Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 1.25 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.25 g/10 min @Load 4.76 lb, Temperature 446 °F |
Condition L; ASTM D1238 |
PolyMirae Moplen HP640G Sheet and Thermoforming Grade Polypropylene Moplen HP640G is the polypropylene Homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP640G is a homopolymer particularly suitable for sheet and thermof.. |
|||
Melt Flow | 1.25 g/10 min | 1.25 g/10 min | ExxonMobil Method |
ExxonMobil Exceed™ 1318CA Blown Film Resin
(discontinued **) Exceed 1318CA resin is a hexene copolymer produced using ExxonMobil Chemicals EXXPOL® Technology. Films made from 1318CA resin have outstanding tensile, impact strength and puncture. These superi.. |
|||
Melt Flow | 1.25 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.25 g/10 min @Load 4.76 lb, Temperature 446 °F |
Condition L; ASTM D1238 |
PolyMirae Moplen HP500G Sheet and Thermoforming Grade Polypropylene Moplen HP500G is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP500G is a homopolymer particularly suitable for sheet, thermofor.. |
|||
Melt Flow | 1.25 g/10 min | 1.25 g/10 min | ASTM D1238 |
Westlake EF444 4.7% Ethylene Vinyl Acetate Copolymer
(discontinued **) Excellent haze and gloss, excellent impact strength and very good sealability.Application/UsesHigh clarity packagingHigh impactFDA: This material complies with FDA regulations in 21 CFR, section 177.. |
|||
Melt Flow | 1.25 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.25 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Borealis FG5199 Linear Low Density Polyethylene FG5199 is a Butene Linear Low Density Polyethylene for Film Extrusion. Includes antioxidant, anti-Fog and cling additives. The grade is developed for blown cling film. Film made from FG5199 is suit.. |
|||
Melt Flow | 1.25 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.25 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Westlake EF418 Low Density Polyethylene WESTLAKE polyethylene EF418 is a LDPE formula with excellent optical properties suggested by light and medium duty packaging.Application/UsesLight and medium duty produce bagsClarity packagingGenera.. |
|||
Melt Flow | 1.25 g/10 min | 1.25 g/10 min | ExxonMobil Method |
ExxonMobil LD 334.57 Clear, High Impact Film Resin LD 334 resins produce films with superior impact strength, good heat sealability, and low temperature properties.Information provided by ExxonMobil Chemical |
|||
Melt Flow | 1.25 g/10 min | 1.25 g/10 min | ExxonMobil Method |
ExxonMobil LD 334.82 Clear, High Impact Film Resin LD 334 resins produce films with superior impact strength, good heat sealability, and low temperature properties.Information provided by ExxonMobil Chemical |