High Density Polyethylene - Blow Molding HDPE 2008 SN 60 is a high density polyethylene with very high stiffness and low viscosity. It has been specifically designed for the manufacture of thin walled containers for foodstuffs.HDPE 2008 S.. |
|||
Environmental Stress Crack Resistance | 10 hour | 10 hour | FNCT; ISO 16770 |
Total HDPE 53090 High Density Polyethylene - Blow Molding HDPE 53090 is a semi high molecular weight (SHMW) high density polyethylene with high resistance to impact, rigidity and good Environmental Stress Crack Resistance. It has been specifically designe.. |
|||
Environmental Stress Crack Resistance | 10 hour | 10 hour | F50, Anatarox 100%; ASTM D 1693/B |
Total HDPE HD 6221 High Density Polyethylene - Blow Molding HDPE HD 6221 is a high density polyethylene with very high stiffness and impact resistance. The low viscosity of this grade has been designed for the manufacture of thin walled containers for foods.. |
|||
Environmental Stress Crack Resistance | 10 hour | 10 hour | Condition B, F<sub>50</sub>; ASTM D1693 |
Formosa Plastics Formolene® HB6007 Blow Molding HDPE HomopolymerApplications: Milk, distilled water, soft drink concentrate, fruit juice, etc.Formolene HB6007 is a high quality product for those critical food packaging requirements. It also has excell.. |
|||
Environmental Stress Crack Resistance | 10 hour | 10 hour | Condition B, F<sub>50</sub>; ASTM D1693 |
Formosa Plastics Formolene® HP6000 Pipe HDPE High Density Polyethylene Homopolymer for Pipe Extrusion Formolene® HP6000 is a high quality product for homopolymer pipe extrusion applications. It has excellent stiffness and good stiffness prope.. |
|||
Environmental Stress Crack Resistance | <= 10 hour | <= 10 hour | F<sub>50</sub>; Condition A, 100% Igepal; ASTM D1693 |
NOVA Chemicals Sclair® 2111 LLDPE Injection Molding Resin
(discontinued **) Good processability, Excellent impact resistance, Excellent flexibility and freedom from warpageApplications: Automotive splash-guards, Large containers, Closures and lids for food applicationsAddit.. |