Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 2.4 g/10 min @Load 5.00 kg, Temperature 200 °C |
2.4 g/10 min @Load 11.0 lb, Temperature 392 °F |
Procedure A Condition G; ASTM D1238 |
Network Polymers SAN 290 Light Blue Tint Description: SAN - Styrene Acrylonitrile Transparent Engineering ThermoplasticInformation provided by Network Polymers Inc. |
|||
Melt Flow | 2.4 - 3.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.4 - 3.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1283/L |
NIZHNEKAMSKNEFTEKHIM PE 4050Q (50403) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Melt Flow | 2.4 g/10 min @Load 5.00 kg, Temperature 200 °C |
2.4 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Ravago Manufacturing Americas Hylac® GP74 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Melt Flow | 2.4 g/10 min @Load 2.16 kg, Temperature 230 °C |
2.4 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Kuraray SEPTON® S2007 Thermoplastic Rubber SEPTON® is a series of high performance thermoplastic rubbers developed by Kuraray Co. Ltd. using its isoprene technology. SEPTON® resins are hydrogenated styrenic block copolymers, which exhi.. |
|||
Melt Flow | 2.4 g/10 min @Load 6.60 kg, Temperature 295 °C |
2.4 g/10 min @Load 14.6 lb, Temperature 563 °F |
ASTM D 1238 |
SABIC Innovative Plastics Ultem LTX300A PEI Copolymer (Europe-Africa-Middle East) High flow Polyetherimide blend with low toxicity, smoke and flame evolution. ECO Compliant, UL94 V0 listing in recognized colors.This data was supplied by SABIC-IP for the Europe-Africa-Middle East.. |
|||
Melt Flow | 2.4 g/10 min @Load 6.60 kg, Temperature 295 °C |
2.4 g/10 min @Load 14.6 lb, Temperature 563 °F |
ASTM D 1238 |
SABIC Innovative Plastics Ultem UR9076LG PEI Standard flow mineral filled Polyetherimide Blend. Restricted sales to GE Specialty Film & Sheet.This data was supplied by SABIC-IP for the Americas region. |
|||
Melt Flow | 2.4 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.4 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
DuPont Performance Polymers Delrin® 127UV NC010 Acetal (POM)
(Unverified Data**) UV Stabilized High Viscosity Acetal HomopolymerDelrin 127UV is a high viscosity acetal homopolymer with UV stabilizers developed for automotive interior applications. It has improvements in UV aging.. |
|||
Melt Flow | 2.4 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.4 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
DuPont Performance Polymers Delrin® 150 NC010 Acetal (POM)
(Unverified Data**) Nucleated High Viscosity Acetal Homopolymer Developed for Extrusion Delrin 150 NC010 is a high viscosity acetal homopolymer for extrusion processes. It has excellent thermal stability low die deposi.. |
|||
Melt Flow | 2.4 g/10 min @Load 5.00 kg, Temperature 200 °C |
2.4 g/10 min @Load 11.0 lb, Temperature 392 °F |
ISO 1133 |
Denka TE-30 Transparent Resin Polymer (MABS resin) ABS "TX Polymer" (methyl methacrylate styrene), MS resins as an alternative to acrylic resins, with low density, low moisture absorption, and good moldability, "TH Polymer/TP Polymer," MBS resins with a.. |
|||
Melt Flow | 2.4 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.4 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
DuPont Performance Polymers Delrin® 111P NC010 Acetal Homopolymer Delrin® 111P is a high viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage, fewer voids). It has higher tensile strength and mod.. |
|||
Melt Flow | 2.4 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.4 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
DuPont Performance Polymers Delrin® FG150 NC010 Acetal (POM)
(Unverified Data**) High Viscosity Acetal Homopolymer Developed for Food Contact ApplicationsDelrin FG150 NC010 is a high viscosity acetal homopolymer for extrusion processes. It has low die deposit and low porosity. I.. |
|||
Melt Flow | 2.4 - 5.2 g/10 min @Load 5.00 kg, Temperature 190 °C |
2.4 - 5.2 g/10 min @Load 11.0 lb, Temperature 374 °F |
ISO 1133 |
BASF Ecovio® C2224 F Blend Biodegradable Polyester Description: Ecovio® F Blend C2224 is our biodegradable film product containing renewable resources. It is basically a compound of our biodegradable copolyester Ecoflex® F Blend and polylactic aci.. |
|||
Melt Flow | 2.4 g/10 min @Load 3.80 kg, Temperature 230 °C |
2.4 g/10 min @Load 8.38 lb, Temperature 446 °F |
Pellets; ASTM D-1238-94a |
Multibase Multi-ABS 1030 White Data provided by Multibase. |