Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 3.3 g/10 min @Load 2.16 kg, Temperature 230 °C |
3.3 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
SABIC PS 160 General Purpose Polystyrene for Foam Extrusion Product Description: General purpose Polystyrene PS 160 is manufactured by continuous mass polymerization of styrene monomer. It is a crystal-like, hard and brittle material having High molecular .. |
|||
Melt Flow | 3.3 g/10 min @Load 5.00 kg, Temperature 200 °C |
3.3 g/10 min @Load 11.0 lb, Temperature 392 °F |
Procedure A Condition G; ASTM D1238 |
Network Polymers MS 150 Styrene Methyl Methacrylate Terpolymer Description: Styrene Methyl Methacrylate TerpolymerInformation provided by Network Polymers Inc. |
|||
Melt Flow | 3.3 g/10 min @Load 3.80 kg, Temperature 230 °C |
3.3 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
SABIC Innovative Plastics Cycolac® BDT6500 ABS AUTOMOTIVE. Low gloss, color concentratable for interior applications. Natural only. |
|||
Melt Flow | 3.3 g/10 min @Load 2.16 kg, Temperature 190 °C |
3.3 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil Escorene® LL-8461 LLDPE, Rotational Molding Powder
(discontinued **) Data Provided by Exxon Chemical Canada.Characteristics: Fully formulated, UV-8 type protection, Good stiffnessUses: Septic tanks, Chemical storage bins, Potable water tanks |
|||
Melt Flow | 3.3 g/10 min @Load 2.16 kg, Temperature 230 °C |
3.3 g/10 min @Load 4.76 lb, Temperature 446 °F |
Condition L; ASTM D1238 |
PolyMirae Moplen HP450J Stretch/Yarn, Monofilament Grade Polypropylene Moplen HP450J is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP450J is a homopolymer typically used by customers in Raffia and Y.. |
|||
Melt Flow | 3.3 g/10 min | 3.3 g/10 min | Exxon Method |
ExxonMobil Escorene® LL-8461 LMDPE Rotational Molding Grade
(discontinued **) Data provided by the manufacturer, Exxon Chemical.LL-8400 series are linear medium density polyethylene resins that provide outstanding environmental stress crack resistance. LL-8461 is fully formu.. |
|||
Melt Flow | 3.3 g/10 min @Load 2.16 kg, Temperature 190 °C |
3.3 g/10 min @Load 4.76 lb, Temperature 374 °F |
|
LyondellBasell Lupolen® 5236 HX HDPE, Impact Grade Medium flow, impact resistant, high stress-crack resistant grade for closures for bottles that contain carbonated liquids. This product contains a slip agent.Data was collected by ISO methods and o.. |
|||
Melt Flow | 3.3 g/10 min @Load 2.16 kg, Temperature 250 °C |
3.3 g/10 min @Load 4.76 lb, Temperature 482 °F |
|
Lehmann & Voss LUVOCOM® 6-8512 Polyamide 12, with carbon fiber, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Especially suitable at dynamic.. |
|||
Melt Flow | 3.3 g/10 min @Load 2.16 kg, Temperature 250 °C |
3.3 g/10 min @Load 4.76 lb, Temperature 482 °F |
ASTM D1238 |
LG Chemical LUPOY GP5006BH PC/ABS, Heat Resistance, Impact Strength Description: Injection Molding, PC/ABS, Heat Resistance, Impact Strength, High ToughnessApplication: Miscellaneous GoodsCAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical.. |
|||
Melt Flow | 3.3 g/10 min @Load 5.00 kg, Temperature 200 °C |
3.3 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
IRPC Polimaxx Polene 330PC Styrene Acrylonitrile APPLICATIONS: INJECTION MOLDING, HOUSEHOLD PRODUCTS : SANITARY WARE, AUTOPART APPLICATION : LAMP ELECTRICAL APPLIANCES : ELECTRICAL FAN |
|||
Melt Flow | 3.3 g/10 min @Load 21.6 kg, Temperature 150 °C |
3.3 g/10 min @Load 47.6 lb, Temperature 302 °F |
ASTM D1238 |
Solvay Specialty Polymers Cogegum® AFR/710 Polyolefin Cogegum® HFFR -Halogen Free Fire Retardant compound. Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties witho.. |
|||
Melt Flow | 3.3 g/10 min @Load 10.0 kg, Temperature 260 °C |
3.3 g/10 min @Load 22.0 lb, Temperature 500 °F |
ASTM D1238 |
Techmer ES Plastiblend® ABS/PA 1700 B1 Availability: North AmericaForms: PelletsAppearance: Natural ColorInformation provided by TP Composites, Inc. |
|||
Melt Flow | 3.3 g/10 min @Load 5.00 kg, Temperature 200 °C |
3.3 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Samsung Cheil Industries Starex® HF-0660I ABS, Unreinforced Material with high flowability and high stiffness that can be used for vacuum cleaner, telephone, TV, VCR, calculator, radio and air-conditionerInformation provided by Samsung Cheil Industries. |
|||
Melt Flow | 3.3 g/10 min @Load 5.00 kg, Temperature 200 °C |
3.3 g/10 min @Load 11.0 lb, Temperature 392 °F |
ISO 1133 |
Styrolution PS 158 N/L GPPS Styrolution PS 158N/L is a heat resistant, rapid freezing general purpose grade. It is suitable for expanded sheet and film; for blends with high impact polystyrene in heat contact applications; for.. |
|||
Melt Flow | 3.3 g/10 min @Load 2.16 kg, Temperature 230 °C |
3.3 g/10 min @Load 4.76 lb, Temperature 446 °F |
|
Silon Tabond 5010 Adhesive Resin Tabond 5010 is a a chemically modified Polypropylene. This grade is for sheets and bottles composed of Polypropylene (PP) and EVOH or PA.Characteristics: • Strong adhesion to PA / PP and EVOH /.. |
|||
Melt Flow | 3.3 g/10 min @Load 5.00 kg, Temperature 200 °C |
3.3 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Samsung Cheil Industries Starex® HG-0760 ABS, Unreinforced Used in telephones, vacuum cleaners and electric fan standsInformation provided by Samsung Cheil Industries. |
|||
Melt Flow | 3.3 g/10 min @Load 3.80 kg, Temperature 230 °C |
3.3 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
PlastxWorld CEVIAN®-V 450 ABS Heat Resistant ABSThese are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |
|||
Melt Flow | 3.3 g/10 min | 3.3 g/10 min | 2.16/190; ASTM D1238 |
A. Schulman SUPERLINEAR™ XL 0360 Rotational Molding Resin DescriptionSuperlinear XL 0360 is compounded rotational molding resin based on metallocean catalyst technology. This technology allows for high impact and excellent stiffness. It is typically used.. |
|||
Melt Flow | 3.3 g/10 min | 3.3 g/10 min | 2.16/190; ASTM D1238 |
A. Schulman SUPERLINEAR™ XL 0360 Rotational Molding Resin DescriptionSuperlinear XL 0360 is compounded rotational molding resin based on metallocean catalyst technology. This technology allows for high impact and excellent stiffness. It is typically used.. |
|||
Melt Flow | 3.3 g/10 min @Load 2.16 kg, Temperature 230 °C |
3.3 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Borealis Xmod™ GD302HP Polypropylene, Glass Fiber Reinforced Xmod™ GD302HP is a 30 % chemically coupled high performance glass fiber reinforced polypropylene compound intended for injection molding. This material has an excellent balance between impact stre.. |
|||
Melt Flow | 3.3 g/10 min | 3.3 g/10 min | 2.16/190; ASTM D1238 |
A. Schulman SUPERLINEAR™ XL 0360 Rotational Molding Resin DescriptionSuperlinear XL 0360 is compounded rotational molding resin based on metallocean catalyst technology. This technology allows for high impact and excellent stiffness. It is typically used.. |
|||
Melt Flow | 3.3 g/10 min | 3.3 g/10 min | 2.16/190; ASTM D1238 |
A. Schulman SUPERLINEAR™ XL 0360 Rotational Molding Resin DescriptionSuperlinear XL 0360 is compounded rotational molding resin based on metallocean catalyst technology. This technology allows for high impact and excellent stiffness. It is typically used.. |
|||
Melt Flow | 3.3 g/10 min @Load 2.16 kg, Temperature 190 °C |
3.3 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil LL 8460.29 Rotational Molding Resin Product Description: LL 8460 is a linear low density hexene copolymer designed to offer excellent ESCR and toughness. This resin is ideally suited for applications that require the optimum balance o.. |
|||
Melt Flow | 3.3 g/10 min @Load 2.16 kg, Temperature 190 °C |
3.3 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil LLDPE LL 8460.29 Linear Low Density Polyethylene Resin Product Description: LL 8460 is a linear low density hexene copolymer designed to offer excellent ESCR and toughness. This resin is ideally suited for applications that require the optimum balance o.. |
|||
Melt Flow | 3.3 g/10 min @Load 2.16 kg |
3.3 g/10 min @Load 4.76 lb |
Melt flow ratio I10/I2 is 7.7. |
Dow ATTANE™ 4202 Ultra Low Density Polyethylene, Cast Film Grade ATTANE® 4202 copolymer is an ultra low density polyethylene having excellent tear and puncture resistance with good optics. It is designed for cast films used in food packaging applications. It com.. |
|||
Melt Flow | 3.3 g/10 min @Load 2.16 kg, Temperature 230 °C |
3.3 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Braskem H 502HC Thermoforming Polypropylene Homopolymer Disposable cupware and dishware; High-stiffness parts; Hot packaging.Information provided by Braskem. |
|||
Melt Flow | 3.3 g/10 min @Load 2.16 kg, Temperature 190 °C |
3.3 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Azoty Tarnow™ TARNOFORM 300 GF6 BK POM 30% glass fiber reinforced injection molding grade, suitable for applications where increased strength and stiffness is required.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A... |
|||
Melt Flow | 3.3 g/10 min @Load 10.0 kg, Temperature 260 °C |
3.3 g/10 min @Load 22.0 lb, Temperature 500 °F |
ASTM D1238 |
Techmer ES Plastiblend® ABS/PA 1700 Availability: North AmericaForms: PelletsAppearance: Natural ColorInformation provided by TP Composites, Inc. |
|||
Melt Flow | 3.3 g/10 min | 3.3 g/10 min | (Condition I) ASTM D-1238-94a |
Multibase Multi-ABS 3632 High Heat Resistant Data provided by Multibase. |