Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 1.2 g/10 min @Load 3.80 kg, Temperature 230 °C |
1.2 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
SABIC Innovative Plastics Cycolac® MG29 ABS Super high impact ABS. Good low temperature toughness. High gloss. |
|||
Melt Flow | 1.2 g/10 min @Load 3.80 kg, Temperature 230 °C |
1.2 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
SABIC Innovative Plastics Cycolac® MG29 ABS (Asia Pacific) Super high impact ABS. Good low temperature toughness. High gloss. |
|||
Melt Flow | 1.2 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.2 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Premix Thermoplastics PRE-ELEC® PP 1397 Conductive Thermoplastic Compound PRE-ELEC® PP 1397 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-E.. |
|||
Melt Flow | 1.2 - 1.9 g/10 min @Load 5.00 kg, Temperature 230 °C |
1.2 - 1.9 g/10 min @Load 11.0 lb, Temperature 446 °F |
ASTM D1283/L |
NIZHNEKAMSKNEFTEKHIM PP 8332C (EPD60R) Propylene and Ethylene Block Polymer Product obtained by copolymerization of propylene with ethylene in presence of complex metalorganic catalysts. It incorporates increased long-term thermal stability, thermal-oxidative degradation r.. |
|||
Melt Flow | 1.2 g/10 min @Load 5.00 kg, Temperature 230 °C |
1.2 g/10 min @Load 11.0 lb, Temperature 446 °F |
ASTM D1238 |
Solvay Specialty Polymers Solef® 1015/0078 PVDF Homopolymer
(discontinued **) Key features of this grade: Plasticized, Offshore, Piping, Formulated. Recommended processing is extrusion. Available as granules.General information about SOLEF® PVDF: SOLEF® PVDF is a fluorina.. |
|||
Melt Flow | 1.2 g/10 min @Load 5.00 kg, Temperature 230 °C |
1.2 g/10 min @Load 11.0 lb, Temperature 446 °F |
ASTM D1238 |
Solvay Specialty Polymers Solef® 61010 PVDF Copolymer
(discontinued **) Key features of this grade: Permanent Plasticizing, Fuel Line, Piping, Formulated. Recommended processing is extrusion. Available as granules.General information about SOLEF® PVDF: SOLEF® PVDF i.. |
|||
Melt Flow | 1.2 - 1.6 g/10 min @Load 5.00 kg, Temperature 190 °C |
1.2 - 1.6 g/10 min @Load 11.0 lb, Temperature 374 °F |
ASTM D1238 |
Forever Plast Namtene® Recycled Standard HDPE Standard Namtene® is used for dimple sheet, plastic slabs, and agricultural and construction applications. |
|||
Melt Flow | 1.2 g/10 min @Load 5.00 kg, Temperature 190 °C |
1.2 g/10 min @Load 11.0 lb, Temperature 374 °F |
ISO 1133 |
Iran Petrochemical (PCC) BL3 HF 4760 High Density Polyethylene BL3 is a high density polyethylene with 1-Butene as co monomer. It is high density and stiffness, good ESCR, high rigidity, good flowability and impact strength.Applications: small blow molding, bo.. |
|||
Melt Flow | 1.2 g/10 min @Load 5.00 kg, Temperature 200 °C |
1.2 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Kingfa FRABS V-0 Flame Retardant ABS Features:UL 94 V-0 @ 1.5-3.0mmHigh toughnessFor extrusion moldingApplications:PlateElectric and electronic cabinetPCB boardInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Melt Flow | 1.2 g/10 min @Load 5.00 kg, Temperature 190 °C |
1.2 g/10 min @Load 11.0 lb, Temperature 374 °F |
ISO 1133 |
Borealis Borstar® FB3450 HDPE for Film Extrusion Borstar® FB3450 is a high density polyethylene. Borstar® FB3450 is well suited for multilayer coextruded films where higher stiffness and toughness than in standard LDPE and LLDPE is required. Ap.. |
|||
Melt Flow | 1.2 g/10 min @Load 5.00 kg, Temperature 190 °C |
1.2 g/10 min @Load 11.0 lb, Temperature 374 °F |
ISO 1133 |
Unipetrol PE HD LITEN® BB 29 H HDPE Made for blow molding, extrusion, and pipe applications.Information provided by Unipetrol RPA |
|||
Melt Flow | 1.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Total HDPE BM961 High Density Polyethylene, High Gloss Blow Molding Resin Polyethylene: High density High Gloss Blow Molding ResinCharacteristics:High GlossHigh stiffnessGood abrasion resistanceFDA CompliantApplications:Coextruded glossy bottlesBlending agent for other p.. |
|||
Melt Flow | 1.2 g/10 min @Load 5.00 kg, Temperature 200 °C |
1.2 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Chi Mei Polylac® PA-747 ABS High impact |
|||
Melt Flow | 1.2 g/10 min @Load 10.0 kg, Temperature 220 °C |
1.2 g/10 min @Load 22.0 lb, Temperature 428 °F |
Procedure A; ASTM D1238 |
Diamond Polymers ABS 3003 MC Description: High Heat Plating GradeInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 1.2 g/10 min @Load 5.00 kg, Temperature 265 °C |
1.2 g/10 min @Load 11.0 lb, Temperature 509 °F |
Procedure A; ASTM D1238 |
Diamond Polymers ABS 4011 HH Description: Ultra High Heat ABSInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 1.2 g/10 min @Load 5.00 kg, Temperature 200 °C |
1.2 g/10 min @Load 11.0 lb, Temperature 392 °F |
Procedure A Condition G; ASTM D1238 |
Diamond Polymers ABS 9502 Description: Injection Molding Grade, Ultra High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 1.2 g/10 min @Load 5.00 kg, Temperature 200 °C |
1.2 g/10 min @Load 11.0 lb, Temperature 392 °F |
Procedure A Condition G; ASTM D1238 |
Diamond Polymers ABS/PC 7901 Description: Injection Molding Grade, High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 1.2 g/10 min @Load 5.00 kg, Temperature 230 °C |
1.2 g/10 min @Load 11.0 lb, Temperature 446 °F |
ASTM D1238 |
Carmel Olefins CARMELTECH™ QB 79 P Polypropylene Random Copolymer for Pressure Pipe CARMELTECH™ QB 79 P is a high molecular weight, low melt flow rate polypropylene random copolymer, especially designed for extrusion of pressure pipes and injection molding of fittings. This grade .. |