Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 31 g/10 min @Load 5.00 kg, Temperature 260 °C |
31 g/10 min @Load 11.0 lb, Temperature 500 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
SABIC Innovative Plastics Cycoloy® C4215HF PC+ABS (Europe-Africa-Middle East) Cycoloy C4215HF is a 15% glass reinforced, non-FR PC+ABS grade with high heat resistance, excellent strength and rigidity with good cosmetic apprearance. It combines good processability with a low s.. |
|||
Melt Flow | 31 g/10 min @Load 2.16 kg, Temperature 260 °C |
31 g/10 min @Load 4.76 lb, Temperature 500 °F |
ASTM D1238 |
SABIC Innovative Plastics Cycoloy® CY2010 PC+ABS (Europe-Africa-Middle East) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow for a wide variety of thin wall or large size applicat.. |
|||
Melt Flow | 31 g/10 min @Load 2.16 kg, Temperature 260 °C |
31 g/10 min @Load 4.76 lb, Temperature 500 °F |
ASTM D1238 |
SABIC Innovative Plastics Cycoloy® CY5005 PC+ABS Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow for a wide variety of thin wall or large size applicat.. |
|||
Melt Flow | 31 g/10 min @Load 5.00 kg, Temperature 200 °C |
31 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
PolyOne Dynaflex™ G7630-1 (Natural) Thermoplastic Elastomer (TPE) Dynaflex™ G7630-1 (Natural) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Non-Slip Grip - Overmold Adhe.. |
|||
Melt Flow | 31 g/10 min @Load 5.00 kg, Temperature 200 °C |
31 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
PolyOne Dynaflex™ G7630-9 (Black) Thermoplastic Elastomer (TPE) Dynaflex™ G7630-9 (Black) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. *Made with Kraton® Polymer - Non.. |
|||
Melt Flow | 31 g/10 min | 31 g/10 min | ASTM D1238 |
Kolon KOCETAL® WR701 Wear Modified Acetal Resin Improved weather resistant and easy flow grade. Applications: Weather resistant products. Information provided by API-Kolon. |
|||
Melt Flow | 31 g/10 min @Load 2.16 kg, Temperature 270 °C |
31 g/10 min @Load 4.76 lb, Temperature 518 °F |
Estimated using room temperature density; ISO 1133 |
Lanxess Pocan® DP 4035 000000 PBT + PET, 30% Glass Fiber PBT+PET, 30% glass fibers, injection molding, halogen free flame retardant |
|||
Melt Flow | 31 g/10 min @Load 2.16 kg, Temperature 260 °C |
31 g/10 min @Load 4.76 lb, Temperature 500 °F |
Estimated using room temperature density; ISO 1133 |
Lanxess Pocan® DP 7244 000000 PBT, 30% Glass Fiber PBT, 30% glass fibers, injection molding, flame retardant |
|||
Melt Flow | 31 g/10 min @Load 5.00 kg, Temperature 260 °C |
31 g/10 min @Load 11.0 lb, Temperature 500 °F |
ASTM D1238 |
Lucent Polymers PC/PBT-1231 Polycarbonate+PBT, General Purpose, Injection Grade Add "R" for Added ReleaseAdd "U" for UV StabilizerInformation provided by Lucent Polymers, Inc. |
|||
Melt Flow | 31 g/10 min @Load 5.00 kg, Temperature 260 °C |
31 g/10 min @Load 11.0 lb, Temperature 500 °F |
Estimated using room temperature density; ISO 1133 |
Lanxess Pocan® KU 2-7209 Z 000000 PBT, 15% Glass Fiber PBT, 15% glass fibers, injection molding, flame retardant, impact modified |
|||
Melt Flow | <= 31 g/10 min @Load 2.16 kg, Temperature 250 °C |
<= 31 g/10 min @Load 4.76 lb, Temperature 482 °F |
|
Lehmann & Voss LUVOCOM® 1800-7806 PET, with PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Melt Flow | 31 g/10 min @Load 5.00 kg, Temperature 300 °C |
31 g/10 min @Load 11.0 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL TN300 PPE+PS PPE+PS. Transparent. High heat. Color Limited. Injection molding. Laser-Transmission welding applications. |
|||
Melt Flow | 31 g/10 min @Load 10.0 kg, Temperature 220 °C |
31 g/10 min @Load 22.0 lb, Temperature 428 °F |
ISO 1133 |
Styrolution Novodur® M203FC ABS Novodur HD M203FC is an injection molding grade especially suitable for medical applications providing high flowability.Information provided by Styrolution |
|||
Melt Flow | 31 g/10 min @Load 10.0 kg, Temperature 220 °C |
31 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Samsung Cheil Industries Infino® UF-1017B PC, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 31 g/10 min @Load 10.0 kg, Temperature 220 °C |
31 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Samsung Cheil Industries Infino® GC-1150 PC/ABS, FR Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 31 g/10 min @Load 10.0 kg, Temperature 220 °C |
31 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Samsung Cheil Industries Infino® UF-1017B PC, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 31 g/10 min | 31 g/10 min | ASTM D1238 |
Samyang Trimma® SD6320P PMMA, Translucent High scratch resistance; stability against weak acids, strong acids, weak alkalis and inorganic salts.Information provided by Samyang. |
|||
Melt Flow | 31 g/10 min @Load 10.0 kg, Temperature 220 °C |
31 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Samsung Cheil Industries Infino® GC-1150 PC/ABS, FR Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 31 g/10 min | 31 g/10 min | ASTM D1238 |
Total PPH M3865 Metallocene Isostatic Propylene Polymer, Fiber Grade M3865 is an isostatic form of polypropylene made via ATOFINA proprietary technology.Recommended Applications. M3865 is recommended for melt spun and spunbond fiber applications. However, due to it.. |
|||
Melt Flow | 31 g/10 min @Load 2.16 kg, Temperature 330 °C |
31 g/10 min @Load 4.76 lb, Temperature 626 °F |
ISO 1133 |
Covestro Apec® 1797 High-Heat Polycarbonate This linear, amorphous copolycarbonate is most suitable for applications that must withstand high temperatures and exhibit toughness, impact resistance and high transparency. These properties, along.. |
|||
Melt Flow | 31 g/10 min @Load 5.00 kg, Temperature 260 °C |
31 g/10 min @Load 11.0 lb, Temperature 500 °F |
estimated from MVR using room temperature density; ISO 1133 |
Covestro Bayblend® W85 XF* Polycarbonate + ASA Developmental product(PC+ASA) blendinjection molding grade with improved weather resistanceoptimized heat ageing stabilityhigh heat resistanceVicat/B 120 = 132 °CPreprocessingMax. Water content |
|||
Melt Flow | 31 g/10 min @Load 2.16 kg, Temperature 230 °C |
31 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
ExxonMobil Exxtral™ BMV 102W Performance Polyolefin Product Description: Polyolefin injection molding compound with high flow, good low-temperature impact resistance, and excellent processability for painted, partial painted, and molded-in-color auto.. |
|||
Melt Flow | 31 g/10 min @Load 2.16 kg, Temperature 230 °C |
31 g/10 min @Load 4.76 lb, Temperature 446 °F |
Calculated from Volume Flow Rate of 25 cm<sup>3</sup>/10 min; ISO 1133 |
DSM Arnitel® EL630 63 Shore D, Injection Grade Copolyester Elastomer (North America) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Melt Flow | 31 g/10 min @Load 2.16 kg, Temperature 230 °C |
31 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Braskem TR3350CW Random Copolymer Polypropylene Description: Excellent mold release, superior color and processing stability, high melt flow, excellent processability, clarified.Applications: Suggested uses include housewares, fast-cycle injectio.. |
|||
Melt Flow | 31 g/10 min @Load 2.16 kg, Temperature 230 °C |
31 g/10 min @Load 4.76 lb, Temperature 446 °F |
|
BASF Novolen® 1100 RC Polypropylene, Injection Molding Grade Injection molded partsData was collected by ISO methods and provided by BASF. |
|||
Melt Flow | 31 g/10 min @Load 5.00 kg, Temperature 230 °C |
31 g/10 min @Load 11.0 lb, Temperature 446 °F |
ISO 1133 |
Multibase Multibatch® MP 52255 Injection Molding HPP. 70% CaCO3 Filled.Information provided by Multibase |
|||
Melt Flow | 31 g/10 min @Load 2.16 kg, Temperature 190 °C |
31 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Borealis MG9601 Polyethylene MG9601 is a natural high-density polyethylene with high melt-index and narrow molecular weight distribution, which is produced in a low-pressure gas-phase process. The grade is characterized by exce.. |
|||
Melt Flow | 31 g/10 min @Load 2.16 kg, Temperature 230 °C |
31 g/10 min @Load 4.76 lb, Temperature 446 °F |
|
BASF Novolen® 1148 RC Polypropylene Nucleated grade with antistatic agent for injection molded parts.Data was collected by ISO methods and provided by BASF. |
|||
Melt Flow | 31 g/10 min @Load 2.16 kg, Temperature 230 °C |
31 g/10 min @Load 4.76 lb, Temperature 446 °F |
|
BASF Novolen® 3248 RC Polypropylene Grade containing nucleating and antistatic agents for injection molded parts.Data was collected by ISO methods and provided by BASF. |
|||
Melt Flow | 31 g/10 min @Load 2.16 kg, Temperature 260 °C |
31 g/10 min @Load 4.76 lb, Temperature 500 °F |
Estimated using room temperature density; ISO 1133 |
Lanxess Pocan® KU 2-7209 Z 901510 PBT, 15% Glass Fiber PBT, injection molding grade with 15% glass fibers, elastomer modified, UL 94V0 at 0.8 mm (all colors-in house test), UL-listed from 1.5mm thickness. |