Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 17 g/10 min @Load 5.00 kg, Temperature 220 °C |
17 g/10 min @Load 11.0 lb, Temperature 428 °F |
ISO 1133 |
SABIC Innovative Plastics Cycolac® S157 ABS (Europe-Africa-Middle East) CYCOLAC S157 is a high flow flame retardant ABS with good processability developed for applications requiring UL94 V0 at reduced wall thickness.This data was supplied by SABIC-IP for the Europe-Afri.. |
|||
Melt Flow | 17 g/10 min @Load 5.00 kg, Temperature 220 °C |
17 g/10 min @Load 11.0 lb, Temperature 428 °F |
ISO 1133 |
SABIC Innovative Plastics Cycolac® S701 ABS (Europe-Africa-Middle East) CYCOLAC S701 is a new developed ABS providing a superior balance of properties. Its wide processing window, excellent flow and good mechanical properties give this material an excellent fit in appli.. |
|||
Melt Flow | 17 g/10 min @Load 5.00 kg, Temperature 260 °C |
17 g/10 min @Load 11.0 lb, Temperature 500 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Cycoloy® CY200FC PC+ABS (Europe-Africa-Middle East) High flow PC+ABS material designed for local Pacific Automotive applicationsThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Melt Flow | 17 g/10 min @Load 1.20 kg, Temperature 300 °C |
17 g/10 min @Load 2.65 lb, Temperature 572 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Lexan® EXRL0682 PC Copolymer 18 MFR LEXAN High Flow Ductile CopolymerThis data was supplied by SABIC-IP for the Americas region. |
|||
Melt Flow | 17 g/10 min @Load 2.16 kg, Temperature 190 °C |
17 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Iran Petrochemical (PCC) I1 HA 7260 High Density Polyethylene I1 (HA 7260) is a high density polyethylene with propylene as comonomer. It is very easy flowing, high density, hardness and stiffness, largely warpage free, for mass product articles in rapid shot .. |
|||
Melt Flow | 17 g/10 min @Load 5.00 kg, Temperature 210 °C |
17 g/10 min @Load 11.0 lb, Temperature 410 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL WCP700 PPE-TPE Flexible PPE-TPE injection grade suitable for over-molding applications such as plugs, strain relief's, and connectors. Good processability. 70 Shore A hardness. |
|||
Melt Flow | 17 g/10 min @Load 5.00 kg, Temperature 210 °C |
17 g/10 min @Load 11.0 lb, Temperature 410 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL WCP700 PPE-TPE (Asia Pacific) Flexible PPE-TPE injection grade suitable for over-molding applications such as plugs, strain relief's, and connectors. Good processability. 70 Shore A hardness. |
|||
Melt Flow | 17 g/10 min @Load 2.16 kg, Temperature 250 °C |
17 g/10 min @Load 4.76 lb, Temperature 482 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL WCP921 PPE-TPE Flexible Noryl* injection molding grade. Low specific gravity with good non-halogenated flame retardant performance. Developed for evaluation in overmolding applications such as plugs, strain relief.. |
|||
Melt Flow | 17 g/10 min @Load 2.16 kg, Temperature 250 °C |
17 g/10 min @Load 4.76 lb, Temperature 482 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL WCP921 PPE-TPE (Asia Pacific) Flexible Noryl* injection molding grade. Low specific gravity with good non-halogenated flame retardant performance. Developed for evaluation in overmolding applications such as plugs, strain relief.. |
|||
Melt Flow | 17 g/10 min @Load 1.20 kg, Temperature 300 °C |
17 g/10 min @Load 2.65 lb, Temperature 572 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics PC1800 PC PC1800 resin is a medium-high flow (MFR = 18 at 300ºC/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold .. |
|||
Melt Flow | 17 g/10 min @Load 1.20 kg, Temperature 300 °C |
17 g/10 min @Load 2.65 lb, Temperature 572 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics PC1800 PC (Asia Pacific) PC1800 resin is a medium-high flow (MFR = 18 at 300ºC/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold .. |
|||
Melt Flow | 17 g/10 min @Load 1.20 kg, Temperature 300 °C |
17 g/10 min @Load 2.65 lb, Temperature 572 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics PC1800 PC (Europe-Africa-Middle East) PC1800 resin is a medium-high flow (MFR = 18 at 300ºC/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold .. |
|||
Melt Flow | 17 g/10 min @Load 1.20 kg, Temperature 300 °C |
17 g/10 min @Load 2.65 lb, Temperature 572 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics PC1800R PC (Asia Pacific) PC1800R resin is a medium-high flow (MFR = 18 at 300ºC/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.This data was suppli.. |
|||
Melt Flow | 17 g/10 min @Load 1.20 kg, Temperature 300 °C |
17 g/10 min @Load 2.65 lb, Temperature 572 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics PC1800R PC (Europe-Africa-Middle East) PC1800R resin is a medium-high flow (MFR = 18 at 300ºC/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.This data was suppli.. |
|||
Melt Flow | 17 g/10 min @Load 1.20 kg, Temperature 300 °C |
17 g/10 min @Load 2.65 lb, Temperature 572 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics PC1803R PC PC1803R resin is a medium-high flow (MFR = 18 at 300ºC/1.2kg), heat and UV stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.This data was.. |
|||
Melt Flow | 17 g/10 min @Load 5.00 kg, Temperature 360 °C |
17 g/10 min @Load 11.0 lb, Temperature 680 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Ultem HU1000E PEI (Europe-Africa-Middle East) Transparent, standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (.. |
|||
Melt Flow | 17 g/10 min @Load 5.00 kg, Temperature 265 °C |
17 g/10 min @Load 11.0 lb, Temperature 509 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Xenoy® 364 PBT This data was supplied by SABIC-IP for the Americas region. |
|||
Melt Flow | 17 g/10 min @Load 1.20 kg, Temperature 266 °C |
17 g/10 min @Load 2.65 lb, Temperature 511 °F |
ASTM D 1238 |
SABIC Innovative Plastics Xenoy® X6125 PBT+PC Unreinforced, impact modified, thermoplastic alloy (PBT+PC). High impact strength while retaining mechanical and thermal properties.This data was supplied by SABIC-IP for the Americas region. |
|||
Melt Flow | 17 g/10 min @Load 5.00 kg, Temperature 260 °C |
17 g/10 min @Load 11.0 lb, Temperature 500 °F |
ISO 1133 |
Styron Pulse® A35-105 PC/ABS PULSE™ A35-105 engineering resins give exceptional impact strength even at low temperatures and have high heat distortion temperature.Information provided by DowThis product line was spun off f.. |
|||
Melt Flow | 17 g/10 min @Load 2.16 kg, Temperature 250 °C |
17 g/10 min @Load 4.76 lb, Temperature 482 °F |
ASTM D1238 |
SABIC Innovative Plastics Valox® 451E PBT (Europe-Africa-Middle East) VALOX 451E is 20% glass reinforced, flame retardant PBT injection moulding resin. |
|||
Melt Flow | 17 g/10 min @Load 21.6 kg, Temperature 220 °C |
17 g/10 min @Load 47.6 lb, Temperature 428 °F |
ISO 1133 |
Styrolution Terlux® HD 2822 MABS Terlux® HD 2822 is a new standard-injection molding grade based on a MABS polymer. Terlux® HD 2822 offers a well balanced combination of stiffness and toughness and the high transparency well .. |
|||
Melt Flow | 17 g/10 min @Load 5.00 kg, Temperature 260 °C |
17 g/10 min @Load 11.0 lb, Temperature 500 °F |
ISO 1133 |
Styron Pulse® 920 MG PC/ABS An inherently matt medium heat, medium impact PC/ABS resin, PULSE™ 920 MG is designed for interior automotive applications where a matt aesthetic is required.Information provided by DowThis pro.. |
|||
Melt Flow | 17 g/10 min @Load 21.6 kg, Temperature 190 °C |
17 g/10 min @Load 47.6 lb, Temperature 374 °F |
ISO 1133 |
Unipetrol PE HD LITEN® BB 29 HDPE Made for blow molding, extrusion, and pipe applications.Information provided by Unipetrol RPA |
|||
Melt Flow | 17 g/10 min @Load 21.6 kg, Temperature 190 °C |
17 g/10 min @Load 47.6 lb, Temperature 374 °F |
ISO 1133 |
Unipetrol PE HD LITEN® BB 85 HDPE Made for blow molding, extrusion, and pipe applications.Information provided by Unipetrol RPA |
|||
Melt Flow | 17 g/10 min @Load 2.16 kg, Temperature 190 °C |
17 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Unipetrol PE HD LITEN® FB 29 HDPE Made for tubular film applications.Information provided by Unipetrol RPA |
|||
Melt Flow | 17 g/10 min @Load 2.16 kg, Temperature 190 °C |
17 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Unipetrol PE HD LITEN® FB 85 HDPE Made for tubular film applications.Information provided by Unipetrol RPA |
|||
Melt Flow | 17 g/10 min @Load 2.16 kg, Temperature 190 °C |
17 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Unipetrol PE HD LITEN® VL 20 HDPE Extrusion and pipe applications.Information provided by Unipetrol RPA |
|||
Melt Flow | 17 g/10 min @Load 5.00 kg, Temperature 250 °C |
17 g/10 min @Load 11.0 lb, Temperature 482 °F |
ASTM D648 |
Aclo Acculoy PCA083L Polycarbonate ABS Alloy |
|||
Melt Flow | 17 g/10 min @Load 21.6 kg, Temperature 190 °C |
17 g/10 min @Load 47.6 lb, Temperature 374 °F |
ISO 1133 |
Unipetrol PE HD LITEN® VL 20 N HDPE Made for blow molding, extrusion, and pipe applications.Information provided by Unipetrol RPA |
|||
Melt Flow | 17 g/10 min @Load 21.6 kg, Temperature 190 °C |
17 g/10 min @Load 47.6 lb, Temperature 374 °F |
ASTM-D1238 |
Braskem BS600 HDPE Blow Molding Polyethylene Copolymer BS600 resin is a high-density polyethylene (HDPE), bimodal copolymer offering an outstanding combination of impact resistance and environmental stress crack resistance (ESCR). It is thus recommended.. |