Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 78 g/10 min @Load 10.0 kg, Temperature 220 °C |
78 g/10 min @Load 22.0 lb, Temperature 428 °F |
ISO 1133 |
SABIC Innovative Plastics Cycolac® INP564 ABS SABIC INP564 provides compatibility with a wider range of ABS grades than many color concentrate bases; allows better dispersion than pellets; allows concentrate manufacturers to produce both pellet.. |
|||
Melt Flow | 78 g/10 min @Load 10.0 kg, Temperature 220 °C |
78 g/10 min @Load 22.0 lb, Temperature 428 °F |
ISO 1133 |
SABIC Innovative Plastics Cycolac® INP564 ABS+SAN SABIC INP564 provides compatibility with a wider range of ABS grades than many color concentrate bases; allows better dispersion than pellets; allows concentrate manufacturers to produce both pellet.. |
|||
Melt Flow | 78 g/10 min @Load 10.0 kg, Temperature 220 °C |
78 g/10 min @Load 22.0 lb, Temperature 428 °F |
ISO 1133 |
SABIC Innovative Plastics Cycolac® INP576 ABS Can be used as compounding additives for polymer blends. Medium molecular weight SAN. Can be blended with high rubber graft modifier resins to produce customized ABS properties. Suitable for direc.. |
|||
Melt Flow | 78 g/10 min @Load 10.0 kg, Temperature 220 °C |
78 g/10 min @Load 22.0 lb, Temperature 428 °F |
ISO 1133 |
SABIC Innovative Plastics Cycolac® INP576 ABS+SAN Can be used as compounding additives for polymer blends. Medium molecular weight SAN. Can be blended with high rubber graft modifier resins to produce customized ABS properties. Suitable for direc.. |
|||
Melt Flow | 78 g/10 min @Load 10.0 kg, Temperature 220 °C |
78 g/10 min @Load 22.0 lb, Temperature 428 °F |
ISO 1133 |
SABIC Innovative Plastics Cycolac® S157 ABS (Europe-Africa-Middle East) CYCOLAC S157 is a high flow flame retardant ABS with good processability developed for applications requiring UL94 V0 at reduced wall thickness.This data was supplied by SABIC-IP for the Europe-Afri.. |
|||
Melt Flow | 78 g/10 min @Load 1.20 kg, Temperature 300 °C |
78 g/10 min @Load 2.65 lb, Temperature 572 °F |
Procedure A Condition 0; ASTM D1238 |
Network Polymers NPP 808 C2WW Description: Polycarbonate AlloyInformation provided by Network Polymers Inc. |
|||
Melt Flow | 78 g/10 min @Load 1.20 kg, Temperature 300 °C |
78 g/10 min @Load 2.65 lb, Temperature 572 °F |
Procedure A Condition 0; ASTM D1238 |
Network Polymers NPP 908 Description: Polyester CopolymerInformation provided by Network Polymers Inc. |
|||
Melt Flow | 78 - 96 g/10 min @Load 21.6 kg, Temperature 190 °C |
78 - 96 g/10 min @Load 47.6 lb, Temperature 374 °F |
Flow@21.6kg/Flow@2.16kg ratio < 30; ASTM D1283 |
NIZHNEKAMSKNEFTEKHIM PE 4116Q (16403) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Melt Flow | 78 - 96 g/10 min @Load 21.6 kg, Temperature 190 °C |
78 - 96 g/10 min @Load 47.6 lb, Temperature 374 °F |
Flow@21.6kg/Flow@2.16kg ratio < 30; ASTM D1283 |
NIZHNEKAMSKNEFTEKHIM PE 4118Q (18403) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Melt Flow | 78 g/10 min @Pressure 0.655 MPa |
78 g/10 min @Pressure 95.0 psi |
Severs Efflux; Geon® 1010 |
PolyOne Geon™ 120 Series 129 Polyvinyl Chloride Homopolymer The value set forth represent typical values and PolyOne Corporation, therefore, makes no representation that the material in any particular shipment will conform to the listed properties. Packaging.. |
|||
Melt Flow | 78 - 96 g/10 min @Load 21.6 kg, Temperature 190 °C |
78 - 96 g/10 min @Load 47.6 lb, Temperature 374 °F |
Flow@21.6kg/Flow@2.16kg ratio < 30; ASTM D1283 |
NIZHNEKAMSKNEFTEKHIM PE 4318Q (18403) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Melt Flow | 78 g/10 min @Load 1.20 kg, Temperature 300 °C |
78 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
Diamond Polymers NPP 60-908 Polyester Copolymer Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Melt Flow | 78 g/10 min @Load 1.20 kg, Temperature 300 °C |
78 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
Diamond Polymers NPP 808 C2 Polycarbonate Alloy, Natural Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Melt Flow | 78 g/10 min @Load 1.20 kg, Temperature 300 °C |
78 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
Diamond Polymers NPP 808 C2 TDS Polycarbonate Alloy, Natural Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |