Polymer Property : Melt Flow = 21 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 21 g/10 min

@Load 10.0 kg,
Temperature 190 °C
21 g/10 min

@Load 22.0 lb,
Temperature 374 °F
ISO 1133
Multibase TPSiV® 4000-70A Thermoplastic Elastomer
FEATURES & BENEFITS: Soft silky feel; Excellent abrasion and scratch resistance; Excellent bonding to PC, ABS; UV stableAPPLICATIONS: Solution for soft touch overmolding on consumer electronics, mob..
Melt Flow 21 g/10 min

@Load 2.16 kg,
Temperature 230 °C
21 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
RheTech Products HP513-01 High Stiffness Polypropylene Copolymer, Medium Impact, UV Stabilized, Black
Applications: Interior trimI/P componentsCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products.
Melt Flow 21 g/10 min

@Load 2.16 kg,
Temperature 260 °C
21 g/10 min

@Load 4.76 lb,
Temperature 500 °F
ASTM D1238
SABIC Innovative Plastics Cycoloy® CY6012 PC+ABS (Asia Pacific)
Cycoloy* resin grade CY6012 is an injection moldable PC/ABS blend with non-brominated and non-chlorinated flame retardant systems. Excellent impact/flow balance together with a UL-94 V0 & 5VB rating..
Melt Flow 21 g/10 min

@Load 2.16 kg,
Temperature 260 °C
21 g/10 min

@Load 4.76 lb,
Temperature 500 °F
ASTM D1238
SABIC Innovative Plastics Cycoloy® RCY6214 PC+ABS (Asia Pacific)
Cycoloy* RCY6214 resin is an injection moldable PC/ABS blend with non-brominated and non-chlorinated flame retardant. It contains 35% post consumer recycle content with a UL-94 V0 rating @ 1.5 mm. D..
Melt Flow 21 g/10 min
21 g/10 min
Condition L 230/2.16; ASTM D1238
Pinnacle Polymers 1120 H Polypropylene Homopolymer, Injection Molding Grade, Nucleated, with Antistat
This Pinnacle Polymers Polypropylene is made via UNIPOL™ PP technology, which utilizes gas-phase fluidized bed reactors with a high activity catalyst system to ensure uniform physical properties an..
Melt Flow 21 g/10 min
21 g/10 min
ISO 1133
Solvay Engineered Polymers SEQUEL® 1440LS TPO  (discontinued **)
Description: SEQUEL® 1440LS engineered polyolefin material is designed for large automotive exterior applications that require ductile impact properties at low temperatures, excellent processabilit..
Melt Flow 21 g/10 min

@Load 2.16 kg,
Temperature 250 °C
21 g/10 min

@Load 4.76 lb,
Temperature 482 °F
Lehmann & Voss LUVOCOM® 1850-7942/RD PBT, with PTFE, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri..
Melt Flow 21 g/10 min

@Load 2.16 kg,
Temperature 230 °C
21 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Inno-Comp INNOPOL® CS 2-2110 10% Talc-Filled Polypropylene Block-Copolymer
INNOPOL® CS 2-2110 is a 10% talc-filled compound based on polypropylene block-copolymer. This grade is available in nature and custom colored form.INNOPOL® CS 2-2110 is developed for producing..
Melt Flow 21 g/10 min

@Load 2.16 kg,
Temperature 230 °C
21 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
LG Chemical LUPOL MC4352 PP+Rubber+MF
Description: Injection Molding, PP+Rubber+MF, Good Dimensional Stability, Scratch resistance, Good Weatherability, High ImpactApplication: Automotive Exterior (Sill Side Molding, Door Garnish)CAS: 9..
Melt Flow 21 g/10 min
21 g/10 min
ISO 1133
Iran Petrochemical (PCC) EPV 31 RA Polypropylene
A high fluidity heterophasic copolymer for thin wall injection molding exhibits high stiffness, relatively good impact residence.Applications: flower pots, containers, filters, house wares.Informati..
Melt Flow 21 g/10 min

@Load 2.16 kg,
Temperature 230 °C
21 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
SABIC Innovative Plastics SABIC PPCOMPOUND 8620A PP
SABIC® PPcompound 8620A is a mineral filled, impact modified polypropylene TPO. It was originally designed for painted automotive bumper fascia applications where a combination of good flow, hig..
Melt Flow 21 g/10 min

@Load 2.16 kg,
Temperature 250 °C
21 g/10 min

@Load 4.76 lb,
Temperature 482 °F
ASTM D1238
SABIC Innovative Plastics Valox® HX3091HP PBT
PBT for compounding/fibers only. Not intended for injection molding. Biocompatible. Melt viscosity at 250C and 21.6kgf is 3500-4500 poise. Available in Natural color (1001) only.
Melt Flow 21 g/10 min

@Load 2.16 kg,
Temperature 265 °C
21 g/10 min

@Load 4.76 lb,
Temperature 509 °F
ASTM D1238
SABIC Innovative Plastics XYLEX X7300 PC+POLYESTER (Asia Pacific)
PC+POLYESTER unreinforced alloy. High flow, chemically resistant with excellent optical quality. UV-stabilized.
Melt Flow 21 g/10 min

@Load 2.16 kg,
Temperature 300 °C
21 g/10 min

@Load 4.76 lb,
Temperature 572 °F
ASTM D1238
SABIC Innovative Plastics LNP THERMOCOMP DF00A1P PC (Asia Pacific)
LNP* Thermocomp* DF00AIP is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: High Modulus, low warpage, Non-Brominated & Non..
Melt Flow 21 g/10 min

@Load 2.16 kg,
Temperature 250 °C
21 g/10 min

@Load 4.76 lb,
Temperature 482 °F
ASTM D1238
Samsung Cheil Industries Infino® NF-3017 PC/ABS, Unreinforced FR
Flame-retardant scratch resistant material that can be used in notebook B partInformation provided by Samsung Cheil Industries.
Melt Flow 21 g/10 min

@Load 2.16 kg,
Temperature 250 °C
21 g/10 min

@Load 4.76 lb,
Temperature 482 °F
ASTM D1238
Samsung Cheil Industries Infino® VB-5150GL PBT, 15% Glass Filled FR
Information provided by Samsung Cheil Industries.
Melt Flow 21 g/10 min

@Load 5.00 kg,
Temperature 260 °C
21 g/10 min

@Load 11.0 lb,
Temperature 500 °F
ASTM D1238
Samsung Cheil Industries Infino® AE-2130 PC/PET, Unreinforced
Information provided by Samsung Cheil Industries.
Melt Flow 21 g/10 min

@Load 2.16 kg,
Temperature 230 °C
21 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
A. Schulman POLYFORT™ FPP 1876 22% Mineral Filled Copolymer, UV Inhibited Polypropylene
DescriptionPolyfort® FPP 1876 is a 22% mineral filled copolymer UV Inhibited Polypropylene. It is high flow. Information provided by A. Schulman.
Melt Flow 21 g/10 min

@Load 2.16 kg,
Temperature 190 °C
21 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
A. Schulman POLYBATCH™ Cedar 10310U Concentrate Based In LLDPE
DescriptionPOLYBATCH® Cedar 10310U is a cedar color concentrate containing an optimized blend of color and UV stabilizer based in LLDPE. This concentrate was designed to provide color and UV stabi..
Melt Flow 21 g/10 min

@Load 2.16 kg,
Temperature 230 °C
21 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
A. Schulman POLYFORT™ FPP 1876 22% Mineral Filled Copolymer, UV Inhibited Polypropylene
DescriptionPolyfort® FPP 1876 is a 22% mineral filled copolymer UV Inhibited Polypropylene. It is high flow. Information provided by A. Schulman.
Melt Flow 21 g/10 min

@Load 2.16 kg,
Temperature 190 °C
21 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
A. Schulman POLYBATCH™ Red 5500 Concentrate Based In Polyethylene
DescriptionPOLYBATCH® 5500 is a red color concentrate based in polyethylene. This concentrate was designed to provide color in polyolefin film and molding applications. POLYBATCH® 5500 is heavy ..
Melt Flow 21 g/10 min

@Load 2.16 kg,
Temperature 190 °C
21 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
A. Schulman POLYBATCH™ Red 5500 Concentrate Based In Polyethylene
DescriptionPOLYBATCH® 5500 is a red color concentrate based in polyethylene. This concentrate was designed to provide color in polyolefin film and molding applications. POLYBATCH® 5500 is heavy ..
Melt Flow 21 g/10 min

@Load 2.16 kg,
Temperature 230 °C
21 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Entec Hypro™ PP-HP20NS Homopolymer, 20 Melt Flow, Nucleated, Anti-stat
This product is intended for general purpose injection molding applications such as cutlery, caps and closures, and thin-wall containers.Information provided by Entec
Melt Flow 21 g/10 min
21 g/10 min
ASTM D1238
Aclo Accutech Polypropylene Homopolymer HP0339C30L Calcium Reinforced
Melt Flow 21 g/10 min
21 g/10 min
ASTM D1238
Aclo Accutech Polypropylene Homopolymer HP0339C30L1 Calcium Reinforced
Melt Flow 21 g/10 min
21 g/10 min
ASTM D1238
Aclo Accutech Polypropylene Homopolymer HP0339W20L1 Wollastonite Reinforced
Melt Flow 21 g/10 min

@Load 10.0 kg,
Temperature 220 °C
21 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D-1238
Bhansali Engineering Abstron IM-29 ABS Injection Molding Grade
High Impact, Medium, High Flow, General PurposeInformation provided by Bhansali
Melt Flow 21 g/10 min

@Load 5.00 kg,
Temperature 300 °C
21 g/10 min

@Load 11.0 lb,
Temperature 572 °F
ASTM D1238
BLUESTAR LXS 314 G10 PPE-HIPS, 10% Glass Filled
Typical Applications: Water industrial partsInformation provided by Polymer Technology and Services, LLC (PTS).
Melt Flow 21 g/10 min
21 g/10 min
ASTM D1238
Aclo Accutech Polypropylene Homopolymer HP0339T20L Talc Reinforced
Melt Flow 21 g/10 min
21 g/10 min
(Condition L) ASTM D-1238
Multibase Multi-Flex® TPE A 6404 BLK
Ash is 41%. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.