Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 5.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
5.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Polimeri Europa Eraclene® MM 84 High Density Polyethylene - Injection Molding Eraclene MM 84 is a high density polyethylene resin (HDPE) with antioxidants, suitable for injection molding application.Eraclene MM 84 is characterized by high rigidity and good impact resistance. .. |
|||
Melt Flow | 5.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
5.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D 1238 |
SABIC Innovative Plastics Lexan® EXL1036 PC Copolymer Lexan* EXL1036 polycarbonate (PC) siloxane copolymer resin is a UV stabilized high viscosity grade designed for (co-)extrusion. This resin offers extreme low temperature (-60 C) ductility and good h.. |
|||
Melt Flow | 5.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
5.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D 1238 |
SABIC Innovative Plastics Lexan® EXL1036 PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1036 polycarbonate (PC) siloxane copolymer resin is a UV stabilized high viscosity grade designed for (co-)extrusion. This resin offers extreme low temperature (-60 C) ductility and good h.. |
|||
Melt Flow | 5.5 - 11 g/10 min @Load 2.16 kg, Temperature 230 °C |
5.5 - 11 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Solvay Specialty Polymers Solef® 6008 Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Solef® 6008 PVDF homopolymer is a low-viscosity PVDF resin and is typically processed by injection molding.Information provided by Solvay Specialty Polymers. |
|||
Melt Flow | 5.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
5.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
EVALCA EVAL® LC-E105A Ethylene Vinyl Alcohol Copolymer Resin
(discontinued **) 44 mol % Ethylene.Data provided by EVALCA. Applications: Cast film, melt phase forming, solid phase pressure forming, tubes, coex coating. EVOH is used in packaging applications because of its out.. |
|||
Melt Flow | 5.5 g/10 min @Load 2.16 kg, Temperature 230 °C |
5.5 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
LyondellBasell Moplen HP400L Polypropylene Homopolymer Description: All ingredients in HP400L meet the chemical registration requirements of TSCA (U.S.) and DSL (Canada). Uses: Toys, containers, lids, medical applications, closure capsInformation provid.. |
|||
Melt Flow | 5.5 - 11 g/10 min @Load 2.16 kg, Temperature 230 °C |
5.5 - 11 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Solvay Specialty Polymers Solef® 6008 Polyvinylidene Fluoride (PVDF) Solef® 6008 PVDF homopolymer is a low-viscosity PVDF resin and is typically processed by injection molding.Features: Homopolymer; Low ViscosityAdditional Properties: Crystallization Heat - ASTM D.. |
|||
Melt Flow | 5.5 g/10 min @Load 10.0 kg, Temperature 220 °C |
5.5 g/10 min @Load 22.0 lb, Temperature 428 °F |
ISO 1133 |
Styrolution Luran® S 797 SE ASA Luran S 797 SE is an extrusion ASA grade with especially high notched impact strength, used for sheet and profile extrusions. The data representable is based on extruded sheet.Information provided .. |
|||
Melt Flow | 5.5 g/10 min @Load 2.16 kg, Temperature 230 °C |
5.5 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Topas Advanced Polymers TOPAS® 9506F-500 Cyclic Olefin Copolymer (COC) TOPAS® 9506F-500 is a high clarity extrusion grade for use in shrink, food and medical packaging as either a discrete layer in multilayer film or in blends with polyethylene. It is designed to del.. |
|||
Melt Flow | 5.5 g/10 min @Load 21.6 kg, Temperature 190 °C |
5.5 g/10 min @Load 47.6 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil HDPE BA53-055 High Density Polyethylene Resin Product Description: BA53-055 is a high molecular weight, high density polyethylene copolymer.Availability: Latin America, North America and South America Additive: Antistatic: NoApplications: Dru.. |
|||
Melt Flow | 5.5 g/10 min @Load 21.6 kg, Temperature 190 °C |
5.5 g/10 min @Load 47.6 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil HDPE BU46-055 High Density Polyethylene Resin Product Description: BU46-055 is a high molecular weight, high density polyethylene copolymer which contains a UV inhibitor. It possesses a combination of excellent processability, outstanding melt .. |
|||
Melt Flow | 5.5 g/10 min @Load 5.00 kg, Temperature 200 °C |
5.5 g/10 min @Load 11.0 lb, Temperature 392 °F |
ISO 1133 |
Denka TP-801 Transparent Resin Polymer (MBS resin) Polymethacrylate Butadiene Styrene "TX Polymer" (methyl methacrylate styrene), MS resins as an alternative to acrylic resins, with low density, low moisture absorption, and good moldability, "TH Polymer/TP Polymer," MBS resins with a.. |
|||
Melt Flow | 5.5 g/10 min @Load 3.80 kg, Temperature 230 °C |
5.5 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
Diamond Polymers Diamaloy ABS VP-22 Flame Retardant ABS Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Melt Flow | 5.5 g/10 min @Load 3.80 kg, Temperature 230 °C |
5.5 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
Diamond Polymers DIAMALOY VP22 Flame Retardant ABS Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Melt Flow | 5.5 g/10 min @Load 3.80 kg, Temperature 230 °C |
5.5 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
Techmer ES Plastiblend® APC100 UV Availability: North AmericaForms: PelletsAdditive: UV StabilizerFeatures: Good UV ResistanceInformation provided by TP Composites, Inc. |
|||
Melt Flow | 5.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
5.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Polimeri Europa Eraclene® MM 84 U High Density Polyethylene - Injection Molding Eraclene MM 84 U is a gas phase high density polyethylene resin (HDPE) with antioxidants, suitable for injection molding application.Eraclene MM 84 U is characterized by high rigidity and good impac.. |
|||
Melt Flow | 5.5 g/10 min @Load 3.80 kg, Temperature 230 °C |
5.5 g/10 min @Load 8.38 lb, Temperature 446 °F |
Cond. I; ASTM D1238 |
Polimeri Europa SINKRAL L320 ABS
(discontinued **) Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,095-25-16-25 General purpose, high flow injection moulding grade having good impact resistance coupled with an .. |