SABIC Innovative Plastics NORYL WCP921 PPE-TPE (Asia Pacific)

Category Polymer , Thermoplastic , Elastomer, TPE , Polyphenylene Ether/PPO
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Noryl
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics NORYL WCP921 PPE-TPE (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Flexible Noryl* injection molding grade. Low specific gravity with good non-halogenated flame retardant performance. Developed for evaluation in overmolding applications such as plugs, strain reliefs, and connectors. UL 94 V-0 performance with good processability.
Physical Properties Metric English Comments
Specific Gravity 1.04 g/cc
1.04 g/cc
ASTM D792
Water Absorption 0.060 %

@Time 173000 sec
0.060 %

@Time 48.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0055 cm/cm

@Time 86400 sec
0.0055 in/in

@Time 24.0 hour
ASTM D955
Linear Mold Shrinkage, Transverse 0.0065 cm/cm

@Time 86400 sec
0.0065 in/in

@Time 24.0 hour
ASTM D955
Melt Flow 15 g/10 min

@Load 5.00 kg,
Temperature 210 °C
15 g/10 min

@Load 11.0 lb,
Temperature 410 °F
ASTM D1238
17 g/10 min

@Load 2.16 kg,
Temperature 250 °C
17 g/10 min

@Load 4.76 lb,
Temperature 482 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 88
88
30S reading; ASTM D2240
Tensile Strength at Break 15.0 MPa
2180 psi
Type I, 50 mm/min; ASTM D638
15.0 MPa
2180 psi
50 mm/min; ISO 527
Elongation at Break 140 %
140 %
50 mm/min; ISO 527
150 %
150 %
Type I, 50 mm/min; ASTM D638
Flexural Modulus 0.180 GPa
26.1 ksi
12.5 mm/min, 100 mm span; ASTM D790
0.200 GPa
29.0 ksi
12.5 mm/min; ISO 178
Thermal Properties Metric English Comments
Brittleness Temperature <= -40.0 °C
<= -40.0 °F
ASTM D746
Flammability, UL94 V-0

@Thickness 6.00 mm
V-0

@Thickness 0.236 in
UL 94
Oxygen Index 24 %
24 %
ISO 4589
Glow Wire Test 725 °C
1340 °F
IEC 60695-2-13
850 °C

@Thickness 3.00 mm
1560 °F

@Thickness 0.118 in
IEC 60695-2-12
Electrical Properties Metric English Comments
Volume Resistivity 7.10e+15 ohm-cm
7.10e+15 ohm-cm
ASTM D257
Dielectric Constant 2.8

@Frequency 1.00e+6 Hz
2.8

@Frequency 1.00e+6 Hz
IEC 60250
Dielectric Strength 25.0 kV/mm

@Thickness 2.00 mm
635 kV/in

@Thickness 0.0787 in
in oil; IEC 60243-1
Dissipation Factor 0.029

@Frequency 1.00e+6 Hz
0.029

@Frequency 1.00e+6 Hz
IEC 60250
Comparative Tracking Index 600 V
600 V
IEC 60112