Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 457 - 559 microns | 18.0 - 22.0 mil | Overall |
Arlon 515880R020 0.020" (0.508 mm) Uncured Silicone Rubber with Fiberglass Substrate
(discontinued **)&l Design/Construction:Side 1: Uncured Silicone Rubber Appearance: Red silicone gum on fiberglass clothThis data Represents typical values for the production material. The data should not be used to wr.. |
|||
Thickness | 457 microns | 18.0 mil | Gauge, nominal |
Mid-Mountain Materials ARMATEX® FF18 Fluoroelastomer Coated Glass Fabric Description: Armatex Coatings are applied to base textiles that range in chemical composition, confiation and weight. Mid-Mountain specializes in engineered coatings, both polymer and mineral based... |
|||
Thickness | 457 - 559 microns | 18.0 - 22.0 mil | Side 1 |
Arlon 15370T020 0.020" (0.508 mm) Uncatalyzed, Unsupported Rubber on a Mylar Carrier Design/Construction:Side 1: Uncatalyzed, Unsupported Rubber on a Mylar CarrierAppearance: Translucent high viscosity gumThis data represents typical values for the production material. The data shou.. |
|||
Thickness | 457 microns | 18.0 mil | Prime Coated 162 Fiberglass, Substrate |
Arlon 55191R030 0.030" (0.762 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone Rubber Appearance: Red silicone gum on fiberglass clothThis data Represents typical values for the production material. Th.. |
|||
Thickness | 457 microns | 18.0 mil | Substrate; Arlon SQA-TMS-003 |
Arlon 55576R030 0.030" (0.762 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone Rubber Substrate: Style 162 Fiberglass Side 2: Uncured Silicone Rubber Interleave: LDPE This data represents typical values for the production material. T.. |
|||
Thickness | 457 microns | 18.0 mil | Substrate; Arlon SQA-TMS-003 |
Arlon 55576R060 0.060" Cured/Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 162 FiberglassSide 2: Uncured Silicone RubberInterleave: 3 mil PEThis data represents typical values for the production material .. |
|||
Thickness | 457 microns | 18.0 mil | Prime Coated 162 Style Fiberglass, Substrate |
Arlon 55579R043W 0.043" (1.09 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured layer on top of a cured layer on one side This data Represents typical values for the production material. The data should not be used to write, or in place of, m.. |
|||
Thickness | 457 microns | 18.0 mil | Prime Coated 162 Style Fiberglass, Substrate |
Arlon 55580R030 0.030" (0.762 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberAppearance: Red silicone gum on fiberglass clothThis data Represents typical values for the production material. The data should not be used to wri.. |
|||
Thickness | 457 microns | 18.0 mil | Prime Coated 162 Fiberglass, Substrate |
Arlon 55609R028 0.028" (0.711 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone Rubber LayerSide 2: Uncured Silicone RubberProduct Use: Flexible heater insulationAppearance: Red silicone gum on fiberglass with polymer release linersThi.. |
|||
Thickness | 457 microns | 18.0 mil | Substrate; Arlon SQA-TMS-003 |
Arlon 55759R028 0.029" (0.737 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: PolyethyleneLayer 2: Uncured Silicone Rubber Layer 1: Cured Silicone Rubber Substrate: 162 Style Fiberglass This data represents typical values for the production ma.. |
|||
Thickness | 457 microns | 18.0 mil | substrate; Arlon SQA-TMS-003 |
Arlon 55946C028 Silicone Rubber/Fiberglass Laminate Side 1: cured silicone rubber; Substrate: 162 fiberglass; Side 2: uncured silicone rubber; Interleave: 3 mil polyethylene |
|||
Thickness | 457 microns | 18.0 mil | Substrate |
Arlon 56606R026 0.027" Cured/Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 1564 FiberglassSide 2: Uncured Silicone RubberInterleave: 3 mil PEThis data represents typical values for the production materia.. |
|||
Thickness | 457 - 559 microns | 18.0 - 22.0 mil | Overall |
Arlon LW201Xxx-M1 0.020" (0.508 mm) Self-Fusing Silicone Tape (Triangular, Unsupported) with Mylar Interleave Design/Construction:Cross Section Type: TriangularArlon LevelWrap® Tape: LevelWrap® has tapered edges and a colored line along its apes. The purpose of the line is to act as a guide for subsequent.. |
|||
Thickness | 457 - 559 microns | 18.0 - 22.0 mil | Overall |
Arlon LW201Xxx-P1 0.020" (0.508 mm) Self-Fusing Silicone Tape (Triangular, Unsupported) with Poly Interleave Design/Construction:Triangular Cross Section Fusible TapeArlon LevelWrap® Tape: LevelWrap® has tapered edges and a colored line along its apes. The purpose of the line is to act as a guide for sub.. |
|||
Thickness | 457 - 559 microns | 18.0 - 22.0 mil | Overall |
Arlon LW202Bxx-P1 0.020" (0.508 mm) Self-Fusing Silicone Tape (Triangular, Unsupported) with Poly Interleave Design/Construction:Triangular Cross Section Fusible TapeArlon LevelWrap® Tape: LevelWrap® has tapered edges and a colored line along its apes. The purpose of the line is to act as a guide for sub.. |
|||
Thickness | 457 microns | 18.0 mil | Prime Coated 162 Fiberglass, Substrate |
Arlon R30651R062 0.062" (1.57 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place .. |
|||
Thickness | 457 - 559 microns | 18.0 - 22.0 mil | Overall |
Arlon R35066R020 0.020" (0.508 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place of.. |
|||
Thickness | 457 microns | 18.0 mil | Overall Thickness; Arlon SQA-TMS-003 |
Arlon 51583R018 0.018" Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave 1: 2.5 mil LDPESide 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Cured Silicone RubberInterleave 2: 2.5 mil LDPEThis data represents typical val.. |
|||
Thickness | 457 microns | 18.0 mil | Substrate |
Arlon 55359R062 62 mil Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 3 mil PELayer 2: Uncured Silicone RubberLayer 1: Cured Silicone RubberSubstrate: Style 162 FiberglassThis data represents typical values for the production materi.. |
|||
Thickness | 457 microns | 18.0 mil | Substrate; Arlon SQA-TMS-003 |
Arlon 55560R030 0.030" (0.762 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1: Uncured Silicone Rubber Substrate: Style 162 Fiberglass Appearance: Red silicone gum on fiberglass fabricThis data represents typical values for.. |
|||
Thickness | 457 microns | 18.0 mil | Substrate; Arlon SQA-TMS-003 |
Arlon 55572R028 0.028" (0.711 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 162 Fiberglass Appearance: Red silicone rubber on fiberglass clothThis data Represents typical values for the production material. T.. |
|||
Thickness | 457 microns | 18.0 mil | Substrate; Arlon SQA-TMS-003 |
Arlon 55586R040 0.040" (1.02 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone Rubber Substrate: Style 162 FiberglassSide 2: Uncured Silicone RubberInterleave: LDPEAppearance: Red silicone gum and rubber on fiberglass clothThis data .. |
|||
Thickness | 457 microns | 18.0 mil | Substrate; Arlon SQA-TMS-003 |
Arlon 55589G028 0.0295" (0.749 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: PolyethyleneLayer 2: Uncured Silicone Rubber Layer 1: Cured Silicone Rubber Substrate: 162 Style FiberglassAppearance: Green silicone gum and rubber on fiberglass Th.. |
|||
Thickness | 457 microns | 18.0 mil | Prime Coated 162 Fiberglass, Substrate |
Arlon 55949C028 0.029" (0.737 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone Rubber LayerSide 2: Uncured Silicone Rubber Appearance: Brown silicone rubber and gum on fiberglass clothThis data Represents typical values for the produc.. |
|||
Thickness | 457 microns | 18.0 mil | Side 1 |
Arlon 59463X068CT 0.068" (1.73 mm) Textured, Cured Rubber with Fiberglass Substrate Design/Construction:Side 1: Textured, Cured Rubber Side 2: Textured, Cured Rubber This data Represents typical values for the production material. The data should not be used to write, or in place o.. |
|||
Thickness | 457 - 559 microns | 18.0 - 22.0 mil | Overall |
Arlon R33889R020 0.020" (0.508 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Layer-on-Layer This data Represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information .. |
|||
Thickness | 457 microns | 18.0 mil | Prime Coated 162 Style Fiberglass, Substrate |
Arlon R34369R028 0.029" (0.737 mm) Uncured Layer on Top of a Cured Layer on One Side with Fiberglass Substrate, 38" wide Design/Construction:Side 1: Uncured Layer on Top of a Cured Layer on One SideThis data Represents typical values for the production material. The data should not be used to write, or in place of, ma.. |
|||
Thickness | 457 - 559 microns | 18.0 - 22.0 mil | Side 1 |
Arlon R34880T020 0.020" (0.508 mm) Uncatalyzed, Unsupported rubber on a Mylar Carrier Design/Construction:Side 1: Uncatalyzed, Unsupported rubber on a Mylar Carrier This data Represents typical values for the production material. The data should not be used to write, or in place of, .. |
|||
Thickness | 457 - 559 microns | 18.0 - 22.0 mil | Overall |
Arlon 44602W020 0.020" (0.508 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberProduct Use: Flexible heater insulationAppearance: White silicone rubber on fiberglassThis data represents typical values for the production material.. |
|||
Thickness | 457 microns | 18.0 mil | Prime Coated 162 Fiberglass, Substrate |
Arlon 55090R028 0.028 (0.711 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberAppearance: Red silicone gum on fiberglass fabricThis data Represents typical values for the production material. The data should not be used to wr.. |