Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 4.3 g/10 min | 4.3 g/10 min | (Condition L) ASTM D-1238 |
Multibase Multi-Flex® TPE A 8502 EXCEL GREY Heating aging the material 1000 hours at 125°C leads to a +7% change in the tensile strength, +4% change in elongation, and +12% change in tear strength. Ash is 16%. Multi-Flex TPE contains Krato.. |
|||
Melt Flow | 4.3 g/10 min @Load 3.80 kg, Temperature 230 °C |
4.3 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D-1238 |
Plaskolite Optix® CA - 71 General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Melt Flow | 4.3 g/10 min | 4.3 g/10 min | Condition 230/2-8; ASTM D1238 |
Plaskolite Optix® CA-71 General Purpose Acrylic Resin Injection Molding and Extrusion Grade Pellets. High heat resistance, medium flow. |
|||
Melt Flow | 4.3 g/10 min @Load 3.80 kg, Temperature 230 °C |
4.3 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D-1238 |
Plaskolite Optix® CP - 71 General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Melt Flow | 4.3 g/10 min @Load 3.80 kg, Temperature 230 °C |
4.3 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D-1238 |
Plaskolite Optix® CP - 71 LL General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Melt Flow | 4.3 g/10 min @Load 3.80 kg, Temperature 230 °C |
4.3 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D-1238 |
Plaskolite West Optix® CP - 71 General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Melt Flow | 4.3 g/10 min @Load 3.80 kg, Temperature 230 °C |
4.3 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D-1238 |
Plaskolite West Optix® CP - 71 LL General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Melt Flow | 4.3 g/10 min | 4.3 g/10 min | Condition 230/2-8; ASTM D1238 |
Plaskolite West Optix® CA-71 General Purpose Acrylic Resin Injection Molding and Extrusion Grade Pellets. High heat resistance, medium flow. |
|||
Melt Flow | 4.3 g/10 min @Load 2.16 kg, Temperature 250 °C |
4.3 g/10 min @Load 4.76 lb, Temperature 482 °F |
cm³/10 min |
Polimeri Europa KOBLEND HI 41 F1 PBT+PC, Impact Grade
(discontinued **) Symbol according to ISO 1043/1: PBT+PC-HI Similar to KOBLEND HI 41 with improved fluidity. Main application fields: bumpers Unfilled. Suitable for Injection Molding. Supplied as pellets.ISO data.. |
|||
Melt Flow | 4.3 g/10 min @Load 1.20 kg, Temperature 300 °C |
4.3 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® 3412R PC (Asia Pacific) 20% GR, provides improved mechanical properties and UL94 V-1 rated at 0.058"". Internal mold release added. |
|||
Melt Flow | 4.3 g/10 min @Load 2.16 kg, Temperature 230 °C |
4.3 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Phillips 66 COPYLENE® CH043EW Polypropylene, Homopolymer, Slit Film, LWCO, Cordage COPYLENE™ CH043EW is a medium flow polypropylene homopolymer resin suitable for general injection molding or extrusion applications. Applications: Raffia/tapes/strapping. Equivalent to Pro-fax® HL.. |
|||
Melt Flow | 4.3 g/10 min @Load 2.16 kg, Temperature 230 °C |
4.3 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Phillips 66 COPYLENE® CH043L Polypropylene, Homopolymer, Lube, Straw COPYLENE™ CH043L is a high antistatic, medium flow polypropylene homopolymer resin, suitable for injection molding or extrusion applications. Applications: Housewares. Equivalent to Pro-fax® HL782.. |
|||
Melt Flow | 4.3 g/10 min | 4.3 g/10 min | ASTM D1238 |
SPS Guang Zhou POLLITEâ„¢ 1002G20 Flame-retarded/GF20%-Polycarbonate Characteristic: High mechanical properties, high rigidity, high heat resistant, good dimensional stability, good flame retardanceApplications: E/E parts, power tool, office suppliesInformation Provi.. |
|||
Melt Flow | 4.3 g/10 min @Load 10.0 kg, Temperature 220 °C |
4.3 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Samsung Cheil Industries Starex® ST-0185 ABS, Unreinforced Extrusion Grade Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 4.3 g/10 min @Load 10.0 kg, Temperature 220 °C |
4.3 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Samsung Cheil Industries Starex® QU-0191S ABS, Unreinforced Extrusion Grade Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 4.3 g/10 min @Load 10.0 kg, Temperature 220 °C |
4.3 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Samsung Cheil Industries Starex® ST-0185 ABS, Unreinforced Extrusion Grade Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 4.3 g/10 min @Load 5.00 kg, Temperature 200 °C |
4.3 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Supreme Petrochem SC 202EL General Purpose Polystyrene CharacteristicsHigh strength grade Excellent process ability Reduces processing cycle timeProcessing MoldingApplicationsAudio cassettes housing and covers, CD jewel boxes Medical products like disp.. |
|||
Melt Flow | 4.3 g/10 min @Load 2.16 kg, Temperature 235 °C |
4.3 g/10 min @Load 4.76 lb, Temperature 455 °F |
ASTM D1238R |
UBE UBESTA® 3030JI9L Plasticized Automotive Grade Nylon 12 Description: UBE UBESTA® Automotive grade Nylon 12Comments: meet DIN73378 PHLYInformation provided by UBE. |
|||
Melt Flow | 4.3 g/10 min @Load 2.16 kg, Temperature 190 °C |
4.3 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil LLDPE LL 3404.48 Linear Low Density Polyethylene Resin Product Description: LL 3404.48 is a hexane medium density polyethylene cast film grade for applications requiring high strength and high stiffness. Films produced from this resin exhibit good tensi.. |
|||
Melt Flow | 4.3 g/10 min @Temperature 230 °C |
4.3 g/10 min @Temperature 446 °F |
ASTM D1238 |
Dow 5E89 Polypropylene Resin DOW 5E89 is intended for use in stretched tape (raffia) processes, from which the raffia is used to produce woven fabrics for carpet backing, sacking, industrial and geotextile applications.Informat.. |
|||
Melt Flow | 4.3 g/10 min @Load 2.16 kg, Temperature 190 °C |
4.3 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Azoty Tarnow™ TARNOFORM 300 GF6 POM 30% glass fiber reinforced injection molding grade, suitable for applications where increased strength and stiffness is required.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A... |
|||
Melt Flow | 4.3 g/10 min | 4.3 g/10 min | ASTM D1238 |
ExxonMobil LL 3404.48 Cast Film Resin
(discontinued **) LL 3404.48 is a hexene medium density polyethylene cast film grade for applications requiring high strength and high stiffness. It can also be used in blown films. Films produced from this resin ex.. |
|||
Melt Flow | 4.3 g/10 min @Load 2.16 kg, Temperature 190 °C |
4.3 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
DuPont™ Surlyn® 1802 Sodium Ionomer Resin for Blown/Cast Film and Extrusion Coating Surlyn® 1802 is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment and extrusion coating and coextrusion coating equipment designed to proces.. |
|||
Melt Flow | 4.3 g/10 min | 4.3 g/10 min | Condition G |
Ineos Nova 5120 High Impact Polystyrene
(discontinued **) Good balance of toughness and rigidity, Superior gloss, USP Class VIApplications: Refrigeration, Appliances, High gloss applicationsProperties were determined on injection molded specimens at 23°C .. |
|||
Melt Flow | 4.3 g/10 min | 4.3 g/10 min | Condition G |
Ineos Nova 5124 High Impact Polystyrene
(discontinued **) Good balance of toughness and rigidity, Superior gloss, USP Class VIApplications: Refrigeration, Appliances, High gloss applicationsProperties were determined on injection molded specimens at 23°C .. |
|||
Melt Flow | 4.3 g/10 min @Load 1.20 kg, Temperature 300 °C |
4.3 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® 3412R PC 20% GR, provides improved mechanical properties and UL94 V-1 rated at 0.058"". Internal mold release added. |
|||
Melt Flow | 4.3 g/10 min @Load 2.16 kg, Temperature 230 °C |
4.3 g/10 min @Load 4.76 lb, Temperature 446 °F |
|
BASF Novolen® 1104 K Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Melt Flow | 4.3 g/10 min @Load 2.16 kg, Temperature 190 °C |
4.3 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
DuPont Bynel® 3859 Anhydride-Modified Ethylene Vinyl Acetate Adhesive Resin
(discontinued **) Bynel® Series 3800 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p.. |