Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 2.2 g/10 min | 2.2 g/10 min | (Condition L) ASTM D-1238-94a |
Multibase Multi-Pro® 0001 Black Polypropylene This product was specially designed for one customer's extrusion application needs. Data is taken from sample material only.Data provided by Multibase. |
|||
Melt Flow | 2.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Polimeri Europa Riblene® FL 24 Low Density Polyethylene - Blown Film Extrusion Riblene FL 24 is a low density polyethylene (LDPE) with added slip and antiblocking agents, suitable for blown film extrusion. Riblene FL 24 is characterized by a good balance between processabilit.. |
|||
Melt Flow | 2.2 g/10 min @Load 2.16 kg, Temperature 250 °C |
2.2 g/10 min @Load 4.76 lb, Temperature 482 °F |
cm³/10 min |
Polimeri Europa KOBLEND HI PD 19 PBT+PC, Impact Grade
(discontinued **) Symbol according to ISO 1043/1: PBT+PC-HI Elastomer modified PBT+PC blend with a very good impact behaviour, good stiffness and higher thermal properties than KOBLEND HI 18. Main application field.. |
|||
Melt Flow | 2.2 g/10 min | 2.2 g/10 min | ASTM D1238 |
Huntsman Rexell® M3104 Blown Film Extrusion LLDPE
(discontinued **) Linear-low medium density copolymer, cast film extrusion, FDA compliant.Features: Excellent combination of toughness, stiffness, and optics with good temperature resistance.Applications: Diaper film.. |
|||
Melt Flow | 2.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
NOVA Chemicals Novapol® LF-0222-A LDPE Wire and Cable Resin
(discontinued **) NOVA Chemicals NOVAPOL® LF-0222-A is a medium molecular weight low density polyethylene. Resin consistency and purity are very high which make it suitable as a base resin in Wire and Cable applicat.. |
|||
Melt Flow | 2.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
NOVA Chemicals Novapol® LF-0225-B LDPE Clarity Film Resin
(discontinued **) Features: High optical clarityExcellent processability Applications: Produce and bakery filmLinersTextile packaging filmGeneral packaging requiring high clarity filmInformation provided by Nova Chem.. |
|||
Melt Flow | 2.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
DuPont Bynel® 39E622 Adhesive Resin
(discontinued **) Bynel® Series 3900 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p.. |
|||
Melt Flow | 2.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Iran Petrochemical (PCC) 09X02 Linear Low Density Polyethylene 09X02 is a high performance LLDPE (HP-LLDPE) cast film grade combines ease of processing with low gels and good film strength. Its excellent stretchability makes this grade particularly suited for s.. |
|||
Melt Flow | 2.2 g/10 min | 2.2 g/10 min | ISO 1133 |
Lucite International Elvakon® 4494 Low Gloss Acrylic Capstock Coextrusion grade developed to provide high aesthetic control, outstanding weatherability and impact and scratch resistance, the Elvakon® series enables protection of substrates with a durable pr.. |
|||
Melt Flow | 2.2 g/10 min @Load 2.16 kg |
2.2 g/10 min @Load 4.76 lb |
ISO 1133 |
SIDPEC EGYPTENE® LL 0220 KJ LLDPE Film Applications: Light and medium duty film.Film properties were measured on 38 micron film extruded at a blow up ratio of 2:1.Information provided by Interchim s.r.l., official distributor of Sidi Ke.. |
|||
Melt Flow | 2.2 g/10 min @Load 5.00 kg, Temperature 190 °C |
2.2 g/10 min @Load 11.0 lb, Temperature 374 °F |
ISO 1133/ASTM D1238 |
Silon Taborex TA 1133 HD Chemically-Crosslinkable HDPE Compound TABOREX TA 1133 HD is a crosslinkable compound made of Silane grafted ethylene polymer. This graft polymer constitutes together with a Masterbatch containing the crosslinking catalyst a “SIOPLA.. |
|||
Melt Flow | 2.2 g/10 min @Load 3.80 kg, Temperature 230 °C |
2.2 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM Data |
Styron Magnum™ 941 ABS MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Melt Flow | 2.2 g/10 min @Load 3.80 kg, Temperature 230 °C |
2.2 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM Data |
Styron Magnum™ 1040 ABS, Very High impact MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Melt Flow | 2.2 g/10 min @Load 2.16 kg, Temperature 230 °C |
2.2 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Borealis HB601WG Polypropylene Homopolymer HB601WG is a polypropylene homopolymer intended for injection molding and blow molding. The product is available in natural but other colors can be provided on request. This material has excellent .. |
|||
Melt Flow | 2.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Westlake EF606 Low Density Polyethylene Westlake EF606 is a LDPE resin suggested for use in multiwall and general purpose liners, and for use as a blend resin in general purpose packaging applications. It has excellent processability, and.. |
|||
Melt Flow | 2.2 g/10 min | 2.2 g/10 min | ASTM D1238 |
ExxonMobil Exact™ 4151 Ethylene-based Plastomer Resin Product Description: Exact 4151 is an ethylene-based hexane plastomer produced using ExxonMobil Chemical’s EXXPOL® Catalyst Technology. Exact 4151 is designed for both monolayer and multilayer coe.. |
|||
Melt Flow | 2.2 g/10 min | 2.2 g/10 min | ExxonMobil Method |
ExxonMobil EXACT™ 4151 Plastomer for Cast Film Product Description: Exact 4151 is an ethylene-based hexane plastomer produced using ExxonMobil Chemical’s EXXPOL® Catalyst Technology. Exact 4151 is designed for both monolayer multilayer coextru.. |
|||
Melt Flow | 2.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
DuPont Performance Polymers Delrin® 100TL NC010 Acetal (POM)
(Unverified Data**) Teflon® Lubricated High Viscosity Acetal Homopolymer with Low Wear and Low FrictionDelrin 100TL NC010 (formerly Delrin 100TL NC000) is a high viscosity acetal homopolymer with 1.5% TeflonInformatio.. |
|||
Melt Flow | 2.2 g/10 min @Load 10.0 kg, Temperature 220 °C |
2.2 g/10 min @Load 22.0 lb, Temperature 428 °F |
Melt Volume Rate (ml/10 min); ISO 1133 |
Chi Mei Polyrex® PG-383 Polystyrene High heat; high strength |
|||
Melt Flow | 2.2 g/10 min | 2.2 g/10 min | Condition D; ASTM D 1238 |
CPT C-Flex® R70-214 Opaque Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
Melt Flow | 2.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238, ISO 1133 |
DuPont™ Bynel® 41E766 Anhydride Modified LLDPE BYNEL® Series 4100 series resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All BYNEL Series 4100 series resins are available in pellet form for use in conventional ext.. |
|||
Melt Flow | 2.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
DuPont Performance Polymers Delrin® FG100TL NC010 Acetal (POM)
(Unverified Data**) Teflon® Lubricated High Viscosity Acetal Homopolymer with Low Wear and Low Friction Developed for Food Contact Applications Delrin 100TL is a high viscosity acetal homopolymer containing 1.5% Teflo.. |
|||
Melt Flow | 2.2 g/10 min @Load 2.16 kg, Temperature 235 °C |
2.2 g/10 min @Load 4.76 lb, Temperature 455 °F |
|
Arkema Group Rilsan® BZM 23 G9 Nylon 11, 23% Glass Fiber Filled (Conditioned) Designation ISO 1874-PA11,MS,18-040,(G+C)(F+D)(25+05)Rigid grade with glass fiber (23%) and graphite filler for injection molding. Available color: steel black gray. Additive free.Rigidity. Low fric.. |
|||
Melt Flow | 2.2 g/10 min @Load 2.16 kg, Temperature 235 °C |
2.2 g/10 min @Load 4.76 lb, Temperature 455 °F |
|
Arkema Group Rilsan® AZM 30 GT8LD Nylon 12, 30% Glass Fiber Filled (Dry) Designation ISO 1874-PA12,MHLS,16-050,(G+C)(F+D)(30+05)Rigid grade with glass fiber (30%) and graphite filler for injection molding. Available color: steel black gray. Reinforced light and heat stab.. |
|||
Melt Flow | 2.2 g/10 min | 2.2 g/10 min | ASTM D1238 |
Aclo Accucomp ABS ABS803L Medium Impact Grade |
|||
Melt Flow | 2.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Radici Heraform® R 350 Acetal Copolymer Standard grade for injection molding of thick wall parts, stiff-flowing, extrusion grade for tubes and sheet.Information provided by Radici group. |
|||
Melt Flow | 2.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil Exceed™ 2227ED Metallocene Polyethylene Resin (European Grade) Product Description: Exceed 2227ED is a metallocene ethylene-hexene copolymer. It offers an excellent balance of high modulus and impact strength. The higher melt index makes it ideally suited for L.. |
|||
Melt Flow | 2.2 g/10 min | 2.2 g/10 min | Exxon Method |
ExxonMobil Escorene® LD-316 EVA Film Resin, High Clarity, High Impact
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 1.9% vinyl acetate copolymer, high clarity film resin. Film made from LD-316 offers improved impact strength and heat sealability versus homopoly.. |