Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 102 - 114 microns | 4.00 - 4.50 mil | with adhesive |
3M Scotchcal™ 50-1 Graphic Film Film series 50 is a 3-mil calendered vinyl film, available in 28 colors. The film has a clear, pressure-sensitive film with a blue liner on the white films for easier visibility when wedding, and a .. |
|||
Thickness | 102 - 114 microns | 4.00 - 4.50 mil | with adhesive |
3M Scotchcal™ 50-10 Graphic Film Film series 50 is a 3-mil calendered vinyl film, available in 28 colors. The film has a clear, pressure-sensitive film with a blue liner on the white films for easier visibility when wedding, and a .. |
|||
Thickness | 102 - 114 microns | 4.00 - 4.50 mil | with adhesive |
3M Scotchcal™ 50-12 Graphic Film Film series 50 is a 3-mil calendered vinyl film, available in 28 colors. The film has a clear, pressure-sensitive film with a blue liner on the white films for easier visibility when wedding, and a .. |
|||
Thickness | 102 - 114 microns | 4.00 - 4.50 mil | with adhesive |
3M Scotchcal™ 50--120 Graphic Film Film series 50 is a 3-mil calendered vinyl film, available in 28 colors. The film has a clear, pressure-sensitive film with a blue liner on the white films for easier visibility when wedding, and a .. |
|||
Thickness | 102 - 114 microns | 4.00 - 4.50 mil | with adhesive |
3M Scotchcal™ 50-24 Graphic Film Film series 50 is a 3-mil calendered vinyl film, available in 28 colors. The film has a clear, pressure-sensitive film with a blue liner on the white films for easier visibility when wedding, and a .. |
|||
Thickness | 102 - 114 microns | 4.00 - 4.50 mil | with adhesive |
3M Scotchcal™ 50-27 Graphic Film Film series 50 is a 3-mil calendered vinyl film, available in 28 colors. The film has a clear, pressure-sensitive film with a blue liner on the white films for easier visibility when wedding, and a .. |
|||
Thickness | 102 - 114 microns | 4.00 - 4.50 mil | with adhesive |
3M Scotchcal™ 50-44 Graphic Film Film series 50 is a 3-mil calendered vinyl film, available in 28 colors. The film has a clear, pressure-sensitive film with a blue liner on the white films for easier visibility when wedding, and a .. |
|||
Thickness | 102 - 114 microns | 4.00 - 4.50 mil | with adhesive |
3M Scotchcal™ 50-483 Graphic Film Film series 50 is a 3-mil calendered vinyl film, available in 28 colors. The film has a clear, pressure-sensitive film with a blue liner on the white films for easier visibility when wedding, and a .. |
|||
Thickness | 102 - 114 microns | 4.00 - 4.50 mil | with adhesive |
3M Scotchcal™ 50-49 Graphic Film Film series 50 is a 3-mil calendered vinyl film, available in 28 colors. The film has a clear, pressure-sensitive film with a blue liner on the white films for easier visibility when wedding, and a .. |
|||
Thickness | 102 - 114 microns | 4.00 - 4.50 mil | with adhesive |
3M Scotchcal™ 50-54 Graphic Film Film series 50 is a 3-mil calendered vinyl film, available in 28 colors. The film has a clear, pressure-sensitive film with a blue liner on the white films for easier visibility when wedding, and a .. |
|||
Thickness | 102 - 114 microns | 4.00 - 4.50 mil | with adhesive |
3M Scotchcal™ 50-64 Graphic Film Film series 50 is a 3-mil calendered vinyl film, available in 28 colors. The film has a clear, pressure-sensitive film with a blue liner on the white films for easier visibility when wedding, and a .. |
|||
Thickness | 102 - 114 microns | 4.00 - 4.50 mil | with adhesive |
3M Scotchcal™ 50-73 Graphic Film Film series 50 is a 3-mil calendered vinyl film, available in 28 colors. The film has a clear, pressure-sensitive film with a blue liner on the white films for easier visibility when wedding, and a .. |
|||
Thickness | 102 - 114 microns | 4.00 - 4.50 mil | with adhesive |
3M Scotchcal™ 50-745 Graphic Film Film series 50 is a 3-mil calendered vinyl film, available in 28 colors. The film has a clear, pressure-sensitive film with a blue liner on the white films for easier visibility when wedding, and a .. |
|||
Thickness | 102 - 114 microns | 4.00 - 4.50 mil | with adhesive |
3M Scotchcal™ 50-76 Graphic Film Film series 50 is a 3-mil calendered vinyl film, available in 28 colors. The film has a clear, pressure-sensitive film with a blue liner on the white films for easier visibility when wedding, and a .. |
|||
Thickness | 102 - 114 microns | 4.00 - 4.50 mil | with adhesive |
3M Scotchcal™ 50-79 Graphic Film Film series 50 is a 3-mil calendered vinyl film, available in 28 colors. The film has a clear, pressure-sensitive film with a blue liner on the white films for easier visibility when wedding, and a .. |
|||
Thickness | 102 - 114 microns | 4.00 - 4.50 mil | with adhesive |
3M Scotchcal™ 50-84 Graphic Film Film series 50 is a 3-mil calendered vinyl film, available in 28 colors. The film has a clear, pressure-sensitive film with a blue liner on the white films for easier visibility when wedding, and a .. |
|||
Thickness | 102 - 114 microns | 4.00 - 4.50 mil | with adhesive |
3M Scotchcal™ 50-88 Graphic Film Film series 50 is a 3-mil calendered vinyl film, available in 28 colors. The film has a clear, pressure-sensitive film with a blue liner on the white films for easier visibility when wedding, and a .. |
|||
Thickness | 102 - 114 microns | 4.00 - 4.50 mil | with adhesive |
3M Scotchcal™ 50-90 Graphic Film Film series 50 is a 3-mil calendered vinyl film, available in 28 colors. The film has a clear, pressure-sensitive film with a blue liner on the white films for easier visibility when wedding, and a .. |
|||
Thickness | 102 - 114 microns | 4.00 - 4.50 mil | with adhesive |
3M Scotchcal™ 50-914 Graphic Film Film series 50 is a 3-mil calendered vinyl film, available in 28 colors. The film has a clear, pressure-sensitive film with a blue liner on the white films for easier visibility when wedding, and a .. |
|||
Thickness | 102 - 114 microns | 4.00 - 4.50 mil | with adhesive |
3M Scotchcal™ 50-94 Graphic Film Film series 50 is a 3-mil calendered vinyl film, available in 28 colors. The film has a clear, pressure-sensitive film with a blue liner on the white films for easier visibility when wedding, and a .. |
|||
Thickness | 102 - 114 microns | 4.00 - 4.50 mil | with adhesive |
3M Scotchcal™ 50-97 Graphic Film Film series 50 is a 3-mil calendered vinyl film, available in 28 colors. The film has a clear, pressure-sensitive film with a blue liner on the white films for easier visibility when wedding, and a .. |
|||
Thickness | 38.1 - 114 microns | 1.50 - 4.50 mil | Side 2 |
Arlon 47091R012 0.012" (0.305 mm) Uncured Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured RubberSide 2: Uncured RubberAppearance: Red silicone gum on polymer linerThis data represents typical values for the production material. The data should not be u.. |
|||
Thickness | 63.5 - 114 microns | 2.50 - 4.50 mil | Side 1 |
Arlon 51971R015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone Rubber Appearance: Red gum on glass fiber fabricThis data Represents typical values for the production material. The data .. |
|||
Thickness | 63.5 - 114 microns | 2.50 - 4.50 mil | Side 2 |
Arlon 51971R015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone Rubber Appearance: Red gum on glass fiber fabricThis data Represents typical values for the production material. The data .. |
|||
Thickness | 102 - 114 microns | 4.00 - 4.50 mil | with adhesive |
3M Scotchcal™ 50-100 Graphic Film Film series 50 is a 3-mil calendered vinyl film, available in 28 colors. The film has a clear, pressure-sensitive film with a blue liner on the white films for easier visibility when wedding, and a .. |
|||
Thickness | 102 - 114 microns | 4.00 - 4.50 mil | with adhesive |
3M Scotchcal™ 50-34 Graphic Film Film series 50 is a 3-mil calendered vinyl film, available in 28 colors. The film has a clear, pressure-sensitive film with a blue liner on the white films for easier visibility when wedding, and a .. |
|||
Thickness | 102 - 114 microns | 4.00 - 4.50 mil | with adhesive |
3M Scotchcal™ 50-58 Graphic Film Film series 50 is a 3-mil calendered vinyl film, available in 28 colors. The film has a clear, pressure-sensitive film with a blue liner on the white films for easier visibility when wedding, and a .. |
|||
Thickness | 102 - 114 microns | 4.00 - 4.50 mil | with adhesive |
3M Scotchcal™ 50-78 Graphic Film Film series 50 is a 3-mil calendered vinyl film, available in 28 colors. The film has a clear, pressure-sensitive film with a blue liner on the white films for easier visibility when wedding, and a .. |
|||
Thickness | 102 - 114 microns | 4.00 - 4.50 mil | with adhesive |
3M Scotchcal™ 50-82 Graphic Film Film series 50 is a 3-mil calendered vinyl film, available in 28 colors. The film has a clear, pressure-sensitive film with a blue liner on the white films for easier visibility when wedding, and a .. |
|||
Thickness | 102 - 114 microns | 4.00 - 4.50 mil | with adhesive |
3M Scotchcal™ 50-92 Graphic Film Film series 50 is a 3-mil calendered vinyl film, available in 28 colors. The film has a clear, pressure-sensitive film with a blue liner on the white films for easier visibility when wedding, and a .. |