Network Polymers SAN 279 Water White Color

Category Polymer , Thermoplastic , SAN Polymer , Styrene Acrylonitrile (SAN), Transparent
Manufacturer Network Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Network Polymers SAN 279 Water White Color.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: SAN - Styrene Acrylonitrile Transparent Engineering ThermoplasticInformation provided by Network Polymers Inc.
Physical Properties Metric English Comments
Specific Gravity 1.08 g/cc
1.08 g/cc
ASTM D792
Linear Mold Shrinkage 0.0030 - 0.0070 cm/cm
0.0030 - 0.0070 in/in
ASTM D955
Melt Flow 2.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
2.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
Procedure A Condition G; ASTM D1238
7.5 g/10 min

@Load 3.80 kg,
Temperature 230 °C
7.5 g/10 min

@Load 8.38 lb,
Temperature 446 °F
Procedure A Condition I; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 123
123
ASTM D785
Tensile Strength, Yield 71.7 MPa
10400 psi
chs 2 in/min; ASTM D638
Flexural Modulus 3.45 GPa
500 ksi
Tangent, chs 0.05 in/min; ASTM D790
Izod Impact, Notched 0.214 J/cm
0.400 ft-lb/in
0.125 inch bar; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 88.9 °C
192 °F
Unannealed/Conditioned 48 hours at 23°C; ASTM D648
Vicat Softening Point 101 °C
214 °F
0.125 inch bar, 1 Kg; ASTM D1525
Flammability, UL94 HB
HB
0.0625 in
Optical Properties Metric English Comments
Haze 1.9 %
1.9 %
ASTM D1003
Transmission, Visible 89 %
89 %
ASTM D1003