Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 5.0 - 22 g/10 min | 5.0 - 22 g/10 min | (Condition L) ASTM D-1238 |
Multibase Multi-Flex® TPE A 7150 BLK The burn rate is 1 in/min (25 mm/min) based on ASTM FM VSS 302. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Melt Flow | 5.0 - 22 g/10 min @Load 6.70 kg, Temperature 337 °C |
5.0 - 22 g/10 min @Load 14.8 lb, Temperature 639 °F |
ASTM D1238 |
Polymer Resources PEI-G10 Polyetherimide, 10% Glass Reinforced Polyetherimide, 10% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Poly.. |
|||
Melt Flow | 5.0 - 22 g/10 min @Load 6.70 kg, Temperature 337 °C |
5.0 - 22 g/10 min @Load 14.8 lb, Temperature 639 °F |
ASTM D1238 |
Polymer Resources PEI-G20 Polyetherimide, 20% Glass Reinforced Polyetherimide, 20% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Poly.. |
|||
Melt Flow | 5.0 - 22 g/10 min @Load 6.70 kg, Temperature 337 °C |
5.0 - 22 g/10 min @Load 14.8 lb, Temperature 639 °F |
ASTM D1238 |
Polymer Resources PEI-G30 Polyetherimide, 30% Glass Reinforced Polyetherimide, 30% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Poly.. |
|||
Melt Flow | 6.0 - 22 g/10 min @Load 6.70 kg, Temperature 337 °C |
6.0 - 22 g/10 min @Load 14.8 lb, Temperature 639 °F |
ASTM D1238 |
Polymer Resources PEI-GP1 Polyetherimide, Flame Retardant Polyetherimide, Flame Retardant, High Heat ResistanceProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information.. |
|||
Melt Flow | 10 - 22 g/10 min @Load 0.325 kg, Temperature 270 °C |
10 - 22 g/10 min @Load 0.716 lb, Temperature 518 °F |
|
Plastcom SLOVAMID 6 FRC 2 218/1M PA6, flame retardant Packaging, transport, stockingThe product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.0.. |
|||
Melt Flow | 17 - 22 g/10 min @Load 2.16 kg, Temperature 300 °C |
17 - 22 g/10 min @Load 4.76 lb, Temperature 572 °F |
ISO 1133 |
PolyOne Edgetek® ET3500-5002 BK Acrylonitrile Styrene Acrylate + PC (ASA+PC) The Edgetek™ Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Melt Flow | 5.0 - 22 g/10 min | 5.0 - 22 g/10 min | ASTM D1238 |
Polymer Resources PEI-G40 Polyetherimide, 40% Glass Reinforced
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Melt Flow | 18 - 22 g/10 min | 18 - 22 g/10 min | ASTM D1238 |
Micropol L20 Low density polyethylene rotational molding powder Has a high gloss finish, and outstanding toughness. Information provided by Micropol Limited |
|||
Melt Flow | 18 - 22 g/10 min @Load 2.16 kg, Temperature 235 °C |
18 - 22 g/10 min @Load 4.76 lb, Temperature 455 °F |
ASTM D1238 |
Gromax CCP PBT 1100-630S Product Description: PBT unreinforced medium viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce.. |
|||
Melt Flow | 18 - 22 g/10 min @Load 2.16 kg, Temperature 235 °C |
18 - 22 g/10 min @Load 4.76 lb, Temperature 455 °F |
ASTM D1238 |
Gromax PBT 1100-211M Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce.. |
|||
Melt Flow | 18.1 - 22 g/10 min @Load 1.20 kg, Temperature 300 °C |
18.1 - 22 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
Iran Petrochemical (PCC) PC 1822 Polycarbonate Suitable for injection moldingInformation provided by Iran Petrochemical Commercial Co. |
|||
Melt Flow | 18 - 22 g/10 min @Load 2.16 kg, Temperature 240 °C |
18 - 22 g/10 min @Load 4.76 lb, Temperature 464 °F |
ASTM D1238 |
Samyang Triel® 5722EM Thermoplastics Polyetherester Elastomer, Extrusion Excellent mechanical characteristics, elasticity, thermal resistance and chemical resistance.5722EM is an extrusion grade.Information provided by Samyang. |
|||
Melt Flow | 5.0 - 22 g/10 min | 5.0 - 22 g/10 min | ASTM D1238 |
Polymer Resources PEI-G10 Polyetherimide, 10% Glass Reinforced
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Melt Flow | 5.0 - 22 g/10 min | 5.0 - 22 g/10 min | ASTM D1238 |
Polymer Resources PEI-G20 Polyetherimide, 20% Glass Reinforced
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Melt Flow | 5.0 - 22 g/10 min | 5.0 - 22 g/10 min | ASTM D1238 |
Polymer Resources PEI-G30 Polyetherimide, 30% Glass Reinforced
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Melt Flow | 20 - 22 g/10 min | 20 - 22 g/10 min | Cond. O |
Ashley Polymers Ashlene® P1051R Polycarbonate A high flow transparent polycarbonate with good impact properties.Data provided by the manufacturer |
|||
Melt Flow | 20 - 22 g/10 min | 20 - 22 g/10 min | Cond. O |
Ashley Polymers Ashlene® P1053R Polycarbonate A high flow transparent polycarbonate with good impact properties containing UV stabilizer.Data provided by the manufacturer |