Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 10 g/10 min | 10 g/10 min | (Condition L) ASTM D-1238-94a |
Multibase Multi-Pro® 1010 C Natural 10% Filler Content Polypropylene Data provided by Multibase. |
|||
Melt Flow | 10 g/10 min @Load 0.325 kg, Temperature 270 °C |
10 g/10 min @Load 0.716 lb, Temperature 518 °F |
|
Plastcom SLOVASTER® B/A GF 30 PBT, 30% glass fibre FeaturesPBT/ASA for injection moulding, chemically reinforced with 30% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and ben.. |
|||
Melt Flow | 10 g/10 min @Load 1.20 kg, Temperature 300 °C |
10 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® HPX4 PC Copolymer Medium flow specialty polycarbonate - improved processability & autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP.. |
|||
Melt Flow | 10 g/10 min @Load 1.20 kg, Temperature 300 °C |
10 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® SLX2432T PC Copolymer (Asia Pacific) Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colors. |
|||
Melt Flow | 10 g/10 min @Load 0.325 kg, Temperature 270 °C |
10 g/10 min @Load 0.716 lb, Temperature 518 °F |
|
Plastcom SLOVALEN PC 69 GF 40 PP, 40% glass beads, mod. of mech. properties FeaturesModified copolymer PP for injection moulding, chemically reinforced with 40% glass fibre, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP. A.. |
|||
Melt Flow | 10 g/10 min @Load 5.00 kg, Temperature 200 °C |
10 g/10 min @Load 11.0 lb, Temperature 392 °F |
G; ASTM D1238 |
Resirene Resirene® READ 9500 Ignition Resistant Impact Polystyrene Features:High FlowIgnition ResistantNo Pre-drying RequiredHigh ImpactColors AvailableApplications:Injection MoldingDark ColorsTV CabinetsElectronic EquipmentInformation provided by US distributor Ca.. |
|||
Melt Flow | 10 g/10 min @Load 2.16 kg, Temperature 230 °C |
10 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Reliance Industries Repol T100MK Polypropylene REPOL Polypropylene T100MK is manufactured using Unipol PP process which combines the production efficiency of gas phase fluidized bed reactor technology with the high activity stereospecific cataly.. |
|||
Melt Flow | 10 g/10 min | 10 g/10 min | 230/2.16 (typical); ASTM D1238 |
Fiberfil® PP-60/TC/20/FD Polypropylene Homopolymer, 20% Talc Filled, FDA compliant Information provided by FIBERFIL Engineered Plastics |
|||
Melt Flow | 10 g/10 min @Load 2.16 kg, Temperature 190 °C |
10 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
LG Chemical LUCEL GC225 POM+GF25%, High Rigidity Feature: Injection Molding, POM+GF25%, High RigidityApplication: Casings of Pump and Pivot BearingsCAS No. 66455-31-0 and 65997-17-3Information provided by LG Chemical |
|||
Melt Flow | 10 g/10 min @Load 2.16 kg, Temperature 230 °C |
10 g/10 min @Load 4.76 lb, Temperature 446 °F |
L; ASTM D1238 |
Global PCC-0310 Standard Grade Polypropylene Information provided by Global Polymers Corporation. |
|||
Melt Flow | 10 - 13 g/10 min @Load 1.20 kg, Temperature 300 °C |
10 - 13 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
LTL Color Compounds ColorRxâ„¢ PC-1005ARX Biocompatible Polycarbonate A biocompatible, 10 melt grade of Polycarbonate for healthcare applications, containing a high level of antimicrobial protection for FDA regulated medical devices.All information provided by LTL Col.. |
|||
Melt Flow | 10 g/10 min @Load 2.16 kg, Temperature 230 °C |
10 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Lucent Polymers CPP-0107 Polypropylene Homopolymer Recycled ContentAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Melt Flow | 10 g/10 min @Load 21.6 kg |
10 g/10 min @Load 47.6 lb |
|
Lubrizol Advanced Materials PEARLCOAT® 163K Thermoplastic Polyurethane Elastomer PEARLCOAT® 163K is a polyether based TPU, supplied in form of translucent, colorless pellets, combining hardness with excellent low temperature flexibility and very good hydrolysis resistance. PE.. |
|||
Melt Flow | 10 g/10 min @Load 10.0 kg, Temperature 250 °C |
10 g/10 min @Load 22.0 lb, Temperature 482 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL WCA901 PPE-TPE (Asia Pacific) Non-Halogenated flame retardant, flexible Noryl resin intended for evaluation in wire and cable applications, capable of meeting VW-1 and 105°C end use temperature requirements as defined by UL.. |
|||
Melt Flow | 10 g/10 min @Load 21.6 kg, Temperature 230 °C |
10 g/10 min @Load 47.6 lb, Temperature 446 °F |
ASTM D1238 |
Solvay Specialty Polymers Solef® 460/461 Polyvinylidene Fluoride (PVDF) Solef® 460/461 PVDF homopolymer has high melt viscosity and is typically processed by extrusion.Features: High Viscosity; HomopolymerAdditional Properties: Crystallization Heat - ASTM D3418 46.0 .. |
|||
Melt Flow | 10 g/10 min @Load 2.16 kg, Temperature 250 °C |
10 g/10 min @Load 4.76 lb, Temperature 482 °F |
ASTM D1238 |
Samsung Cheil Industries Infino® GP-5400G PBT, 40% Glass Filled Material with 40% GF reinforcement that is used in motor insulatorsInformation provided by Samsung Cheil Industries. |
|||
Melt Flow | 10 g/10 min @Load 1.20 kg, Temperature 300 °C |
10 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
Styron EMERGEâ„¢ 4610-10 Polycarbonate EMERGEâ„¢ PC 4610-10 advanced resin is formulated to deliver both outstanding clarity and enhanced ignition resistance while maintaining excellent physical properties and processability. Applica.. |
|||
Melt Flow | 10 g/10 min @Load 2.16 kg, Temperature 230 °C |
10 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex MONPRENE® MP 2770 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Melt Flow | 10 g/10 min | 10 g/10 min | ASTM D1238 |
A. Schulman POLYFORT™ FPP1666 Talc Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 1666 is a 10% talc filled homopolymer polypropylene compound. Information provided by A. Schulman. |
|||
Melt Flow | 10 g/10 min @Load 2.16 kg, Temperature 190 °C |
10 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
A. Schulman POLYBATCH™ Green 3011E Concentrate Based In Polyethylene DescriptionPOLYBATCH® 3011E is a green color concentrate based in polyethylene. This concentrate was designed to provide color in polyolefin film and molding applications. POLYBATCH® 3011E is he.. |
|||
Melt Flow | 10 g/10 min | 10 g/10 min | ASTM D1238 |
A. Schulman POLYFORT™ FPP 3715 Glass Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 3715 is a 15% glass filled homopolymer polypropylene product. Information provided by A. Schulman. |
|||
Melt Flow | 10 g/10 min | 10 g/10 min | ASTM D1238 |
A. Schulman POLYFORT™ FPP1666 Talc Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 1666 is a 10% talc filled homopolymer polypropylene compound. Information provided by A. Schulman. |
|||
Melt Flow | 10 g/10 min @Load 2.16 kg, Temperature 190 °C |
10 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
A. Schulman POLYBATCH™ Red 5330 Concentrate Based In Polyethylene DescriptionPOLYBATCH® 5330 is a red color concentrate based in polyethylene. This concentrate was designed to provide color in polyolefin film and molding applications. POLYBATCH® 5330 is heavy .. |
|||
Melt Flow | 10 g/10 min | 10 g/10 min | ASTM D1238 |
A. Schulman POLYFLAM™ FLP 3714 20% Glass Filled HDPE DescriptionPolyfort® FLP 3714 is a 20% glass filled HDPE product. Information provided by A. Schulman. |
|||
Melt Flow | 10 g/10 min @Load 2.16 kg, Temperature 230 °C |
10 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
A. Schulman POLYFORT™ FPP 1640 Glass Reinforced, Mineral Fortified Homopolymer Polypropylene DescriptionPolyfort® FPP 1640 is a high stiffness, high heat hybrid glass reinforced mineral fortified homopolymer polypropylene.Information provided by A. Schulman. |
|||
Melt Flow | 10 - 25 g/10 min @Load 8.70 kg, Temperature 170 °C |
10 - 25 g/10 min @Load 19.2 lb, Temperature 338 °F |
|
Lubrizol ESTANE® GP65AE Ester Based Thermoplastic Polyurethane Type: Estane® GP 65AE is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b.. |
|||
Melt Flow | 10 g/10 min @Load 2.16 kg, Temperature 190 °C |
10 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
A. Schulman POLYBATCH™ Green 3373 Concentrate Based In Polyethylene DescriptionPOLYBATCH® 3373 is a green color concentrate based in polyethylene. This concentrate was designed to provide color in polyolefin film and molding applications. POLYBATCH® 3373 is typi.. |
|||
Melt Flow | 10 g/10 min | 10 g/10 min | ISO 1133 |
Addiplast Addilene H 490 M40F Flame Retardant Polypropylene, 40% Mineral Filled Flame retardant, mineral filled, with halogensInformation provided by Addiplast. |
|||
Melt Flow | 10 g/10 min | 10 g/10 min | |
Toyobo GLAMIDE® T-779 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |