Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 50 g/10 min @Load 2.16 kg, Temperature 190 °C |
50 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Polimeri Europa Flexirene® MT 40 A Linear Low Density Polyethylene Flexirene MT 40 A is a linear low density polyethylene (LLDPE), with antioxidants, suitable for injection molding application.Flexirene MT 40 A is characterized by a good processability and impact r.. |
|||
Melt Flow | 50 g/10 min @Load 2.16 kg, Temperature 190 °C |
50 g/10 min @Load 4.76 lb, Temperature 374 °F |
Procedure A Condition E; ASTM D1238 |
Network Polymers NPP 11-5026 Description: Linear Low Density Polyethylene (LLDP)Information provided by Network Polymers Inc. |
|||
Melt Flow | 50 g/10 min @Load 2.16 kg |
50 g/10 min @Load 4.76 lb |
ASTM D1238 |
Reliance Industries Reclair M26500 Polyethylene High flow Linear Low Density Polyethylene grade. Reclair M26500 is a butene comonomer with optimum levels of antioxidants.Characteristics:narrow molecular weight distribution, excellent processabi.. |
|||
Melt Flow | 50 g/10 min | 50 g/10 min | Condition L 230/2.16; ASTM D1238 |
Pinnacle Polymers 2150 H Medium Impact Polypropylene Copolymer, Injection Molding Grade This Pinnacle Polymers Polypropylene is made via UNIPOL™ PP technology, which utilizes gas-phase fluidized bed reactors with a high activity catalyst system to ensure uniform physical properties an.. |
|||
Melt Flow | 50 g/10 min @Load 2.16 kg, Temperature 275 °C |
50 g/10 min @Load 4.76 lb, Temperature 527 °F |
ASTM D1238 |
Solvay Specialty Polymers Halar® 1450LC Polyethylene, Chlorotrifluoroethylene (ECTFE)
(Unverified Data**) Information provided by Solvay Specialty Polymers. |
|||
Melt Flow | 50 g/10 min @Load 2.16 kg, Temperature 230 °C |
50 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
M. Holland Company CP850 Polypropylene Impact Copolymer Impact copolymerFast production cycleHigh flowHigh stiffnessApplications: ContainersHousehold goodsThin-walled parts |
|||
Melt Flow | 50 g/10 min @Load 2.16 kg, Temperature 230 °C |
50 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
IRPC Polimaxx Polene 2541TC Polypropylene Block Copolymer CHARACTERISTICS: EXCELLENT FLOWABILITY, HIGH STIFFNESS, HEAT STABILITY, HIGH IMPACTAPPLICATIONS: INJECTION MOLDING SPECIALLY FOR WASHING TUB, ELECTRICAL APPLIANCES, THIN WALL CONTAINERS |
|||
Melt Flow | 50 - 60 g/10 min @Load 2.16 kg, Temperature 235 °C |
50 - 60 g/10 min @Load 4.76 lb, Temperature 455 °F |
ASTM D1238 |
Gromax PBT 1200-211L Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce.. |
|||
Melt Flow | 50 g/10 min @Load 5.00 kg, Temperature 250 °C |
50 g/10 min @Load 11.0 lb, Temperature 482 °F |
ASTM D1238 |
SABIC Innovative Plastics Valox® IQ507 PBT+PC (Asia Pacific) Valox iQ507 resin: Environmentally responsible, sustainable, and low carbon footprint resin that is 30% glass fiber reinforced PBT+PC alloy. Valox iQ507 offers good mechanical and thermal characte.. |
|||
Melt Flow | 50 g/10 min @Load 10.0 kg, Temperature 250 °C |
50 g/10 min @Load 22.0 lb, Temperature 482 °F |
ASTM D1238 |
Samsung Cheil Industries Infino® LB-1010W PC, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 50 g/10 min @Load 5.00 kg, Temperature 250 °C |
50 g/10 min @Load 11.0 lb, Temperature 482 °F |
ASTM D1238 |
Samyang Tribit® 1500G15 Polybutylene Terephthalate, 15% Glass Reinforced Characteristics:G/F reinforcedHeat and Impact resistantApplications:AutomotiveConnectorGearOutdoor handleIgnition systemElectronicConnectorGas valveCoil bobbinSwitch caseRelay caseO/A partsAll infor.. |
|||
Melt Flow | 50 g/10 min @Load 2.16 kg, Temperature 250 °C |
50 g/10 min @Load 4.76 lb, Temperature 482 °F |
ASTM D1238 |
Samyang Tribit® 1500G20 PBT, Reinforced General Purpose Crystallization is fast, formability is excellent and thermal resistance, chemical resistance, electrical properties and abrasion resistance are excellent.1500G20 is a reinforced, general purpose gr.. |
|||
Melt Flow | 50 g/10 min @Load 1.20 kg, Temperature 300 °C |
50 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
Samyang Trirex® 3015NF Polycarbonate, Flame Retardancy PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3015NF is a flame retardant grade.Applications: Mobile Phone - battery caseInformation.. |
|||
Melt Flow | 50 g/10 min @Load 2.16 kg, Temperature 230 °C |
50 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Borealis Bormed™ BH348MO Polypropylene Heteroplastic Copolymer for Injection Molding Bormed™ BH348MO is a polypropylene copolymer characterized by high impact strength, fast flow and crystallization speed. The material is nucleated with Borstar® Nucleation Technology (BNT). This .. |
|||
Melt Flow | 50 g/10 min @Temperature 230 °C |
50 g/10 min @Temperature 446 °F |
ASTM D1238 |
A. Schulman PP 3471-01 Polypropylene High Flow Homopolymer Polypropylene DescriptionPolypropylene PP 3471-01 is an ultra high flow homopolymer polypropylene designed for high speed, thin wall injection molding.Information provided by A. Schulman. |
|||
Melt Flow | 50 g/10 min @Temperature 230 °C |
50 g/10 min @Temperature 446 °F |
ASTM D1238 |
A. Schulman PP 3471-01 Polypropylene High Flow Homopolymer Polypropylene DescriptionPolypropylene PP 3471-01 is an ultra high flow homopolymer polypropylene designed for high speed, thin wall injection molding.Information provided by A. Schulman. |
|||
Melt Flow | 50 g/10 min @Load 2.16 kg, Temperature 230 °C |
50 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Total PPC 11812 S01 Polypropylene, Heterophasic Copolymer, Injection Molding Polypropylene PPC 11812 S01 has been developed for high speed injection molding of thin walled packaging containers requiring top level impact resistance at cold temperature (-20°C). It is charact.. |
|||
Melt Flow | 50 g/10 min | 50 g/10 min | ASTM D1238 |
Total PPC 4944WZ Polypropylene, Impact Copolymer ATOFINA 4944 polypropylene is a nucleated and controlled rheology impact copolymer. 4944WZ is characterized by improved stiffness and impact resistance, as well as low shrinkage and low warpage. I.. |
|||
Melt Flow | 50 g/10 min @Temperature 230 °C |
50 g/10 min @Temperature 446 °F |
I<sub>2</sub>; ASTM D1238 |
Formosa Plastics Formolene® 2550A Thin Walled Injection Molding Polypropylene Medium Impact CopolymerApplications: Housewares, containers and other rigid packaging.Formolene 2550A is a medium impact, high flow, controlled rheology copolymer of polypropylene designed for such .. |
|||
Melt Flow | >= 50 g/10 min @Load 10.0 kg, Temperature 240 °C |
>= 50 g/10 min @Load 22.0 lb, Temperature 464 °F |
ISO 1133 |
Cossa Polimeri ESTABLEND PA 6000 ABS / Nylon 6 Blend ESTABLEND PA is a blend of acrylonitrile butadiene styrene and polyamide 6.Easy processing, high surface quality, high chemical resistance, good heat resistanceInformation provided by Cossa Polimeri.. |
|||
Melt Flow | 50 g/10 min @Load 10.0 kg, Temperature 220 °C |
50 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D 1238 |
Cossa Polimeri ESTADIENE 1050 AS Acrylonitrile Butadiene Styrene General purpose ABSGood impact resistance, high melt flow rate, high gloss, with antistatic, excellent processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Melt Flow | 50 g/10 min @Load 2.16 kg, Temperature 190 °C |
50 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil LL 6201.19 Injection Molding Resin Product Description: LL 6201 is a narrow molecular weight butane copolymer designed for applications that require excellent toughness. This resin offers easy processability for applications that req.. |
|||
Melt Flow | 50 g/10 min @Load 2.16 kg, Temperature 230 °C |
50 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
ExxonMobil PP7505KNE2 Polypropylene Homopolymer Product Description: A medium to high impact copolymer designed for injection molded large consumer and industrial parts requiring high melt flow rate.Availability: North America Features:Balanced .. |
|||
Melt Flow | 50 g/10 min @Load 2.16 kg |
50 g/10 min @Load 4.76 lb |
Melt flow ratio I10/I2 is 8.5. |
Dow DOWLEX™ IP-50 High Density Polyethylene DOWLEX® IP-50 resin is an improved processing high density polyethylene resin with controlled molecular weight distribution designed for thin wall food containers. This resin is recommended for flo.. |
|||
Melt Flow | 50 g/10 min @Load 2.16 kg, Temperature 235 °C |
50 g/10 min @Load 4.76 lb, Temperature 455 °F |
|
Arkema Group Rilsan® AMN Y TLD Nylon 12, MoS2 Filled (Conditioned) Designation ISO 1874-PA12,MHLS,14-010,MD05Grade with molybdenum filler for injection molding. Available color: steel gray. Light and heat stabilized. Mold-release agent.Low friction coefficient. Goo.. |
|||
Melt Flow | 50 g/10 min @Load 5.00 kg, Temperature 275 °C |
50 g/10 min @Load 11.0 lb, Temperature 527 °F |
ISO 1133 |
Azoty Tarnow™ Tarnamid® T-29 MS Polyamide 6 - Natural Medium-high viscosity extrusion grade for mono or multilayer blown film, including biaxial oriented films, also for production of monofilament; can be used for injection molding and compounding.For .. |
|||
Melt Flow | 50 g/10 min @Load 5.00 kg, Temperature 275 °C |
50 g/10 min @Load 11.0 lb, Temperature 527 °F |
ISO 1133 |
Azoty Tarnow™ Tarnamid® T-29 Polyamide 6 - Natural Medium-high viscosity extrusion grade for mono or multilayer blown film, including biaxial oriented films, also for production of monofilament; can be used for injection molding and compounding.Tarn.. |
|||
Melt Flow | 50 g/10 min @Load 5.00 kg, Temperature 275 °C |
50 g/10 min @Load 11.0 lb, Temperature 527 °F |
ISO 1133 |
Azoty Tarnow™ Tarnamid® T-27 MT30 Polyamide 6 - Mineral Reinforced 30% Mineral filled, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main properties:High mechani.. |
|||
Melt Flow | 50 g/10 min @Load 2.16 kg, Temperature 230 °C |
50 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Braskem TI6500WV High Impact Copolymer Polypropylene Description: High melt flow, superior low temperature impact, nucleated, good mold release, antistatic.Applications: Suggested uses include compounding, furniture, toys, packaging, large part inject.. |