Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 9.0 g/10 min @Load 5.00 kg, Temperature 220 °C |
9.0 g/10 min @Load 11.0 lb, Temperature 428 °F |
ISO 1133 |
SABIC Innovative Plastics Cycolac® FR23 ABS Flame retardant ABS (non-PBBE additives). Good properties/toughness. Excellent moldability. UL94 V-0 rated. |
|||
Melt Flow | 9.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
9.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Premix Thermoplastics PRE-ELEC® PP 1383 PRE-ELEC PP 1383 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELE.. |
|||
Melt Flow | 9.0 g/10 min @Load 2.16 kg, Temperature 260 °C |
9.0 g/10 min @Load 4.76 lb, Temperature 500 °F |
ASTM D1238 |
SABIC Innovative Plastics Cycoloy® CX7720 PC+ABS (Asia Pacific) Cycoloy resin CX7720 is a non brominated and non chlorinated flame retardant PC/ABS resin grade featuring high heat resistance and thin wall FR. It is UL-94 listed at 1.2 mm V0 and 1.5mm 5VB. Its hi.. |
|||
Melt Flow | 9.0 g/10 min @Load 5.00 kg, Temperature 260 °C |
9.0 g/10 min @Load 11.0 lb, Temperature 500 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Geloy XTWM206 ASA (Europe-Africa-Middle East) Next generation ASA optimized for outstanding weatherability, colorability and higher heat applications requiring UV exposure resistance.This data was supplied by SABIC-IP for the Europe-Africa-Midd.. |
|||
Melt Flow | 9.0 - 12.6 g/10 min @Load 21.6 kg, Temperature 190 °C |
9.0 - 12.6 g/10 min @Load 47.6 lb, Temperature 374 °F |
Flow@21.6kg/Flow@5kg ratio > 18; ASTM D1283 |
NIZHNEKAMSKNEFTEKHIM PE 6749F (486H6) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Melt Flow | 9.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
9.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Lexan® EXL1413T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1413T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers excellent low temperature (-30 °C) ductility in combination with medium f.. |
|||
Melt Flow | 9.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
9.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Lexan® EXL1463T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1463T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers excellent low temperature (-30 C) ductility in combination with medium flow ch.. |
|||
Melt Flow | 9.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
9.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Lexan® EXL1493T PC Copolymer Lexan* EXL1493T polycarbonate (PC) siloxane copolymer resin is an injection molding grade with FDA and EU food contact compliance, with mold release. This resin offers excellent low temperature (-3.. |
|||
Melt Flow | 9.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
9.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Lexan® FXD1433T PC Copolymer (Europe-Africa-Middle East) Clear PC-siloxane copolymer with excellent processability in special light diffusion colors. Medium flow, UV stabilized. Improved toughness compared to standard PC in same color. Color package may .. |
|||
Melt Flow | 9.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
9.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Lexan® FXG1414T PC Copolymer (Europe-Africa-Middle East) PC-siloxane copolymer in special "Diamond Sparkle" colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance.This data was supp.. |
|||
Melt Flow | 9.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
9.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Lexan® HPM1944 PC Medium flow specialty polycarbonate with enhanced hemocompatibility. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). .. |
|||
Melt Flow | 9.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
9.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Lexan® ML6430 PC Copolymer Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colorsThis data was supplied by SABIC-IP for the Americas re.. |
|||
Melt Flow | 9.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
9.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Lexan® SLX1431D PC Copolymer (Europe-Africa-Middle East) Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. Available in diffusion colors.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Melt Flow | 9.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
9.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Lexan® SLX1432T PC Copolymer (Europe-Africa-Middle East) Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. Available in transparent and tinted colors.This data was supplied by SABIC-IP for the Europe-Africa-Middle East .. |
|||
Melt Flow | 9.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
9.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Lexan® SLX2431T PC Copolymer (Europe-Africa-Middle East) Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colorsThis data was supplied by SABIC-IP for the Europe-Afri.. |
|||
Melt Flow | 9.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
9.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Lexan® SLX2432D PC Copolymer (Europe-Africa-Middle East) Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. V2 rated. Available in diffusion colors.This data was supplied by SABIC-IP for the Europe-Africa-Middle East reg.. |
|||
Melt Flow | 9.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
9.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Lexan® SLX2432T PC Copolymer (Europe-Africa-Middle East) Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colors.This data was supplied by SABIC-IP for the Europe-Africa-M.. |
|||
Melt Flow | 9.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
9.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics PC1000 PC PC1000 resin is a medium-low flow (MFR = 10 at 300ºC/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold r.. |
|||
Melt Flow | 9.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
9.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics PC1000R PC PC1000R resin is a medium-low flow (MFR = 10 at 300ºC/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.This data was supplie.. |
|||
Melt Flow | 9.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
9.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics PC1000R PC (Europe-Africa-Middle East) PC1000R resin is a medium-low flow (MFR = 10 at 300ºC/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.This data was supplie.. |
|||
Melt Flow | 9.0 g/10 min @Load 1.20 kg, Temperature 250 °C |
9.0 g/10 min @Load 2.65 lb, Temperature 482 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics PC6300 PC (Europe-Africa-Middle East) PC6300 resin is a very high flow (MFR = 9.5 at 250ºC/1.2kg) polycarbonate product designed for use in the optical media market.This data was supplied by SABIC-IP for the Europe-Africa-Middle East.. |
|||
Melt Flow | 9.0 g/10 min @Load 1.20 kg, Temperature 265 °C |
9.0 g/10 min @Load 2.65 lb, Temperature 509 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Xenoy® 6380U PBT+PET (Asia Pacific) XENOY 6380U is a 30% glass reinforced, UV stabilized grade, that combines high stiffness with improved ductility. The combination of mechanical properties at high and low temperatures and chemical r.. |
|||
Melt Flow | 9.0 g/10 min @Load 10.0 kg, Temperature 220 °C |
9.0 g/10 min @Load 22.0 lb, Temperature 428 °F |
ISO 1133 |
Styrolution Novodur® 4140PG ABS Novodur Ultra 4140PG is a PC modified plating grade combining high heat resistance and excellent impact strength with the unique surface properties of a Novodur ABS material.Information provided by .. |
|||
Melt Flow | 9.0 g/10 min @Load 5.00 kg, Temperature 280 °C |
9.0 g/10 min @Load 11.0 lb, Temperature 536 °F |
ASTM D 1238 |
SABIC Innovative Plastics Noryl GTX GTX977 PPE+PA66 Noryl GTX GTX977 resin is a mineral reinforced conductive Noryl GTX with a improved CTE (7) with a balanced performance of Impact and stiffness. (developmental grade : EXNX0074)This data was supplie.. |
|||
Melt Flow | 9.0 g/10 min @Load 2.16 kg, Temperature 250 °C |
9.0 g/10 min @Load 4.76 lb, Temperature 482 °F |
ASTM D1238 |
SABIC Innovative Plastics Valox® SHF4960 PBT (Europe-Africa-Middle East) Valox Super high flow grade, 30% glass filled Flame retardant, High CTI, heat stabilized with mold release. |
|||
Melt Flow | 9.0 g/10 min @Load 2.16 kg, Temperature 280 °C |
9.0 g/10 min @Load 4.76 lb, Temperature 536 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Noryl GTX GTX4110 PPE+PA66 Non-brominated, non-chorinated Flame Retardant PPE/PA66 alloy, 10% glass reinforced. Combines ductility, modulus and high CTI with dimensional stability.This data was supplied by SABIC-IP for the A.. |
|||
Melt Flow | 9.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
9.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
cm³/10min; ISO 1133 |
DuPont Performance Polymers Delrin® 500TE NC010 Acetal (POM)
(Unverified Data**) Toughened Medium Viscosity Acetal Homopolymer with Very Low Emissions Delrin 500TE NC010 (formerly DE20560) is a medium viscosity toughened acetal homopolymer with very low VOC emissions. Processing.. |
|||
Melt Flow | 9.0 g/10 min @Load 2.16 kg, Temperature 220 °C |
9.0 g/10 min @Load 4.76 lb, Temperature 428 °F |
cm³/10min; ISO 1133 |
DuPont Performance Polymers Hytrel® 4068 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D High Performance Polyester Elastomer with Non-discoloring StabilizerInformation provided by DuPont Performance Polymers |
|||
Melt Flow | 9.0 g/10 min @Load 5.00 kg, Temperature 190 °C |
9.0 g/10 min @Load 11.0 lb, Temperature 374 °F |
ISO 1133 |
Unipetrol PE HD LITEN® MB/ML 47 HDPE Made for injection molding and special applicationsInformation provided by Unipetrol RPA |
|||
Melt Flow | 9.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
9.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Lexan® SLX1482T PC Copolymer (Europe-Africa-Middle East) Medium viscosity PC Copolymer, enhanced UV stabilization. Transprarent and tinted colors. Higher mold release content than SLX1432T.This data was supplied by SABIC-IP for the Europe-Africa-Middle E.. |