Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 5.4 g/10 min @Load 21.6 kg, Temperature 190 °C |
5.4 g/10 min @Load 47.6 lb, Temperature 374 °F |
ISO 1133 |
SABIC FI0644 Bimodal High Density Polyethylene for Blown Film Product Description: FI0644 is a high molecular weight high density polyethylene copolymer grade specifically designed for blown film applications. Its high molecular weight, broad molecular weigh.. |
|||
Melt Flow | 5.4 g/10 min @Load 5.00 kg, Temperature 200 °C |
5.4 g/10 min @Load 11.0 lb, Temperature 392 °F |
Procedure A Condition G; ASTM D1238 |
Network Polymers Softflex® 5000 Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc. |
|||
Melt Flow | 5.4 - 9.0 g/10 min @Load 21.6 kg, Temperature 190 °C |
5.4 - 9.0 g/10 min @Load 47.6 lb, Temperature 374 °F |
Flow@21.6kg/Flow@5kg ratio > 18; ASTM D1283 |
NIZHNEKAMSKNEFTEKHIM PE 6250D (506H4) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Melt Flow | 5.4 g/10 min @Load 21.6 kg, Temperature 190 °C |
5.4 g/10 min @Load 47.6 lb, Temperature 374 °F |
ISO 1133 |
Iran Petrochemical (PCC) EX 6HT HM 9455 HT High Density Polyethylene EX 6HT is a high density polyethylene with 1-Butene as co monomer. It has good toughness, low gel level, good tear strength, high tenacity.Applications: film extrusion, blending partner, refuse ba.. |
|||
Melt Flow | 5.4 g/10 min @Load 3.80 kg, Temperature 230 °C |
5.4 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
Diamond Polymers ASA S124 ASA Weatherable Polymers Injection Molding Grade, Medium Modulus Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Melt Flow | 5.4 g/10 min @Load 3.80 kg, Temperature 230 °C |
5.4 g/10 min @Load 8.38 lb, Temperature 446 °F |
Procedure A Condition I; ASTM D1238 |
Diamond Polymers ASA S210 Description: ASA Weatherable Polymer, Injection Molding Grade, Medium ModulusInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 5.4 g/10 min @Load 3.80 kg, Temperature 230 °C |
5.4 g/10 min @Load 8.38 lb, Temperature 446 °F |
Procedure A Condition I; ASTM D1238 |
Diamond Polymers ASA S210B Description: ASA Weatherable Polymer, Injection Molding Grade, Medium ModulusInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 5.4 g/10 min @Load 3.80 kg, Temperature 230 °C |
5.4 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
Diamond Polymers ASA S-210E ASA Weatherable Polymers Extrusion Molding Grade, Medium Modulus Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |