Physical Properties Metric English Comments
Thickness 20.1 microns
0.790 mil
ExxonMobil Method
ExxonMobil Bicor™ 20MB080 OPP Film
Product Description: Bicor 20NB080 is a biaxially oriented polypropylene film metallizable on one side, with a heat sealable surface on the other side. Designed to be used after metallization as a s..
Thickness 20.1 microns
0.790 mil
ExxonMobil Method
ExxonMobil Bicor™ 20MB400 OPP Film
Product Description: Bicor 20MB400 is a one side treated, sealable coextruded OPP film. It is designed for use in laminations.Availability: Africa & Middle East, Asia Pacific and EuropeKey Features:..
Thickness 20.1 microns
0.790 mil
ExxonMobil Method
ExxonMobil Bicor™ 20MB666 OPP Film
Product Description: Bicor 20MB666 is a biaxially oriented transparent polypropylene film acrylic coated two sides. It provides outstanding performance on all packaging machines and is mainly propos..
Thickness 20.1 microns
0.790 mil
ExxonMobil Method
ExxonMobil Bicor™ 20MB668 OPP Film
Product Description: Bicor 20MB668 is a high speed transparent, biaxially oriented polypropylene film, coated one side acrylic, one side very low temperature seal (VLTS) coating. VLTS coating provid..
Thickness 20.1 microns
0.790 mil
ExxonMobil Method
ExxonMobil Metallyte™ 20MM480 OPP Film
Product Description: A metalized biaxially oriented polypropylene film, metalized on one side, heat sealable on the other side. It is typically used in lamination with other substrates on HFFS and V..
Thickness 20.1 microns
0.790 mil
ExxonMobil Method
ExxonMobil Bicor™ 20MBT666 OPP Film
Product Description: Bicor 20MBT666 is a biaxially oriented transparent polypropylene film acrylic coated two sides. This film is specifically suitable for unprinted overwrapping, offering unique as..