Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 0.400 - 50.0 g/10 min | 0.400 - 50.0 g/10 min | Average value: 12.2 g/10 min Grade Count:117 |
Overview of materials for Polyester Thermoplastic Elastomer This property data is a summary of similar materials in the MatWeb database for the category "Polyester Thermoplastic Elastomer". Each property range of values reported is minimum and maximum values.. |
|||
Melt Flow | 5.00 - 50.0 g/10 min | 5.00 - 50.0 g/10 min | Average value: 20.0 g/10 min Grade Count:6 |
Overview of materials for Polyphthalamide (PPA) This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide". Each property range of values reported is minimum and maximum values of appropriate Ma.. |
|||
Melt Flow | 17.0 - 50.0 g/10 min | 17.0 - 50.0 g/10 min | Average value: 27.7 g/10 min Grade Count:10 |
Overview of materials for Polyetheretherketone, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, PTFE Filled". Each property range of values reported is minimum and maximum values.. |
|||
Melt Flow | 1.00 - 50.0 g/10 min | 1.00 - 50.0 g/10 min | Average value: 18.1 g/10 min Grade Count:18 |
Overview of materials for Polyphenylene Ether, Heat Resistant This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Heat Resistant". Each property range of values reported is minimum and maximum valu.. |
|||
Melt Flow | 2.00 - 50.0 g/10 min | 2.00 - 50.0 g/10 min | Average value: 14.8 g/10 min Grade Count:206 |
Overview of materials for Polycarbonate, Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Unreinforced, Flame Retardant". Each property range of values reported is minimum and max.. |
|||
Melt Flow | 2.00 - 50.0 g/10 min | 2.00 - 50.0 g/10 min | Average value: 17.8 g/10 min Grade Count:16 |
Overview of materials for Modified ETFE, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Modified ETFE, Unreinforced". Each property range of values reported is minimum and maximum values of ap.. |
|||
Melt Flow | 1.00 - 50.0 g/10 min | 1.00 - 50.0 g/10 min | Average value: 6.53 g/10 min Grade Count:20 |
Overview of materials for Nylon 66, Heat Stabilized This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Heat Stabilized". Each property range of values reported is minimum and maximum values of appr.. |
|||
Melt Flow | 3.00 - 50.0 g/10 min | 3.00 - 50.0 g/10 min | Average value: 9.70 g/10 min Grade Count:8 |
Overview of materials for Nylon 12, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Melt Flow | 1.10 - 50.0 g/10 min | 1.10 - 50.0 g/10 min | Average value: 17.4 g/10 min Grade Count:3 |
Overview of materials for Nylon 12, 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. .. |
|||
Melt Flow | 15.0 - 50.0 g/10 min @Load 21.6 kg, Temperature 190 °C |
15.0 - 50.0 g/10 min @Load 47.6 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Sinpolene MBB1511 Linear Low Density Polyethylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Carbon Black (500000 ppm) Features: General Purpose Forms: PelletsInformation Provided by Teknor Apex |
|||
Melt Flow | 30.0 - 50.0 g/10 min @Load 21.6 kg, Temperature 190 °C |
30.0 - 50.0 g/10 min @Load 47.6 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Sinpolene MBB2691 Linear Low Density Polyethylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Carbon Black (460000 ppm) Features: General Purpose Forms: PelletsInformation Provided by Teknor Apex |
|||
Melt Flow | 30.0 - 50.0 g/10 min @Load 21.6 kg, Temperature 190 °C |
30.0 - 50.0 g/10 min @Load 47.6 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Sinpolene MBB7532 Low Density Polyethylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Carbon Black (500000 ppm) Features: General Purpose Forms: PelletsInformation Provided by Teknor Apex |
|||
Melt Flow | 2.00 - 50.0 g/10 min | 2.00 - 50.0 g/10 min | Average value: 6.30 g/10 min Grade Count:67 |
Overview of materials for Linear Medium Density Polyethylene (LMDPE), Rotational Molded This property data is a summary of similar materials in the MatWeb database for the category "Linear Medium Density Polyethylene (LMDPE), Rotational Molded". Each property range of values reported i.. |
|||
Melt Flow | 3.00 - 50.0 g/10 min | 3.00 - 50.0 g/10 min | Average value: 17.4 g/10 min Grade Count:12 |
Overview of materials for Nylon 6, Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Film Grade". Each property range of values reported is minimum and maximum values of appropriat.. |
|||
Melt Flow | 5.00 - 50.0 g/10 min | 5.00 - 50.0 g/10 min | Average value: 22.7 g/10 min Grade Count:3 |
Overview of materials for Polyphthalamide (PPA), 10% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% are .. |