Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 55 g/10 min @Load 10.0 kg, Temperature 190 °C |
55 g/10 min @Load 22.0 lb, Temperature 374 °F |
ISO 1133 |
Multibase TPSiV® 4000-50A Thermoplastic Elastomer FEATURES & BENEFITS: Soft silky feel; Excellent abrasion and scratch resistance; Excellent bonding to PC, ABS; UV stableAPPLICATIONS: Solution for soft touch overmolding on consumer electronics, mob.. |
|||
Melt Flow | 55 g/10 min @Load 2.16 kg, Temperature 230 °C |
55 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
NCMT NanoPAC™ HS402 High Performance Polypropylene Nanocomposite Applications: Electrical AppliancesInformation provided by Nano Composite Materials Technology Limited |
|||
Melt Flow | 55 g/10 min @Load 1.20 kg, Temperature 300 °C |
55 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® HFD1930 PC Copolymer (Asia Pacific) 55 MFR LEXAN High Flow Ductile Copolymer, Natural color only |
|||
Melt Flow | 55 g/10 min @Load 1.20 kg, Temperature 300 °C |
55 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® HFD1930 PC Copolymer (Europe-Africa-Middle East) 55 MFR LEXAN High Flow Ductile Copolymer, Natural color only |
|||
Melt Flow | 55 g/10 min | 55 g/10 min | ASTM D1238 |
ExxonMobil Santoprene® 912BA Thermoplastic Elastomer
(discontinued **) A hard, black, super high-flow thermoplastic olefin (TPO) in the thermoplastic elastomer (TPE) family. This grade of Vistaflex TPE is temperature-dependent and can be processed on conventional therm.. |
|||
Melt Flow | 55 g/10 min @Load 1.20 kg, Temperature 300 °C |
55 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® HFD1910 PC Copolymer 55 MFR LEXAN High Flow Ductile Copolymer, Natural colors only |
|||
Melt Flow | 55 g/10 min @Load 1.20 kg, Temperature 300 °C |
55 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® HFD1910 PC Copolymer (Asia Pacific) 55 MFR LEXAN High Flow Ductile Copolymer, Natural colors only |
|||
Melt Flow | 55 g/10 min | 55 g/10 min | 55 cm<sup>3</sup>/10 min; Melt Volume Rate |
Huntsman IROGRAN® A 85 P 4394 FCM Ether-Based TPU-For Food Contact Extrusion grade; High microbial resistance, high transparencyInformation provided by Huntsman |
|||
Melt Flow | 55 g/10 min | 55 g/10 min | ASTM D1238 |
Hyosung Topilene J945 PP J945 Injection Impact CopolymerApplications: Very large articles:Washing M/C partsIndustrial applianceCharacteristics:High flowabilityHigh stiffnessInformation provided by Hyosung Corporation |
|||
Melt Flow | 55 g/10 min @Load 5.00 kg, Temperature 260 °C |
55 g/10 min @Load 11.0 lb, Temperature 500 °F |
Estimated using room temperature density; ISO 1133 |
Lanxess Durethan® DP 1852/30 000000 Nylon 6, 30% Glass Fiber PA 6, 30% glassfibers, UL V-0 at 0.75 mm (listed),GWIT:775°C at 0,75 mm, GWFI:960°C at 0.75 mm, CTI/A:400, good flowabilityApplication Examples: Hand-held barrel pump housings |
|||
Melt Flow | 55 g/10 min @Load 5.00 kg, Temperature 275 °C |
55 g/10 min @Load 11.0 lb, Temperature 527 °F |
ISO 1133 |
Gromax BFG30-BN00B2 Nylon 6 33% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Melt Flow | 55 g/10 min @Load 10.0 kg, Temperature 220 °C |
55 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Samsung Cheil Industries Infino® NH-1027HF PC/ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 55 g/10 min @Load 2.16 kg, Temperature 250 °C |
55 g/10 min @Load 4.76 lb, Temperature 482 °F |
ASTM D1238 |
Samsung Cheil Industries Infino® ASF-9810F PBT/PET, Mineral Filled General Purpose Material for automobile lamp with high flowInformation provided by Samsung Cheil Industries. |
|||
Melt Flow | 55 g/10 min @Load 2.16 kg, Temperature 250 °C |
55 g/10 min @Load 4.76 lb, Temperature 482 °F |
ASTM D1238 |
Samyang Tribit® 1550GN15 PBT Alloy, Reinforced Flame Retardancy Crystallization is fast, formability is excellent and thermal resistance, chemical resistance, electrical properties and abrasion resistance are excellent.1550GN15 is a reinforced, flame retardant (.. |
|||
Melt Flow | 55 g/10 min @Load 2.16 kg, Temperature 190 °C |
55 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
A. Schulman POLYBATCH™ White L8350 HSF Concentrate Based In High-Flow LLDPE DescriptionPOLYBATCH® L8350 HSF is a specialty white color concentrate containing 50% TiO2 based in high flow LLDPE. This products stearate free and has also been designed to offer excellent dispe.. |
|||
Melt Flow | 55 g/10 min @Load 2.16 kg, Temperature 190 °C |
55 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
A. Schulman POLYBATCH™ White L8350 HSF Concentrate Based In High-Flow LLDPE DescriptionPOLYBATCH® L8350 HSF is a specialty white color concentrate containing 50% TiO2 based in high flow LLDPE. This products stearate free and has also been designed to offer excellent dispe.. |
|||
Melt Flow | 55 g/10 min @Load 2.16 kg, Temperature 190 °C |
55 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
A. Schulman POLYBATCH™ White L8350 HSF Concentrate Based In High-Flow LLDPE DescriptionPOLYBATCH® L8350 HSF is a specialty white color concentrate containing 50% TiO2 based in high flow LLDPE. This products stearate free and has also been designed to offer excellent dispe.. |
|||
Melt Flow | 55 - 60 g/10 min @Load 10.0 kg, Temperature 220 °C |
55 - 60 g/10 min @Load 22.0 lb, Temperature 428 °F |
ISO 1133 |
Polyram RamShine PV527 Acrylonitrile Butadiene Styrene, Flame Retardant Flame retardant ABS for injection molding applications.Information provided by Polyram. |
|||
Melt Flow | 55 g/10 min @Temperature 230 °C |
55 g/10 min @Temperature 446 °F |
I<sub>2</sub>; ASTM D1238 |
Formosa Plastics Formolene® 3355E Random Copolymer Polypropylene Random Copolymer for Containers, Totes and Bins, and Closures Formolene® 3355E is a high melt flow random copolymer with fast cycle time and good mold and denesting release. It is designed for inje.. |
|||
Melt Flow | 55 g/10 min @Temperature 230 °C |
55 g/10 min @Temperature 446 °F |
I<sub>2</sub>; ASTM D1238 |
Formosa Plastics Formolene® 3355O Random Copolymer Polypropylene Random Copolymer for Clear Storage Containers and Food and Beverage Containers Formolene® 3355O is a high melt flow random copolymer with fast cycle time and easy mold release. It is designed for i.. |
|||
Melt Flow | 55 g/10 min @Load 2.16 kg, Temperature 230 °C |
55 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Total PPH 11012 Polypropylene Homopolymer, Injection Molding Polypropylene PPH 11012 is a nucleated controlled-rheology antistatic homopolymer with a high melt flow index of 55 g/10 min.Polypropylene PPH 11012 is characterized by high fluidity for high speed .. |
|||
Melt Flow | 55 g/10 min @Load 2.16 kg, Temperature 230 °C |
55 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Total PPC 12712 Polypropylene, Heterophasic Copolymer ATOFINA Propylene 12712 is a nucleated controlled-rheology heterophasic copolymer. PPC 12712 is characterized by good stiffness and impact resistance as well as low shrinkage and low warpage. It h.. |
|||
Melt Flow | 55 g/10 min | 55 g/10 min | |
Toyobo GLAMIDE® T-802 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Melt Flow | 55 g/10 min @Load 2.16 kg, Temperature 190 °C |
55 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
A. Schulman POLYBATCH™ White L8350 HSF Concentrate Based In High-Flow LLDPE DescriptionPOLYBATCH® L8350 HSF is a specialty white color concentrate containing 50% TiO2 based in high flow LLDPE. This products stearate free and has also been designed to offer excellent dispe.. |
|||
Melt Flow | 55 g/10 min @Load 2.16 kg |
55 g/10 min @Load 4.76 lb |
Melt flow ratio I10/I2 is 8. |
Dow LDPE 959I Low Density Polyethylene DOW LDPE 959I resin is a medium molecular weight distribution homo polymer designed to offer excellent clarity and flexibility with low warpage for lids. This resin has good processability over a wi.. |
|||
Melt Flow | 55 g/10 min @Load 2.16 kg, Temperature 230 °C |
55 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Carmel Olefins CAPILENE® W 77 AV Polypropylene Homopolymer CAPILENE® W 77 AV is a very high melt flow rate polypropylene homopolymer for injection molding with antistatic and nucleating additives. It offers a good balance of stiffness and flow, high de-mol.. |
|||
Melt Flow | 55 - 65 g/10 min | 55 - 65 g/10 min | ISO 1133 |
Beijing Ranger Chem BLUESTAR® 1084 PBT Can be used directly for spinning, and producing color concentrates. It can also be used for production after reinforcement & compounding.Information provided by Beijing Ranger Chemical Co. |
|||
Melt Flow | 55 g/10 min @Load 5.00 kg, Temperature 275 °C |
55 g/10 min @Load 11.0 lb, Temperature 527 °F |
ISO 1133 |
Azoty Tarnow™ Tarnamid® T-27 GF25 Polyamide 6 - Glass Fiber Reinforced 25% Glass fiber reinforced, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main properties:High.. |
|||
Melt Flow | 55 g/10 min @Load 2.16 kg, Temperature 190 °C |
55 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |