Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 305 microns | 12.0 mil | |
Rogers Corporation Poron® 4701-50 Supported Urethane Foam, Firm, PET Supported Firm material used for managing high energy impact with gasketing needs. Standard available thickness range from 0.012" to 0.500" (0.30 mm to 12.7 mm).Features and Benefits of PORON Products: Exce.. |
|||
Thickness | 305 microns | 12.0 mil | |
Rogers Corporation Poron® 4790-92-30012 P Urethane Foam, Extra Soft, Slow Rebound, PET Film Reinforced Extra soft, slow rebound with a very low closure force. Available with thickness of 0.012" (0.30 mm).Features and Benefits of PORON Products: Excellent compression set resistance which enables dura.. |
|||
Thickness | 305 microns | 12.0 mil | Cured Ply |
Park Electrochemical Nelcote® E-718 Epoxy Prepreg, T-700 24K Uni-Tape Reinforced Nelcote® E-718 is a modified epoxy resin system. E-718 is designed to provide excellent mechanical properties at low cure pressures.Key Features and Benefits:Good low pressure consolidationExcellen.. |
|||
Thickness | 305 microns | 12.0 mil | cured laminate, per ply |
Park Electrochemical Nelcote® F-502 Phenolic Prepreg, 581 Quartz Reinforced Nelcote® F-502 is a MIL-R-9299 phenolic resin system suitable for impregnation on any MIL-C-9084 fabric with a compatible finish. F-502 is used in the manufacture of ablative reinforcements in rock.. |
|||
Thickness | 305 microns | 12.0 mil | |
Zircar Zirconia ZYK-15 Zirconia Cloth Insulation Zirconia Cloth Type ZYK-15 is a tricot knit cloth nominally 0.012” thick composed of yttria stabilized zirconia fibers. This material offers extreme temperature and chemical resistance in a flexibl.. |
|||
Thickness | 305 microns | 12.0 mil | |
Fibre Glast 549 Kevlar® Fabric This was one of the first high strength synthetic fibers to gain acceptance in the reinforced plastic industry. Unlike the previous synthetic reinforcing fibers, Kevlar® has a considerably higher.. |
|||
Thickness | 305 microns | 12.0 mil | at 0.06 MPa |
Zircar Ceramics APA-3 Alumina Paper ZIRCAR Alumina Papers are uniform structures made principally of alumina fiber. APA-3 is a thin uniformly rigidized sheet of alumina fiber and binder. Applications include thermal insulation in lo.. |
|||
Thickness | 305 microns | 12.0 mil | Nominal |
DuPont™ Nomex® 410 Paper, 12 mil Nominal Thickness Nomex® Type 410 is a calendared insulation paper which offers high inherent dielectric strength, mechanical toughness, flexibility, and resilience. It is the original form of Nomex® paper and is .. |
|||
Thickness | 305 microns | 12.0 mil | Nominal |
DuPont™ Nomex® 414 Paper, 12 mil Nominal Thickness Nomex® Type 414 is designed for uses requiring a strong, yet flexible and conformable sheet. It is electrically and thermally similar to Type 410. Type 414 was designed as slot insulation in hand.. |
|||
Thickness | 305 microns | 12.0 mil | Backing; ASTM D3652 |
3M 436/Silver Damping Foils Low temperature vibration dampingInformation provided by 3M |
|||
Thickness | 305 microns | 12.0 mil | |
3M 5959 Outdoor Masking and Stucco Tape 3M™ Outdoor Masking and Stucco Tape 5959 has a high tensile strength backing for pulling through stucco, EIFS and other heavy coatings. Moisture and UV resistant, strong conformable backing. Clean .. |
|||
Thickness | 305 microns | 12.0 mil | Side 1; Arlon SQA-TMS-003 |
Arlon 49481R030 0.030" (0.762 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: Polyethylene Side 1: Uncured Silicone RubberSubstrate: Style 1681 FiberglassSide 2: Uncured Silicone RubberInterleave 2: Polyethylene This data represents typical .. |
|||
Thickness | 305 microns | 12.0 mil | Silicone; Arlon SQA-TMS-003 |
Arlon 51044R020 0.020" Semi-Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 2.5 mil PolyethyleneSide 1: Semi-cured Silicone RubberSubstrate: Style 7628 FiberglassThis data represents typical values for the production material and should no.. |
|||
Thickness | >= 305 microns | >= 12.0 mil | Side 1 |
Arlon 51582R020 0.020" (0.508 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberThis data Represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Inform.. |
|||
Thickness | 305 microns | 12.0 mil | Side 1; Arlon SQA-TMS-003 |
Arlon 55572R030 0.030" (0.762 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 162 Fiberglass Appearance: Red silicone rubber on fiberglass clothThis data Represents typical values for the production material. T.. |
|||
Thickness | 305 microns | 12.0 mil | Side 1; Arlon SQA-TMS-003 |
Arlon 55590R030 0.030" (0.762 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: PolyethyleneSide 1: Uncured Silicone Rubber Substrate: Style 162 FiberglassThis data represents typical values for the production material. The data should not be us.. |
|||
Thickness | 305 microns | 12.0 mil | Prime Coated 1581 Fiberglass, Substrate |
Arlon 57226R020 0.020" (0.508 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone Rubber Side 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place o.. |
|||
Thickness | 305 microns | 12.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon Thermabond® 51A42X012 0.012" (0.305 mm) Cured Silicone Rubber with Fiberglass Substrate Description: Thermabond® - Electrically insulating, thermally conductive, thermal interface material (TIM)Design/Construction: Liner: Polyethylene Side 1: Cured Silicone RubberSubstrate: Style 7628.. |
|||
Thickness | <= 305 microns | <= 12.0 mil | |
3M Scotchkote™ EG 513 Epoxy Ceramic Rebuild Scotchkote Epoxy Ceramic Repair EG 513 has been specifically developed as a ceramic filled repair system for rebuilding and repairing equipment requiring good mechanical strength, combined with abra.. |
|||
Thickness | 305 microns | 12.0 mil | Side 1 |
Arlon 51393R032 0.032" (0.813 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Cured Silicone Rubber Pad Life: Temperature and time dependentThis data represents typical values for the production material. The data shoul.. |
|||
Thickness | 305 microns | 12.0 mil | Side 2 |
Arlon 51393R032 0.032" (0.813 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Cured Silicone Rubber Pad Life: Temperature and time dependentThis data represents typical values for the production material. The data shoul.. |
|||
Thickness | 305 microns | 12.0 mil | Side 1; Arlon SQA-TMS-003 |
Arlon 55100R030 0.030" (0.762 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1: Uncured Silicone RubberSubstrate: Style 162 Fiberglass Product Use: Flexible heater insulationAppearance: Red silicone gum on fiberglass fabricT.. |
|||
Thickness | 305 microns | 12.0 mil | Side 1; Arlon SQA-TMS-003 |
Arlon 55272R028 0.028" (0.711 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1: Cured Silicone Rubber Substrate: Style 162 FiberglassThis data represents typical values for the production material. The data should not be use.. |
|||
Thickness | 305 microns | 12.0 mil | Side 1; Arlon SQA-TMS-003 |
Arlon 55560R030 0.030" (0.762 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1: Uncured Silicone Rubber Substrate: Style 162 Fiberglass Appearance: Red silicone gum on fiberglass fabricThis data represents typical values for.. |
|||
Thickness | 305 microns | 12.0 mil | Side 1; Arlon SQA-TMS-003 |
Arlon 90B32R016AC Aluminum Clad Press Pad with "C-Finish" Design/Construction:Side 2: Alloy 1100 Aluminum FoilSide 1: Cured Silicone RubberThis data represents typical values for the production material and should not be used as material specifications.I.. |
|||
Thickness | 305 microns | 12.0 mil | Silicone; Arlon SQA-TMS-003 |
Arlon 91B32R016AC Aluminum Clad Silicone Press Pad with "C-finish" Design/Construction:Side 2: Alloy 1100 H18 Aluminum FoilSide 1: Cured Silicone RubberThis data represents typical values for the production material and should not be used as material specificatio.. |
|||
Thickness | 305 microns | 12.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon R38041X012 0.012" (0.305 mm) Uncured Fluorosilicone with Fiberglass Substrate Design/Construction: Interleave 1: PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Style 2116 FiberglassSide 2: Uncured Silicone Rubber Interleave 2: Polyethylene Appearance: Gray silicone gum.. |
|||
Thickness | 305 microns | 12.0 mil | Nominal |
AK Steel CARLITE® M-5 Grain Oriented Electrical Steel Oriented Electrical Steels are iron-silicon alloys that were developed to provide the low core loss and high permeability required for efficient and economical electrical transformers. First produce.. |
|||
Thickness | 305 microns | 12.0 mil | Overall Thickness; Arlon SQA-TMS-003 |
Arlon 47571R012 0.012" Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: LDPESide 1: Uncured Silicone RubberSubstrate: Style 2113 FiberglassSide 2: Uncured Silicone RubberInterleave: LDPEThis data represents typical values for the produ.. |
|||
Thickness | 305 microns | 12.0 mil | Rubber; Arlon SQA-TMS-012 |
Arlon T1012-R004-xx 0.012" Self-Fusing Silicone Rubber Tape 1 inch wide, 12 mil thick, red, rectangular cross-section, self-fusing silicone tape. Product is supplied in various yard long roll lengths as indicated by the xx characters in the part number.Desi.. |