Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

3M Scotchcal™ 50-54 Graphic Film

Category Polymer , Film
Manufacturer 3M
Trade Name ScotchCal™
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF 3M Scotchcal™ 50-54 Graphic Film.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Film series 50 is a 3-mil calendered vinyl film, available in 28 colors. The film has a clear, pressure-sensitive film with a blue liner on the white films for easier visibility when wedding, and a white liner on all other film colors. Use this versatile film in both indoor and outdoor applications for thermal mass transfer and electronic cutting. It is removable with heat for up to three years and permanent for up to five years. This 3-mil film may be printed with thermal mass transfer and electronically cut.Information provided by 3M
Physical Properties Metric English Comments
Thickness 76.2 microns
3.00 mil
without adhesive
102 - 114 microns
4.00 - 4.50 mil
with adhesive
Mechanical Properties Metric English Comments
Tensile Strength at Break >= 18.4 MPa
>= 2670 psi
Peel Strength 0.526 kN/m
3.00 pli
Adhesion to Glass
0.701 kN/m
4.00 pli
Adhesion to Acrylic
0.701 kN/m
4.00 pli
Adhesion to Fruehauf pre-painted panel
0.701 kN/m
4.00 pli
Adhesion to Polycarbonate
0.877 kN/m
5.00 pli
Adhesion to Alodine, aluminum
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 38.0 °C
100 °F
Minimum Service Temperature, Air 4.00 °C
39.2 °F
Descriptive Properties Value Comments
Appearance Gold
Users viewing this material also viewed the following: