Physical Properties Metric English Comments
Melt Flow 39 g/10 min
39 g/10 min
(Condition L) ASTM D-1238
Multibase Multi-Flex® TPE A 7321 BLK
Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
Melt Flow 39 g/10 min

@Load 1.20 kg,
Temperature 300 °C
39 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
SABIC Innovative Plastics Lexan® HP1HF PC
Very high flow, biocompatible polycarbonate for healthcare applications. EtO sterilizable.
Melt Flow 39 g/10 min

@Load 1.20 kg,
Temperature 300 °C
39 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
SABIC Innovative Plastics Lexan® HP1HF PC (Europe-Africa-Middle East)
Very high flow, biocompatible polycarbonate for healthcare applications. EtO sterilizable.
Melt Flow 39 g/10 min

@Load 1.20 kg,
Temperature 300 °C
39 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
SABIC Innovative Plastics Lexan® ML3729 PC
Excellent flow, UV stabilized, grade which contains a release agent to ensure easy processing.
Melt Flow 39 g/10 min

@Load 1.20 kg,
Temperature 300 °C
39 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
SABIC Innovative Plastics Lexan® HP1HF PC (Asia Pacific)
Very high flow, biocompatible polycarbonate for healthcare applications. EtO sterilizable.
Melt Flow 39 - 47 g/10 min

@Load 2.16 kg,
Temperature 190 °C
39 - 47 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238-00
Ipiranga Petrochem PRB 4215 Polypropylene
The production of polypropylene (PP) employs Spheripol technology from Montell / Italy. This technology has been acclaimed all over the world and is known as clean technology, because it does not pr..
Melt Flow 39 g/10 min

@Load 2.16 kg,
Temperature 250 °C
39 g/10 min

@Load 4.76 lb,
Temperature 482 °F
ASTM D1238
SABIC Innovative Plastics Valox® SHF434HR PBT
PBT, Super High Flow, 20% glass reinforced,hydrolytically resistant.
Melt Flow 39 g/10 min

@Load 5.00 kg,
Temperature 280 °C
39 g/10 min

@Load 11.0 lb,
Temperature 536 °F
ASTM D 1238
SABIC Innovative Plastics Noryl GTX GTX8430W PPE+PA
30% Glass Reinforced PPE+PA Alloy. Typically used for automotive connectors.This data was supplied by SABIC-IP for the Americas region.
Melt Flow 39 g/10 min

@Load 8.70 kg,
Temperature 190 °C
39 g/10 min

@Load 19.2 lb,
Temperature 374 °F
ASTM D1238
Lubrizol Estane® 2103-80PF Thermoplastic Polyurethane Elastomer
Formerly PellethaneFeature: Film and profile resinAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in..
Melt Flow 39 g/10 min

@Load 2.16 kg,
Temperature 230 °C
39 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
ExxonMobil Exxtral™ BMV 208 Performance Polyolefin
Product Description: Polyolefin injection molding compound with very high flow, high stiffness, good low temperature impact resistance, and excellent processability for automotive exterior trim appl..
Melt Flow 39 g/10 min
39 g/10 min
ISO 1133 D
Asahi Kasei Tenac® 7054 Homopolymer Acetal Resin
High-flow grade with high crystallization rate for higher productivity.Information provided by Asahi Kasei Corporation.
Melt Flow 39 g/10 min

@Load 2.16 kg,
Temperature 275 °C
39 g/10 min

@Load 4.76 lb,
Temperature 527 °F
ISO 1133
BASF Ultradur S 4090 G4 LS High Speed BK15077 20% Glass Filled PBT
Melt Flow 39 g/10 min

@Load 2.16 kg,
Temperature 250 °C
39 g/10 min

@Load 4.76 lb,
Temperature 482 °F
Calculated from Volume Flow Rate of 30 cm<sup>3</sup>/10min.; ISO 1133
DSM Arnite® T06 202 XL (T-X01151) PBT (European Grade)
Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame ..