Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 25.4 - 254 microns | 1.00 - 10.0 mil | Average value: 127 microns Grade Count:7 |
Overview of materials for Epoxy, Electrically Conductive This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Electrically Conductive". Each property range of values reported is minimum and maximum values of.. |
|||
Thickness | 76.2 - 254 microns | 3.00 - 10.0 mil | |
Technetics Group PLASTOLON™ Low Density PTFE Tape
(Unverified Data**) Information provided by Technetics Group (formerly Plastomer Technologies) |
|||
Thickness | 203 - 254 microns | 8.00 - 10.0 mil | Overall |
Arlon 48571R009 0.009" (0.229 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured RubberSide 2: Uncured RubberThis data represents typical values for the production material. The data should not be used to write, or in place of, material specif.. |
|||
Thickness | 178 - 254 microns | 7.00 - 10.0 mil | Overall |
Arlon 910-10RXX-P0 0.010" (0.254 mm) Self-Fusing Silicone Tape Design/Construction:Cross Section Type: RectangularArlon Rectangular Tape: Rectangular tape is of uniform thickness and is ideal for applications where a smooth, even layer of tape is not required.P.. |
|||
Thickness | 203 - 254 microns | 8.00 - 10.0 mil | Overall |
Arlon 44560R009 0.009" (0.229 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone Rubber Appearance: Red silicone gum on fiberglass fabricThis data represents typical values for the production material. The data should not be used to w.. |
|||
Thickness | 25.4 - 254 microns | 1.00 - 10.0 mil | |
Technetics Group PLASTOLON™ Skived PTFE Tape
(Unverified Data**) Information provided by Technetics Group (formerly Plastomer Technologies) |