Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 25.0 - 80.0 microns | 0.984 - 3.15 mil | Recommended |
Polimeri Europa Riblene® FL 23 Low Density Polyethylene - Blown Film Extrusion Riblene FL 23 is a low density polyethylene (LDPE) with added slip agent, suitable for blown film extrusion. Riblene FL 23 is characterized by a good balance between processability and mechanical p.. |
|||
Thickness | 25.0 microns | 0.984 mil | |
Premix Thermoplastics PREFLEX E25 Polyphenylene Ether (PPO/PPE) PREFLEX films combine outstanding dielectric properties, good heat stability, low water absorption and chemical resistance in a way not available before. Also rigid boards made of the same material .. |
|||
Thickness | 25.0 microns | 0.984 mil | |
NOVA Chemicals Sclair® FP019-C Octene Copolymer LLDPE Film Resin FP019-C is biologically and chemically inert.Features: Superior toughness, Outstanding melt strength, Excellent sealability, Low gelAdditives: Polymer Process AidApplications: High toughness film,.. |
|||
Thickness | 25.0 microns | 0.984 mil | |
NOVA Chemicals Sclair® FP020-D Octene Copolymer LLDPE Film Resin FP020-D complies with the U.S. FDA specifications for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food. FP020.. |
|||
Thickness | 25.0 microns | 0.984 mil | |
Total Finathene® LL 4010 FE 18 LLDPE film
(discontinued **) Linear low density polyethylene made by gas phase process for blown film applications. Advised temperature profile: 190 to 220°C.Information provided provided by Total Petrochemicals.Total Petroche.. |
|||
Thickness | 25.0 microns | 0.984 mil | extruded at 2:1 BUR |
Lotte Chemical Titan TITANEX® LF1043 Linear low density polyethylene resin
(discontinued **) LF1043 is a pelleted linear low density polyethylene resin formulated with antioxidant, and antiblock agent. This product is used for blown film extrusion which offers outstanding toughness, extrud.. |
|||
Thickness | 25.0 microns | 0.984 mil | extruded at 2:1 BUR |
Lotte Chemical Titan TITANEX® LF2824 Linear low density polyethylene resin
(discontinued **) LF2824 is a pelleted linear low density polyethylene resin formulated with antioxidant. This product is used for blown and cast film extrusion which offers outstanding toughness, extrudability and .. |
|||
Thickness | 25.0 microns | 0.984 mil | extruded at 2:1 BUR |
Lotte Chemical Titan TITANEX® LF1054 Linear low density polyethylene Hexene-1 resin
(discontinued **) LF1054 is a pelleted linear low density polyethylene Hexene-1 resin formulated with antioxidant. This product is used for blown film extrusion which offers outstanding toughness, extrudability and .. |
|||
Thickness | 25.0 microns | 0.984 mil | slot cast film at 280°C |
Lotte Chemical Titan TITANEX® LF2554 Linear low density polyethylene Hexene-1 resin
(discontinued **) LF2554 is a pelleted linear low density polyethylene Hexene-1 resin formulated with antioxidant. This product is used for slot cast extrusion which offers outstanding toughness, extrudability and d.. |
|||
Thickness | 25.0 - 75.0 microns | 0.984 - 2.95 mil | Recommended range for processing |
NOVA Chemicals Surpass® HPs167-AB Homopolymer sHDPE Film Resin HPs167-AB complies with the U.S. FDA regulations for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food.NOVA Che.. |
|||
Thickness | 25.0 microns | 0.984 mil | ± 2.5%; ASTM-252-78 |
Kinlead HSS12 Normal Grade Heat Sealable Film (thickness: 25 µm) HSS12 is a printing, normal grade heat sealable film. It is transparent, and one side is heat sealable. It has low static, good ink adhesion, and good heat seal strength. One side has corona treatme.. |
|||
Thickness | 25.0 microns | 0.984 mil | ± 2.5%; ASTM-252-78 |
Kinlead LSD13 Low Temperature Grade Heat Sealable Film (thickness: 25 µm) LSD13 is a metalizing, low temperature grade heat sealable film. It is transparent, and both sides are heat sealable. It has low static, excellent metal adhesion, and good heat seal strength. One si.. |
|||
Thickness | 25.0 microns | 0.984 mil | ± 2.5%; ASTM-252-78 |
Kinlead LSS11 Low Temperature Grade Heat Sealable Film (thickness: 25 µm) LSS11 is a general, low temperature grade heat sealable film. It is transparent, and one side is heat sealable. It has low static, excellent flatness, and good heat seal strength. One side has coron.. |
|||
Thickness | 25.0 microns | 0.984 mil | ± 2.5%; ASTM-252-78 |
Kinlead PG14 Bag Grade BOPP Plain Film (thickness: 25 µm) PG14 is a low static, bag grade BOPP plain film. It is transparent, low static, and non heat sealable. It has excellent flatness. One side has corona treatment. It is widely used in gift wrapping an.. |
|||
Thickness | 25.0 microns | 0.984 mil | ± 2.5%; ASTM-252-78 |
Kinlead PT11 Adhesive Tape Grade BOPP Plain Film (thickness: 25 µm) PT11 is a general, adhesive tape grade BOPP plain film. It is transparent and non heat sealable. It has excellent glue adhesion, good dimensional stability, and high tensile strength. One side has c.. |
|||
Thickness | 25.0 microns | 0.984 mil | ± 2.5%; ASTM-252-78 |
Kinlead PT12 Adhesive Tape Grade BOPP Plain Film (thickness: 25 µm) PT12 is a super clear, adhesive tape grade BOPP plain film. It is transparent and non heat sealable. It has excellent glue adhesion and high clarity. One side has corona treatment. It is widely used.. |
|||
Thickness | 25.0 microns | 0.984 mil | |
UBE 5033B Nylon 6/66 Film Description: T-die cast film of 25µm in thicknessInformation provided by UBE. |
|||
Thickness | 25.0 microns | 0.984 mil | |
Formosa Plastics Formolene® L42022E2 Film (Butene Grade) LLDPE Butene Copolymer (Low slip and antiblock)Applications: Thin gauge blown filmThin gauge blown filmMeets all requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520, cove.. |
|||
Thickness | 25.0 microns | 0.984 mil | |
Formosa Plastics Formolene® L62030B Film (Hexene Grade) LLDPE Hexene Copolymer (Barefoot)Applications: Cast stretch film and high quality packaging films requiring clarity and toughness.A Hexene Copolymer Linear Low Density Polyethylene for film applications i.. |
|||
Thickness | 25.0 microns | 0.984 mil | As Tested |
Equate EFDA-7047 LLDPE Film Extrusion Resin EFDA-7047 is a linear low-density polyethylene resin for tubular blown film extrusion. Films made from this resin have good toughness, high tensile strength and puncture resistance. EFDA-7047 does n.. |
|||
Thickness | 25.0 microns | 0.984 mil | |
Dow AFFINITY™ PL 1845 Polyolefin Plastomer Film properties below based on a film thickness of 25 µm. Data provided by Dow Chemical. |
|||
Thickness | 25.0 microns | 0.984 mil | |
Dow ATTANE™ 4202 Ultra Low Density Polyethylene, Cast Film Grade ATTANE® 4202 copolymer is an ultra low density polyethylene having excellent tear and puncture resistance with good optics. It is designed for cast films used in food packaging applications. It com.. |
|||
Thickness | 25.0 microns | 0.984 mil | |
Dow ATTANE™ 4402 Ultra Low Density Polyethylene, Cast Film Grade ATTANE® 4402 copolymer is an ultra low density polyethylene having excellent tear and puncture resistance, and outstanding stretchability. It is designed for industrial/consumer cast film applicati.. |
|||
Thickness | 25.0 microns | 0.984 mil | |
Dow DOWLEX™ 2101 Linear Low Density Polyethylene, Blown Film Grade DOWLEX® 2101 Polyethylene resin, a general purpose blown film extrusion resin, is an excellent choice for high speed, thin gauge film applications. It contains medium levels of both slip additive a.. |
|||
Thickness | 25.0 microns | 0.984 mil | |
Braskem BC818 Extrusion Coating Low Density Polyethylene Description: BC818 is a grade produced under high pressure in an autoclave reactor. In the coating process it presents very good optical properties, low neck-in, good film stability, and good adhesi.. |
|||
Thickness | 25.0 microns | 0.984 mil | |
Braskem F2022/0 Cast Film Extrusion Low Density Polyethylene Films for diapers and absorbent articles; Medium resistance films or for general use.Information provided by Braskem. |
|||
Thickness | 25.0 microns | 0.984 mil | |
Braskem Flexus® 9200 Blown Film Extrusion Polyethylene Description: Flexus 9200 is a LLDPE hexene copolymer produced through metallocene catalyst which presents excellent impact and puncture strength, beyond a differential sealing performance comparing .. |
|||
Thickness | 25.0 microns | 0.984 mil | |
Braskem LL118 Blown Film Extrusion Linear Low Density Polyethylene Description: LL218/21 is a LLDPE Butene copolymer produced by Braskem. It was specially designed to provide outstanding processing performance. Films obtained with this grade show good physical and .. |
|||
Thickness | 25.0 microns | 0.984 mil | 4:1 blow-up ratio |
Bapolene® 345F Medium Density Polyethylene Film Resin Description: Bapolene 345F is a medium molecular weight film resin with excellent tensile, impact, and tear properties. Applications: Merchandise bags, produce and trash bags.Bapolene® and Bapolan®.. |
|||
Thickness | 25.0 microns | 0.984 mil | |
Braskem Green PE SLL118 Blow Film Extrusion and Cast Film Extrusion Linear Low Density Polyethylene Description: SLL118 is a Linear Low Density Polyethylene, copolymer of butene-1. Developed for blown film extrusion in blends with polyethylenes. Films obtained with this product show a good process.. |