Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 6.5 g/10 min @Load 2.16 kg, Temperature 230 °C |
6.5 g/10 min @Load 4.76 lb, Temperature 446 °F |
Procedure A Condition L; ASTM D1238 |
Network Polymers PC-1006 Description: Natural PolycarbonateInformation provided by Network Polymers Inc. |
|||
Melt Flow | 6.5 g/10 min @Load 5.00 kg, Temperature 260 °C |
6.5 g/10 min @Load 11.0 lb, Temperature 500 °F |
ASTM D 1238 |
SABIC Innovative Plastics Cycoloy® LG8002 PC+ABS Automotive. Low gloss, high impact and ductility at 73F and -22F. UV-stable colors.This data was supplied by SABIC-IP for the Americas region. |
|||
Melt Flow | 6.5 g/10 min @Load 5.00 kg, Temperature 260 °C |
6.5 g/10 min @Load 11.0 lb, Temperature 500 °F |
ASTM D 1238 |
SABIC Innovative Plastics Cycoloy® LG8002 PC+ABS (Asia Pacific) Automotive. Low gloss, high impact and ductility at 73F and -22F. UV-stable colors.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Melt Flow | 6.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
6.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® BFL2015 PC Non-brominated, non-chlorinated flame retardant, glass reinforced PC. Opaque colors only |
|||
Melt Flow | 6.5 g/10 min | 6.5 g/10 min | ASTM D1238 |
Formosa Plastics Formolene® L63565U Rotational Molding LLDPE
(discontinued **) Hexene CopolymerApplications: Toys, medium tanks, material handling equipment and flat surface rotational molding applications.Formolene L63565U is fully heat and UV stabilized.Meets all requirement.. |
|||
Melt Flow | 6.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
6.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Chevron Phillips LX8119 HDPE Injection Molding Resin
(discontinued **) Resin Type: linear copolymer; ASTM D4976 Classification: PE 233, A 56700Characteristics: warp resistant, excellent impact strength, excellent ESCR, moderate shrinkage resistanceApplications: seats, .. |
|||
Melt Flow | 6.5 g/10 min | 6.5 g/10 min | Exxon Method |
ExxonMobil Escorene® LD-336 EVA Film Resin, Clarity, Very High Drawdown
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 3.5% vinyl acetate copolymer blown film resin capable of very high drawdown with excellent clarity.Applications: Very thin heat seal layers; Light.. |
|||
Melt Flow | 6.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
6.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
Covestro Makrolon® DP1-1243 Polycarbonate, Extrusion
(discontinued **) Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ.. |
|||
Melt Flow | 6.5 g/10 min @Load 2.16 kg, Temperature 343 °C |
6.5 g/10 min @Load 4.76 lb, Temperature 649 °F |
ASTM D1238 |
Solvay Specialty Polymers Udel® GF-110 Polysulfone (PSU)
(Unverified Data**) Udel GF-110, resin is a 10% glass fiber reinforced polysulfone (PSU). Glass fiber substantially increases the rigidity, tensile strength, creep resistance, dimensional stability and chemical resista.. |
|||
Melt Flow | 6.5 g/10 min @Load 2.16 kg, Temperature 343 °C |
6.5 g/10 min @Load 4.76 lb, Temperature 649 °F |
ASTM D1238 |
Solvay Specialty Polymers Udel® GF-120 Polysulfone (PSU)
(Unverified Data**) Udel GF-120, resin is a 20% glass fiber reinforced polysulfone compound. Glass fiber substantially increases the rigidity, tensile strength, creep resistance, dimensional stability and chemical resi.. |
|||
Melt Flow | 6.5 g/10 min @Load 2.06 kg, Temperature 343 °C |
6.5 g/10 min @Load 4.54 lb, Temperature 649 °F |
ASTM D1238 |
Solvay Specialty Polymers Udel® P-1750 MR Polysulfone (PSU)
(Unverified Data**) Udel P-1750 MR is a lower color grade of polysulfone that contains a mold release which aids part ejection when parts with low draft are injection molded. Polysulfones have long been known for trans.. |
|||
Melt Flow | 6.5 g/10 min @Load 5.00 kg, Temperature 400 °C |
6.5 g/10 min @Load 11.0 lb, Temperature 752 °F |
ASTM D1238 |
Solvay Specialty Polymers Supradel® HTS-2600 High Temperature Sulfone Resin
(discontinued **) SUPRADEL HTS-2600 is a high-temperature, high-performance, amorphous, sulfone polymer. In addition to exceptional thermal performance, this resin has the other performance features and attributes t.. |
|||
Melt Flow | 6.5 g/10 min | 6.5 g/10 min | ASTM D1238 |
LyondellBasell Alathon® M5363 High Density Polyethylene ApplicationsALATHON L 4912 is a high molecular weight, high density copolymer with a broad molecular weight distribution. This resin provides excellent stiffness and a good balance of film properti.. |
|||
Melt Flow | 6.5 g/10 min | 6.5 g/10 min | ASTM D1238 |
LyondellBasell Plexar® PX5125 Extrudable Tie-Layer Resin - Anhydride Modified LLDPE ApplicationsPLEXAR tie-layers are chemically modified resins used to bond unlike materials, primarily in packaging and industrial applications. Common adherents include polyethylene resins and copo.. |
|||
Melt Flow | 6.5 g/10 min @Load 10.0 kg, Temperature 220 °C |
6.5 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Kingfa HR-527B Modified ABS Features:UL94 HB @ 1.5-3.2mmExcellent heat resistanceApplications:Automobile partsAutomobile audioDashboard, interior trimAutomobile lamp, mirrorInformation Provided by Kingfa Sci. & Tech. Co., Ltd... |
|||
Melt Flow | 6.5 g/10 min @Load 10.0 kg, Temperature 220 °C |
6.5 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
LG Chemical RS650 ABS Feature: Extrusion Molding, General PurposeApplication: MiscellaneousCAS No. 9003-56-9Information provided by LG Chemical |
|||
Melt Flow | 6.5 g/10 min @Load 6.60 kg, Temperature 337 °C |
6.5 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D1238 |
SABIC Innovative Plastics ULTEM 2200R PEI 20% Glass fiber filled, standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing. |
|||
Melt Flow | 6.5 g/10 min @Load 2.16 kg, Temperature 343 °C |
6.5 g/10 min @Load 4.76 lb, Temperature 649 °F |
ASTM D1238 |
Solvay Specialty Polymers Udel® GF-120 Polysulfone (PSU), Glass Fiber Udel® GF-120, resin is a 20% glass fiber reinforced polysulfone compound. Glass fiber substantially increases the rigidity, tensile strength, creep resistance, dimensional stability and chemical .. |
|||
Melt Flow | 6.5 g/10 min @Load 2.16 kg, Temperature 343 °C |
6.5 g/10 min @Load 4.76 lb, Temperature 649 °F |
ASTM D1238 |
Solvay Specialty Polymers Udel® P-1750 MR Polysulfone (PSU) Udel® P-1750 MR is a lower color grade of polysulfone that contains a mold release which aids part ejection when parts with low draft are injection molded.Polysulfones have long been known for tr.. |
|||
Melt Flow | 6.5 g/10 min @Load 3.80 kg, Temperature 230 °C |
6.5 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM Data |
Styron Magnum™ 9035 ABS, High Gloss MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Melt Flow | 6.5 g/10 min @Load 2.16 kg, Temperature 230 °C |
6.5 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Borealis Borseal™ TD120BF Terpolymer for BOPP Film Borseal TD120BF is a C2/C4 terapolymer film resin especially developed for use as sealing layers in coextruded BOPP film (manufactured on stenter frame and double bubble film process).Borseal TD120B.. |
|||
Melt Flow | 6.5 g/10 min | 6.5 g/10 min | Cond. E; ASTM D1238 |
DuPont Conpol™ 20B Ethylene-Methacrylic Acid Additive Resin Conpol™ additive resins, supplied in pellet form, are designed to modify the surface properties of films or coatings of Surlyn® ionomer resins and Nucrel® acid copolymer resins. They are concentr.. |
|||
Melt Flow | 6.5 g/10 min @Load 5.00 kg, Temperature 200 °C |
6.5 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Total PS CPDS 814 UV Stabilized, Flame Retardant Polystyrene Total Petrochemicals Polystyrene 814 is a heat resistant, UV stabilized V0 Non Deca Polystyrene for injection molding. It is recommended for the manufacturing of articles which require good dimensi.. |
|||
Melt Flow | 6.5 g/10 min | 6.5 g/10 min | Condition E; ASTM D 1238 |
Chevron Phillips MarFlex® 9607 HDPE Cast Film Resin Characteristics: Very Low Gel Levels, Produces Very "Clear" Film, Draws to Thin Gauges, Low Taste and Odor Transfer, Excellent MVTR for a Chill Cast Film, Excellent Processability, Excellent Optical.. |
|||
Melt Flow | 6.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
6.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ISO 1133 |
Covestro Makrolon® ET3117 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Extrusion• High visc.. |
|||
Melt Flow | 6.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
6.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
DuPont Performance Polymers Hytrel® G4078LS NC010 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D Standard Performance Polyester Elastomer with Light ProtectionInformation provided by DuPont Performance Polymers |
|||
Melt Flow | 6.5 g/10 min | 6.5 g/10 min | ASTM D1238 |
Huntsman PE1059 Film Extrusion Polyethylene
(discontinued **) Homopolymer and FDA compliant.Features: Excellent draw down and good processability.Applications: Film extrusion: non-abrasive packaging applications.FDA Notes: Conforms to FDA regulation 21 CFR 177.. |
|||
Melt Flow | 6.5 g/10 min | 6.5 g/10 min | ASTM D1238 |
Huntsman PE8020 Specialty Polyethylene
(discontinued **) Homopolymer and FDA compliant.Features: Yields film with excellent draw down and machinability.Applications: Film extrusion: gel free film applications.FDA Notes: Conforms to FDA regulation 21 CFR 1.. |