Physical Properties | Metric | English | Comments |
---|---|---|---|
Water Vapor Transmission | 15.0 g/m²/day | 0.966 g/100 in²/day | ASTM 1249 |
DuPont™ Clysar® EZ Polyolefin Shrink Packaging Film, 60 Gauge
(discontinued **) Data provided by DuPont Packaging Polymers.A strong, clear, biaxially oriented, heat-shrinkable, multilayer film. Clysar®EZS is a high slip version of EZ. Used where a premium product appearance i.. |
|||
Water Vapor Transmission | 15.0 g/m²/day | 0.966 g/100 in²/day | ASTM 1249 |
DuPont™ Clysar® EZ Polyolefin Shrink Packaging Film, 75 Gauge
(discontinued **) Data provided by DuPont Packaging Polymers.A strong, clear, biaxially oriented, heat-shrinkable, multilayer film. Clysar®EZS is a high slip version of EZ. Used where a premium product appearance i.. |
|||
Water Vapor Transmission | 15.0 g/m²/day | 0.966 g/100 in²/day | Average value: 15.0 g/m²/day Grade Count:4 |
Overview of materials for Polycarbonate, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Extruded". Each property range of values reported is minimum and maximum values of approp.. |
|||
Water Vapor Transmission | 15.0 g/m²/day | 0.966 g/100 in²/day | Average value: 15.0 g/m²/day Grade Count:3 |
Overview of materials for Polycarbonate, Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Unreinforced, Flame Retardant". Each property range of values reported is minimum and max.. |
|||
Water Vapor Transmission | 15.0 g/m²/day | 0.966 g/100 in²/day | Average value: 15.0 g/m²/day Grade Count:11 |
Overview of materials for Polycarbonate, UV Stabilized This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, UV Stabilized". Each property range of values reported is minimum and maximum values of a.. |
|||
Water Vapor Transmission | 15.0 g/m²/day @Thickness 0.100 mm |
0.966 g/100 in²/day @Thickness 0.00394 in |
85% RH, film; ISO 15106-1 |
Covestro Makrolon® 2256 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Food contact quality•.. |
|||
Water Vapor Transmission | 15.0 g/m²/day @Thickness 0.100 mm |
0.966 g/100 in²/day @Thickness 0.00394 in |
85% RH, film; ISO 15106-1 |
Covestro Makrolon® 2400 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low.. |
|||
Water Vapor Transmission | 15.0 g/m²/day @Thickness 0.100 mm |
0.966 g/100 in²/day @Thickness 0.00394 in |
85% RH, film; ISO 15106-1 |
Covestro Makrolon® 2407 MAS070 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low.. |
|||
Water Vapor Transmission | 15.0 g/m²/day @Thickness 0.100 mm |
0.966 g/100 in²/day @Thickness 0.00394 in |
85% RH, film; ISO 15106-1 |
Covestro Makrolon® 2407 MAS145 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low.. |
|||
Water Vapor Transmission | 15.0 g/m²/day @Thickness 0.100 mm |
0.966 g/100 in²/day @Thickness 0.00394 in |
85% RH, film; ISO 15106-1 |
Covestro Makrolon® 2600 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med.. |
|||
Water Vapor Transmission | 15.0 g/m²/day @Thickness 0.100 mm |
0.966 g/100 in²/day @Thickness 0.00394 in |
85% RH, film; ISO 15106-1 |
Covestro Makrolon® 2652 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Food contact quality•.. |
|||
Water Vapor Transmission | 15.0 g/m²/day @Thickness 0.100 mm |
0.966 g/100 in²/day @Thickness 0.00394 in |
85% RH, film; ISO 15106-1 |
Covestro Makrolon® 2665 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Medium viscosity, easy.. |
|||
Water Vapor Transmission | 15.0 g/m²/day @Thickness 0.100 mm |
0.966 g/100 in²/day @Thickness 0.00394 in |
85% RH, film; ISO 15106-1 |
Covestro Makrolon® 2667 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Flame retardant• Med.. |
|||
Water Vapor Transmission | 15.0 g/m²/day @Thickness 0.100 mm |
0.966 g/100 in²/day @Thickness 0.00394 in |
85% RH, film; ISO 15106-1 |
Covestro Makrolon® 2800 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med.. |
|||
Water Vapor Transmission | 15.0 g/m²/day @Thickness 0.100 mm |
0.966 g/100 in²/day @Thickness 0.00394 in |
85% RH, film; ISO 15106-1 |
Covestro Makrolon® 2805 MAS152 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med.. |
|||
Water Vapor Transmission | 15.0 g/m²/day @Thickness 0.100 mm |
0.966 g/100 in²/day @Thickness 0.00394 in |
85% RH, film; ISO 15106-1 |
Covestro Makrolon® 3100 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Hig.. |
|||
Water Vapor Transmission | 15.0 g/m²/day @Thickness 0.100 mm |
0.966 g/100 in²/day @Thickness 0.00394 in |
85% RH, film; ISO 15106-1 |
Covestro Makrolon® 3107 MAS167 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Hig.. |
|||
Water Vapor Transmission | 15.0 g/m²/day @Thickness 0.100 mm |
0.966 g/100 in²/day @Thickness 0.00394 in |
85% RH, film; ISO 15106-1 |
Covestro Makrolon® ET3117 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Extrusion• High visc.. |
|||
Water Vapor Transmission | 15.0 g/m²/day | 0.966 g/100 in²/day | 23°C/85%r.h.; DIS 15106-1/-2 |
EMS-Grivory Grivory® CF 6 S PA* Product description: Grilon CF 6 S is an extracted copolyamide with a low melting point. Very high flexibility and toughnessVery good thermoforming and orientation propertiesHigh shrinkVery good tra.. |
|||
Water Vapor Transmission | 15.0 g/m²/day | 0.966 g/100 in²/day | 23°C/85%r.h.; DIS 15106-1/-2 |
EMS-Grivory Grivory® CR 8 PA* Product description: Grilon CR 8 is a Copolyamide. Grilon CR 8 shows the following features: High flexibility and toughnessGood thermoforming and orientation propertiesHigh shrinkageGood transparen.. |
|||
Water Vapor Transmission | 15.0 g/m²/day | 0.966 g/100 in²/day | 23°C/85%r.h.; DIS 15106-1/-2 |
EMS-Grivory Grivory® CR 9 HV PA* Product description: Grilon CR 9 HV is a high viscosity copolyamide with low temperature. Grilon CR9 HV has the following features:High flexibility and toughnessGood thermoforming and orientation pr.. |
|||
Water Vapor Transmission | 15.0 g/m²/day | 0.966 g/100 in²/day | 23°C/85%r.h.; DIS 15106-1/-2 |
EMS-Grivory Grivory® CR 9 PA* Product description: Grilon CR 9 is a copolyamide with low melting temperature. Grilon CR 9 shows the following features: High flexibility and toughnessGood thermoforming and orientation propertiesH.. |
|||
Water Vapor Transmission | 15.0 g/m²/day | 0.966 g/100 in²/day | 23°C/85%r.h.; DIS 15106-1/-2 |
EMS-Grivory Grivory® F 47 H NL nat 6020 PA6 Product description: Grilon F 47 HNL natural 6020 is a nucleated, high viscosity polyamide 6. This product exhibits the following features: Good mechanical propertiesGood barrier against oils and fa.. |
|||
Water Vapor Transmission | 15.0 g/m²/day @Thickness 0.100 mm |
0.966 g/100 in²/day @Thickness 0.00394 in |
85% RH, film; ISO 15106-1 |
Covestro Makrolon® ET2613 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Extrusion• Medium vi.. |
|||
Water Vapor Transmission | 15.0 g/m²/day @Thickness 0.100 mm |
0.966 g/100 in²/day @Thickness 0.00394 in |
85% RH, film; ISO 15106-1 |
Covestro Makrolon® ET3127 Polycarbonate Makrolon® polycarbonate resinMain characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characterist.. |
|||
Water Vapor Transmission | 15.0 g/m²/day @Thickness 0.100 mm |
0.966 g/100 in²/day @Thickness 0.00394 in |
85% RH, film; ISO 15106-1 |
Covestro Makrolon® ET3227 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Extrusion• High visc.. |
|||
Water Vapor Transmission | 15.0 g/m²/day | 0.966 g/100 in²/day | 23°C/85%r.h.; DIS 15106-1/-2 |
EMS-Grivory Grivory® F 40 NL PA6 Product description: Grilon F 40 NL natural 6018 is a nucleated and lubricated high viscosity polyamide 6. This product exhibits the following features: Good gas barrierGood mechanical propertiesGoo.. |
|||
Water Vapor Transmission | 15.0 g/m²/day | 0.966 g/100 in²/day | ASTM E96 Procedure E |
DuPont Teijin Films Mylar® HS Polyester Film, 150 Gauge (38 µm) Data provided by DuPont Packaging Polymers.An uncoated, transparent polyester packaging film designed for heat shrink applications. It is currently available in 48, 65, 80, and 150 gauges, and othe.. |
|||
Water Vapor Transmission | 15.0 g/m²/day @Thickness 0.100 mm |
0.966 g/100 in²/day @Thickness 0.00394 in |
85% RH, film; ISO 15106-1 |
Covestro Makrolon® LQ2647 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Optical lens, safety g.. |
|||
Water Vapor Transmission | 15.0 g/m²/day | 0.966 g/100 in²/day | 23°C/85%r.h.; DIS 15106-1/-2 |
EMS-Grivory Grivory® F 50 nat 6368 PA6 Product description: Grilon F 50 natural 6368 is a modified, very high viscous Polyamide 6 for extrusion processes: Very high melt strengthGood chemical resistanceGood gas-barrierGood mechanical pro.. |