Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyMirae Moplen HP500G Sheet and Thermoforming Grade Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Sheet/Thermoforming Grade
Manufacturer PolyMirae Company Ltd.
Trade Name Moplen
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyMirae Moplen HP500G Sheet and Thermoforming Grade Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Moplen HP500G is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP500G is a homopolymer particularly suitable for sheet, thermoforming and stripe. Moplen HP500G resin meets the FDA requirements in the Code of Federal Regulations in 21 CFR 178.2010 for food packaging substances with adequate additives. And contains no dangerous substances according to Federal Regulations in 21 CFR 177.1520.Features: Excellent processibility and stretchability; High mechanical properties; High melt strengthApplications: Food packaging and tray (Thermoforming); Bottle (Blow molding); Blown film; High strength for rope, container bag, extruded netsInformation provided by PolyMirae Company Ltd.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 1.25 g/10 min

@Load 2.16 kg,
Temperature 230 °C
1.25 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Condition L; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 100
100
ASTM D785
Tensile Strength, Yield 36.3 MPa
5260 psi
ASTM D638
Elongation at Yield 12 %
12 %
ASTM D638
Flexural Modulus 1.52 GPa
220 ksi
ASTM D790
Izod Impact, Notched 0.490 J/cm
0.918 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 108 °C
226 °F
ASTM D648
Vicat Softening Point 156 °C
313 °F
ASTM D1525
Users viewing this material also viewed the following: