Polymer Property : Melt Flow = 0.30 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 0.30 g/10 min
0.30 g/10 min
Condition 190/2.16; ASTM D1238
Chevron Phillips Marlex® HHM 5502-02 LD High Density Ethylene Hexene Copolymer with Antistat  (discontinued **
High Density Ethylene Hexene Copolymer with AntistatCustomer Benefits: The resin allows the blow molder to reduce inventory of resin types, because it can be used to package bleach and most detergen..
Melt Flow 0.30 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.30 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Chevron Phillips HiD® 9352 HDPE Natural Pipe Resin  (discontinued **)
Resin Type: gas phase linear hexane copolymer; ASTM D3350 Classification 335520A; ASTM D4976 Classification: PE 235, A 55701Applications: corrugated pipe applicationsInformation provided by Chevron ..
Melt Flow 0.30 g/10 min

@Load 2.16 kg,
Temperature 230 °C
0.30 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Condition L; ASTM D1238
NOVA Chemicals Dylark® 250P20 High Performance Glass Filled Styrenic
Very high modulus, High heat resistance, Excellent flow characteristics, Excellent adhesion to urethaneApplications: Instrument panel substrates, consoles, Cluster housing, interior trimInjection Sp..
Melt Flow 0.30 g/10 min

@Load 2.16 kg
0.30 g/10 min

@Load 4.76 lb
ASTM D1238
Reliance Industries Relene F46003 Polyethylene
Relene F46003 is a High Density Polyethylene grade suitable for producing blown parts with superior stiffness and barrier properties. It is recommended for making liners and coextruded film structu..
Melt Flow 0.30 g/10 min
0.30 g/10 min
±30%
Kazanorgsintez 15313-003 High Pressure Polyethylene
Production Method: HDPE is produced by high pressure ethylene polymerization in tubular reactors. Application: Intended for production of bags, pipes, fittings, articles designed for food contac..
Melt Flow 0.30 - 0.65 g/10 min

@Load 5.00 kg
0.30 - 0.65 g/10 min

@Load 11.0 lb
±10% Superior Class, ±15% 1st Class
Kazanorgsintez 271-274K Cable Composition Based on High Density Polyethylene
Production Method: Gaseous-phase method. Application: Compositions are intended for cover insulating lapping, protective covers and cables.Information Provided by Kazanorgsintez
Melt Flow 0.30 - 0.70 g/10 min
0.30 - 0.70 g/10 min
±18%
Kazanorgsintez 298-285 High Density Polyethylene Composite
Production Method: Compositions are achieved by ethylene copolymerization by gaseous-phase method at low pressure using complex catalysts on carrier material. Application: HDPE compositions 296-..
Melt Flow 0.30 - 0.70 g/10 min
0.30 - 0.70 g/10 min
±18%
Kazanorgsintez 298-285D High Density Polyethylene Composite
Production Method: Compositions are achieved by ethylene copolymerization by gaseous-phase method at low pressure using complex catalysts on carrier material. Application: HDPE compositions 296-..
Melt Flow 0.30 g/10 min
0.30 g/10 min
ASTM D1238
LyondellBasell Petrothene® LR732001 High Density Polyethylene (Blow Molding Grade)
ApplicationsThe PETROTHENE LR 7320 series of polyethylene resins exhibits an excellent balance of stiffness and environmental stress crack resistance. Typical applications include bottles for bleac..
Melt Flow 0.30 g/10 min
0.30 g/10 min
ASTM D1238
Hyosung Topilene B200P PP
B200P Applications: Industrial pipesCharacteristics: Chemical resistanceInformation provided by Hyosung Corporation
Melt Flow 0.30 g/10 min
0.30 g/10 min
ASTM D1238
Hyosung Topilene HB240P PP
HB240P Applications:Industrial pipesSewerage pipesCharacteristics:High impact strengthHigh ring stiffnessInformation provided by Hyosung Corporation
Melt Flow 0.30 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.30 g/10 min

@Load 4.76 lb,
Temperature 374 °F
Imerys ImerPlastâ„¢ 15L Recycled Polyolefin for Pipe Extrusion
Polyolefin/Mineral CompoundInformation provided by Imerys.
Melt Flow 0.30 - 1.7 g/10 min

@Load 2.61 kg,
Temperature 190 °C
0.30 - 1.7 g/10 min

@Load 5.75 lb,
Temperature 374 °F
ASTM D1238
LG Chemical SEETEC ES440 Ethylene Vinyl Acetate
Characteristics: Good Mechanical Properties and Good Optical PropertiesApplications: Agricultural Film, Shoe solesCSA No. 24937-78-8Information provided by LG Chemical
Melt Flow 0.30 g/10 min

@Load 5.00 kg,
Temperature 200 °C
0.30 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Techmer ES Plastiblend® ABS E
Availability: North AmericaForms: PelletsFeatures: High ViscosityProcessing Method: Blow Molding and ExtrusionInformation provided by TP Composites, Inc.
Melt Flow 0.30 g/10 min

@Load 2.16 kg,
Temperature 230 °C
0.30 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Borealis BorECO™ BA2000 Polypropylene Block Copolymer for Non-Pressure Pipes
BorECO™ BA2000 is a high molecular weight, low melt flow rate polypropylene block copolymer with a good balance of mechanical properties. This grade offers superior stiffness while keeping good im..
Melt Flow 0.30 g/10 min

@Load 5.00 kg,
Temperature 190 °C
0.30 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ISO 1133
Borealis Borstar® HE3496-LS Yellow Polyethylene Compound for The Coextrusion of Identifying Stripes On Black HD Pipe for Natural Gas
Borstar HE3496-LS is a bimodal, cadmium free, high density polyethylene compound designed for coextrusion of blue identifying stripes. It is fully stabilized against thermal degradation and the die..
Melt Flow 0.30 g/10 min

@Load 5.00 kg,
Temperature 190 °C
0.30 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ISO 1133
Borealis Borstar® HE3498-LS Orange-Yellow Polyethylene Compound for The Coextrusion of Identifying Stripes On Black HD Pipe for Natural Gas
Borstar HE3497-LS is a bimodal, cadmium free, high density polyethylene compound designed for coextrusion of blue identifying stripes. It is fully stabilized against thermal degradation and the die..
Melt Flow 0.30 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.30 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Borealis Himod™ FT3280 LDPE for Film
Himod FT3280 is a tubular, low-density polyethylene grade for the production of packaging films. Compared to standard LDPE grades, the Himod products provide a combination of higher stiffness and i..
Melt Flow 0.30 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.30 g/10 min

@Load 4.76 lb,
Temperature 374 °F
Condition E; ASTM D1238
Formosa Plastics Formolene® HB4903 Blow Molding HDPE
Hexene CopolymerApplications: High performance blow molding applications, fuel tanks, seating, garbage cans, sheet, large industrial containers.Formolene HB4903 is a high performance copolymer that ..
Melt Flow 0.30 g/10 min

@Load 2.16 kg,
Temperature 230 °C
0.30 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Teknor Apex TEKRON® 4000-60 Thermoplastic Elastomer
Information provided by Teknor Apex Company
Melt Flow 0.30 g/10 min

@Load 2.16 kg,
Temperature 230 °C
0.30 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Borealis RA130E-6020 Polypropylene Random Copolymer
RA130E-6020 is a high molecular weight, low melt flow rate polypropylene random copolymer (PP-R) compound and is green colored. Applications: domestic water, heating, relining, plumbing, and indust..
Melt Flow 0.30 g/10 min

@Load 5.00 kg
0.30 g/10 min

@Load 11.0 lb
ISO 1133
Total Xsene® XS10 H HDPE, pipe, injection molding
FINATHENE® XS 10 H is a high density polyethylene based on C6 hexene as co-monomer and is produced by the Fina Double Loop Technology™. FINATHENE® XS 10 H is a high performance dark blue compound..
Melt Flow 0.30 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.30 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
ExxonMobil Enable™ 27-03HH Metallocene Polyethylene Resin
Product Description: Enable 23-05 resins are metallocene ethylene-hexane copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact ..
Melt Flow 0.30 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.30 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
ExxonMobil LDPE LD 317.09 Low Density Polyethylene Resin
Product Description: LD 317.09 resin is a fractional melt index, 6% vinyl acetate copolymer film resin. Film made from LD 317.09 offers excellent impact strength, tensile properties and heat sealabi..
Melt Flow 0.30 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.30 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
ExxonMobil Paxon™ AB50-003 Blow Molding Resin
Product Description: AB50-003 is a blow molding grade high density polyethylene copolymer. This resin has very good stress crack resistance combined with high impact strength and rigidity.Availabili..
Melt Flow 0.30 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.30 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM-D1238
Braskem TX9003 LDPE Blown Film Extrusion Polyethylene
TX9003 is a low-density polyethylene (LDPE) that presents excellent mechanical resistance, good optical properties, and high stiffness. These characteristics provide, in some applications, down gaug..
Melt Flow 0.30 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.30 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Bapolene® 2035 Polyethylene, Blow Molding Grade
Bapolene HD2035 is a high density polyethylene copolymer for blow molding applications. It is recommended for applications that require high top load strength and good ESCR properties. This produc..
Melt Flow 0.30 g/10 min

@Load 5.00 kg
0.30 g/10 min

@Load 11.0 lb
ISO 1133
Total Xsene® XS10 Orange YCF HDPE, pipe
FINATHENE® XS 10 ORANGE YCF is a high density polyethylene based on C6 hexene as co-monomer and is produced by the Fina Double Loop Technology™. FINATHENE® XS 10 ORANGE YCF is a high performance ..
Melt Flow 0.30 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.30 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
ExxonMobil Paxon™ AS55-003 Blow Molding Resin  (discontinued **)
AS55-003 is a blow molding grade high density polyethylene copolymer containing an antistat additive. It provides a good balance of stiffness and stress crack resistance.Information provided by Exx..
Melt Flow 0.30 g/10 min

@Load 5.00 kg
0.30 g/10 min

@Load 11.0 lb
ISO 1133
Total Xsene® XS10 YS HDPE, pipe
FINATHENE® XS 10 YS is a cadmium-free yellow stripe compound designed to be used in combination with the black PE 100 grade FINATHENE® XS 10 B for gas pipe application. The base polymer of FINATHE..