Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 406 microns | 16.0 mil | |
Premix Thermoplastics PRE-ELEC® ABS 1410 PRE-ELEC ABS 1410 is a conductive thermoplastic compound based on ABS. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC ABS 141.. |
|||
Thickness | 406 microns | 16.0 mil | cured laminate, per ply |
Park Electrochemical Nelcote® F-502 Phenolic Prepreg, 3K 8HS PAN Reinforced Nelcote® F-502 is a MIL-R-9299 phenolic resin system suitable for impregnation on any MIL-C-9084 fabric with a compatible finish. F-502 is used in the manufacture of ablative reinforcements in rock.. |
|||
Thickness | 406 microns | 16.0 mil | |
Hexcel® HexForce™ AGP370-5H Carbon Fabric Hexcel's carbon fibers contain high strength-to-weight and stiffness-to-weight ratios. Carbon fabrics are thermally and electrically conductive and exhibit excellent fatigue resistance. When proper.. |
|||
Thickness | 406 microns | 16.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon 51366X015 0.016" (0.406 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1: Cured Silicone RubberSubstrate: Style 7628 Fiberglass Side 2: Uncured Silicone Rubber Flame Resistance: Product is designed to meet Title 14 CFR.. |
|||
Thickness | 406 microns | 16.0 mil | Layer 2; Arlon SQA-TMS-003 |
Arlon 51599R028 0.028" (0.711 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Layer 2: Uncured Silicone RubberLayer 1: Cured Silicone Rubber Substrate: Style 7628 Fiberglass Product Use: Flexible heater insulationAppearance: Red s.. |
|||
Thickness | 406 microns | 16.0 mil | Substrate; Arlon SQA-TMS-003 |
Arlon 55578R036 0.036" (0.914 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: PolyethyleneSide 2, Layer 2: Uncured Silicone Rubber Side 2, Layer 1: Cured Silicone Rubber Substrate: Style 162 Fiberglass Side 1: Cured Silicone Rubber Appearance:.. |
|||
Thickness | 406 microns | 16.0 mil | Substrate; Arlon SQA-TMS-003 |
Arlon 55578XA028 0.0280" Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: LDPESide 2 Layer 2: Uncured Silicone RubberSide 2 Layer 1: Cured Silicone RubberSubstrate: Style 162 FiberglassSide 1: Cured Silicone RubberThis data represents ty.. |
|||
Thickness | 406 microns | 16.0 mil | Substrate; Arlon SQA-TMS-003 |
Arlon 55591R062 0.062" (1.57 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: PolyethyleneSide 1: Uncured Silicone Rubber Substrate: Style 162 FiberglassSide 2: Uncured Silicone RubberInterleave 2: Polyethylene Product Use: Electrical insula.. |
|||
Thickness | 406 microns | 16.0 mil | Substrate; Arlon SQA-TMS-003 |
Arlon 55636R025 0.025" Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 3 mil PESide 2: Uncured Silicone RubberSubstrate: Style 162 FiberglassSide 1: Cured Silicone RubberThis data represents typical values for the production material .. |
|||
Thickness | 406 microns | 16.0 mil | Substrate; Arlon SQA-TMS-003 |
Arlon 55638R030 0.030" (0.762 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: PolyethyleneSide 2: Uncured Silicone Rubber Substrate: Style 162 Fiberglass Side 1: Cured Silicone Rubber Product Use: Flexible heater SubstrateAppearance: Red silic.. |
|||
Thickness | 406 microns | 16.0 mil | Substrate; Arlon SQA-TMS-003 |
Arlon 55833R062 Mar Resistant Press Pad; 1.6 mm Cured Silicone Rubber with Fiberglass Substrate Mar Resistant Press Pad - Product is sold with two finishes options: 55833R062AC - "C-finish" and 55833R062DST - "Smooth with Talc"Design/Construction:Interleave: 3 mil PESide 1: Cured Silicone Ru.. |
|||
Thickness | 406 microns | 16.0 mil | Substrate; Arlon SQA-TMS-003 |
Arlon 56106R026 0.028" (0.711 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: PolyethyleneSide 2: Uncured Silicone Rubber Substrate: 1564 Style Fiberglass Side 1: Cured Silicone Rubber Product Use: Flexible heater insulationAppearance: Red sil.. |
|||
Thickness | 406 microns | 16.0 mil | Substrate; Arlon SQA-TMS-003 |
Arlon 56810R025 0.025" (0.635 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1: Uncured Silicone Rubber Substrate: 1564 Style Fiberglass This data represents typical values for the production material. The data should not be.. |
|||
Thickness | 406 microns | 16.0 mil | Substrate; Arlon SQA-TMS-003 |
Arlon 56811B025 0.026" (0.660 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: Polyethylene Side 1: Uncured Silicone Rubber Substrate: 1564 Style Fiberglass Side 2: Uncured Silicone Rubber Interleave 2: Polyethylene Product Use: Hose and Duct.. |
|||
Thickness | 406 microns | 16.0 mil | substrate; Arlon SQA-TMS-003 |
Arlon 56976R026 Silicone Rubber/Fiberglass Laminate Interleave: 3 mil PE; Side 1: cured silicone rubber; Substrate: 1564 fiberglass; Side 2: uncured silicone rubber |
|||
Thickness | 406 microns | 16.0 mil | Substrate; Arlon SQA-TMS-003 |
Arlon 56986XA028 0.028" (0.711 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone Rubber Substrate: 1564 Style Fiberglass Side 2: Uncured Silicone Rubber Interleave: Polyethylene Product Use: Flame Resistant-flexible heater substrateApp.. |
|||
Thickness | 406 microns | 16.0 mil | Side 1; Arlon SQA-TMS-003 |
Arlon P30670R020 0.020" (0.508 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Uncured Silicone Rubber Substrate: Style 1165 FiberglassAppearance: Red silicone gum on fiberglass with polymer release linersThis data represents typical values for the.. |
|||
Thickness | 406 microns | 16.0 mil | WFT |
3M Scotchkote™ FP 812 External Wall Coating 3M Scotchkote External Wall Coating FP 812 has been specifically developed as a low maintenance, high build coating for cemetitious and plaster wall surfaces.Information provided by 3M |
|||
Thickness | 406 microns | 16.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon 51576R016A 0.016" (0.406 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1: Cured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2: Uncured Silicone Rubber This data represents typical values for the production mat.. |
|||
Thickness | 406 microns | 16.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon 51986XA015 0.016" (0.406 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone RubberSubstrate: Style 7628 Fiberglass Side 2: Uncured Silicone Rubber Interleave: Polyethylene Appearance: Gray silicone gum and rubber on fiberglass clo.. |
|||
Thickness | 406 microns | 16.0 mil | Substrate; Arlon SQA-TMS-003 |
Arlon 55272R024 0.024" (0.610 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1: Cured Silicone Rubber Substrate: Style 162 FiberglassThis data represents typical values for the production material. The data should not be use.. |
|||
Thickness | 406 microns | 16.0 mil | Substrate; Arlon SQA-TMS-003 |
Arlon 55272R028 0.028" (0.711 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1: Cured Silicone Rubber Substrate: Style 162 FiberglassThis data represents typical values for the production material. The data should not be use.. |
|||
Thickness | 406 microns | 16.0 mil | Substrate; Arlon SQA-TMS-003 |
Arlon 55279R033 0.033" (0.838 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Layer 2: Uncured Silicone Rubber Layer 1: Cured Silicone Rubber Substrate: Style 162 Fiberglass Product Use: Flexible heater insulationAppearance: Red s.. |
|||
Thickness | 406 microns | 16.0 mil | Substrate; Arlon SQA-TMS-003 |
Arlon 55638R025 0.025" (0.635 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: PolyethyleneSide 2: Uncured Silicone Rubber Substrate: Style 162 Fiberglass Side 1: Cured Silicone Rubber Product Use: Flexible heater SubstrateAppearance: Red silic.. |
|||
Thickness | 406 microns | 16.0 mil | Substrate; Arlon SQA-TMS-003 |
Arlon 56866R026 0.028" Cured/Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 1564 FiberglassSide 2: Uncured Silicone RubberInterleave: 3 mil LDPEThis data represents typical values for the production mater.. |
|||
Thickness | 406 microns | 16.0 mil | substrate; Arlon SQA-TMS-003 |
Arlon 56946C026 Silicone Rubber/Fiberglass Laminate Side 1: cured silicone rubber; Substrate: 1564 fiberglass; Side 2: uncured silicone rubber; Interleave: 3 mil polyethylene |
|||
Thickness | 406 microns | 16.0 mil | Substrate; Arlon SQA-TMS-003 |
Arlon 56986R028 0.028" (0.711 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone Rubber Substrate: 1564 Style Fiberglass Side 2: Uncured Silicone Rubber Interleave: Polyethylene Product Use: Flame Resistant-flexible heater substrateApp.. |
|||
Thickness | 406 - 483 microns | 16.0 - 19.0 mil | Overall |
Arlon R31678R016 0.0175" (0.444 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone/Kapton Side 2: Uncured Silicone Rubber Appearance: Red silicone gum on fiberglass cloth with Kapton® film on opposite side.This data Represents typical va.. |
|||
Thickness | 406 microns | 16.0 mil | Substrate; Arlon SQA-TMS-003 |
Arlon 55276R030 0.030" (0.762 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 2: Uncured Silicone Rubber Substrate: Style 162 FiberglassSide 1: Cured Silicone RubberProduct Use: Flexible heater insulationAppearance: Red silic.. |