Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 45 - 65 g/10 min @Load 5.00 kg, Temperature 200 °C |
45 - 65 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
PolyOne Versaflex™ OM 1245X-1 Thermoplastic Elastomer (TPE) The Versaflex™ OM 1245X-1 is designed for overmolding onto polycarbonate (PC), ABS, and PC/ABS susbstrates. - Excellent Bond to PC, ABS, PC/ABS - Rubbery Feel - Soft TouchColor concentrates with EV.. |
|||
Melt Flow | 45 g/10 min @Load 5.00 kg, Temperature 260 °C |
45 g/10 min @Load 11.0 lb, Temperature 500 °F |
ASTM D 1238 |
SABIC Innovative Plastics Cycoloy® CX7510 PC+ABS Cycoloy* CX7510 resin is an injection moldable, flame retardant PC/ABS blend, with non-chlorinated & non-brominated flame retardants. Key features of Cycoloy CX7510 resin include high heat, high flo.. |
|||
Melt Flow | 45 g/10 min @Load 5.00 kg, Temperature 260 °C |
45 g/10 min @Load 11.0 lb, Temperature 500 °F |
ASTM D 1238 |
SABIC Innovative Plastics Cycoloy® CX7510 PC+ABS (Asia Pacific) Cycoloy* CX7510 resin is an injection moldable, flame retardant PC/ABS blend, with non-chlorinated & non-brominated flame retardants. Key features of Cycoloy CX7510 resin include high heat, high flo.. |
|||
Melt Flow | 45 g/10 min @Load 5.00 kg, Temperature 260 °C |
45 g/10 min @Load 11.0 lb, Temperature 500 °F |
ASTM D 1238 |
SABIC Innovative Plastics Cycoloy® CX7510 PC+ABS (Europe-Africa-Middle East) Cycoloy* CX7510 resin is an injection moldable, flame retardant PC/ABS blend, with non-chlorinated & non-brominated flame retardants. Key features of Cycoloy CX7510 resin include high heat, high flo.. |
|||
Melt Flow | 45 g/10 min @Load 1.20 kg, Temperature 300 °C |
45 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D 1238 |
SABIC Innovative Plastics Lexan® ML7677A PC (Asia Pacific) Commercial grade for Polycarbonate in only nature color. Excellent processability, super high flow, flame retardant, UL rated V-1 at 2.0mm.This data was supplied by SABIC-IP for the Asia Pacific reg.. |
|||
Melt Flow | 45 g/10 min @Load 1.20 kg, Temperature 300 °C |
45 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® ML7686 PC (Asia Pacific) Transparent Polycarbonate in limited colors. Excellent processability, super high flow. UL rated V-2 at 1.5mm. |
|||
Melt Flow | 45 g/10 min @Load 1.20 kg, Temperature 300 °C |
45 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® ML7686 PC (Europe-Africa-Middle East) Transparent Polycarbonate in limited colors. Excellent processability, super high flow. UL rated V-2 at 1.5mm. |
|||
Melt Flow | 45 g/10 min @Load 1.20 kg, Temperature 300 °C |
45 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® ML7686E PC (Europe-Africa-Middle East) Transparent Polycarbonate in natural color. Excellent processability, super high flow. UL compliant 94V-2 at 1.5mm. |
|||
Melt Flow | 45 g/10 min @Load 21.6 kg, Temperature 190 °C |
45 g/10 min @Load 47.6 lb, Temperature 374 °F |
ISO 1133 |
Polimeri Europa Eraclene® PF 92 High Density Polyethylene - Pipe Grade Resin Eraclene PF 92 is a homopolymer high density polyethylene resin (HDPE) with antioxidants, suitable for pipe application. It is characterized by high rigidity, high impact strength and low swelling... |
|||
Melt Flow | 45 g/10 min @Load 1.20 kg, Temperature 300 °C |
45 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® EXRL1061 PC (Asia Pacific) Transparent Polycarbonate in natural color. Excellent processability, super high flow. |
|||
Melt Flow | 45 g/10 min @Load 5.00 kg, Temperature 265 °C |
45 g/10 min @Load 11.0 lb, Temperature 509 °F |
ASTM D1238 |
SABIC Innovative Plastics Valox® 8032UX PBT+PET (Europe-Africa-Middle East) VALOX 8032UX is a 30% glass fibre reinforced, UV stabilized PBT+PET blend with excellent surface finish. This grade is VALOX 8032U with improved weathering resistance. Applications: appliance housin.. |
|||
Melt Flow | 45 g/10 min @Load 5.00 kg, Temperature 266 °C |
45 g/10 min @Load 11.0 lb, Temperature 511 °F |
ASTM D1238 |
SABIC Innovative Plastics Valox® 8032UX PBT+PET (Europe-Africa-Middle East) VALOX 8032UX is a 30% glass fibre reinforced, UV stabilized PBT+PET blend with excellent surface finish. This grade is VALOX 8032U with improved weathering resistance. Applications: appliance housin.. |
|||
Melt Flow | 45 g/10 min @Load 5.00 kg, Temperature 265 °C |
45 g/10 min @Load 11.0 lb, Temperature 509 °F |
ASTM D1238 |
SABIC Innovative Plastics Valox® 830 PBT (Europe-Africa-Middle East) VALOX 830 is a 30% glass fibre reinforced PBT+PET blend with excellent surface finish. Applications: hot air gun housing assemblies, industrial glue guns, appliance housings and handles. |
|||
Melt Flow | 45 g/10 min @Load 5.00 kg, Temperature 280 °C |
45 g/10 min @Load 11.0 lb, Temperature 536 °F |
ASTM D 1238 |
SABIC Innovative Plastics Noryl GTX GTX918WR PPE+PS+PA (Asia Pacific) High flow PPE+PS+PA for under-the-hood and electrical applications. With mold releaseThis data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Melt Flow | 45 g/10 min @Load 2.16 kg, Temperature 220 °C |
45 g/10 min @Load 4.76 lb, Temperature 428 °F |
ASTM D1238 |
Lubrizol Estane® UB310 Thermoplastic Polyurethane Type: Estane® UB310 is a Shore 95A, polyester based, hot melt adhesive with excellent low temperature flexibility thermoplastic polyurethane (TPU).Uses: Extrusion, Powder Coating, Ideal for Fire Ho.. |
|||
Melt Flow | 45 g/10 min @Load 5.00 kg, Temperature 230 °C |
45 g/10 min @Load 11.0 lb, Temperature 446 °F |
ISO 1133 |
Borealis Daplen™ EE137AI Polypropylene Compound 10% Mineral Filled Daplen EE137AI is a 10% mineral filled grade intended for injection molding. EE137AI has been developed especially for the car industry, to be used in interior parts where high scratch resistance i.. |
|||
Melt Flow | 45 g/10 min @Load 5.00 kg, Temperature 230 °C |
45 g/10 min @Load 11.0 lb, Temperature 446 °F |
Volume Resistivity 1000 ohm-cm |
TIMCAL ENSACO™ 250G Conductive Carbon Black ENSACO™ & SUPER P™ conductive carbon blacks are carbon blacks with a high to very high void volume allowing the retention of a carbon network at low to very low filler content. The void volume can.. |
|||
Melt Flow | 45 g/10 min @Load 10.0 kg, Temperature 220 °C |
45 g/10 min @Load 22.0 lb, Temperature 428 °F |
ISO-1133 |
Chi Mei Polylac® PA-756 ABS - High Flow High rigid, high flow |
|||
Melt Flow | >= 45 g/10 min @Load 10.0 kg, Temperature 400 °C |
>= 45 g/10 min @Load 22.0 lb, Temperature 752 °F |
|
BASF Ultrason® E 2010 C6 30% Carbon Filled Carbon fibers and Ultrason® two partners with good properties. The combination of carbon fibers with the amorphous high-temperature plastic Ultrason® guarantees mechanical properties for temperatu.. |