Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 12 g/10 min @Load 2.16 kg, Temperature 230 °C |
12 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
RheTech Products FT2700-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Air deflectorsFuel filler shieldsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Melt Flow | 12 g/10 min @Load 2.16 kg, Temperature 230 °C |
12 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Phillips 66 COPYLENE® CR120LN Polypropylene, Random Copolymer, Nucleated COPYLENE™ CR120LN is a random copolymer nucleated and with antistat for good mold release in injection molding applications. Applications: Containers, Closures, HousewaresInformation provided by P.. |
|||
Melt Flow | 12 g/10 min | 12 g/10 min | ASTM D1238 |
Plaskolite West Optix® CA-927 G HF Clear Impact Modified Acrylic Resin Impact modified acrylic resin, injection molding gradeApplications: A high flow, impact-modified acrylic resin designed for medical or food uses. This resin offers impact strengths up to seven time.. |
|||
Melt Flow | 12 g/10 min @Load 2.16 kg, Temperature 230 °C |
12 g/10 min @Load 4.76 lb, Temperature 446 °F |
STN EN ISO 1133 |
Plastcom SLOVAMID 6 GF 10 FRG 5 Polyamide 6, 10% Glass Fiber, Flame Retardant FeaturesPA 6 for injection moulding, chemically strengthened with 10% glass fiber. Application: impacted mouldings with high strength applied in automotive, electrical, engineering and consumer-goo.. |
|||
Melt Flow | 12 - 18 g/10 min | 12 - 18 g/10 min | ASTM D1238-92 |
Iran Petrochemical (PCC) Tabriz 3630/1 High Impact Polystyrene
(discontinued **) Information provided by Iran Petrochemical Commercial Co. |
|||
Melt Flow | 12 g/10 min @Load 5.00 kg, Temperature 200 °C |
12 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
M. Holland Company GS410WC Polystyrene
(discontinued **) Features: High Clarity, High FlowUses: Household Goods, LabwareApprovals: FDA 21 CFR 177.1640 Processing Method: Injection MoldingInformation provided by M. Holland. |
|||
Melt Flow | 12 g/10 min @Load 1.20 kg, Temperature 300 °C |
12 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
PTS Tristar® PC-10FRNH 12 MFI Non-Bromine Non-Chlorine Flame Retardant Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Melt Flow | 12 g/10 min @Load 2.16 kg, Temperature 380 °C |
12 g/10 min @Load 4.76 lb, Temperature 716 °F |
ASTM D1238 |
Solvay Specialty Polymers Radel® R-7120 Polyphenylsulfone, 20% glass fiber
(discontinued **) RADEL R 7120 is a 20% glass fiber reinforced grade of RADEL R polyphenylsulfone developed specifically for aircraft interior applications. The product complies with the FAA regulation 14CFR Part 25 .. |
|||
Melt Flow | 12 g/10 min @Temperature 190 °C |
12 g/10 min @Temperature 374 °F |
ASTM D1238 |
Kolon KOPEL® KP3340 General Purpose TPE Resin KOPEL® is a thermoplastic polyester elastomer which is a new engineering rubber having combined properties of conventional rubber and thermoplastic. Its flexibility and elastic recovery are very.. |
|||
Melt Flow | 12 g/10 min @Load 1.20 kg, Temperature 300 °C |
12 g/10 min @Load 2.65 lb, Temperature 572 °F |
Calculated from Volume Flow Rate of 10 cm<sup>3</sup>/10min.; ISO 1133 |
Mitsubishi Xantar® F 22 R Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Melt Flow | 12 g/10 min @Load 2.16 kg, Temperature 230 °C |
12 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Multibase Multi-Flamâ„¢ 0112 PP NH Polypropylene Features:Flame RetardantHalogen Content, Low to None Forms:PelletsProcessing Methods:Injection MoldingExtrusionUses:TubingPipingFurnitureInformation provided by Multibase |
|||
Melt Flow | 12 g/10 min @Load 10.0 kg, Temperature 250 °C |
12 g/10 min @Load 22.0 lb, Temperature 482 °F |
ASTM D1238 |
Samsung Cheil Industries Infino® LS-3302 PC, 30% Glass Filled High Impact High-impact resistant PC/GF with 30% GF reinforcement for camera body tubeInformation provided by Samsung Cheil Industries. |
|||
Melt Flow | 12 g/10 min @Load 5.00 kg, Temperature 200 °C |
12 g/10 min @Load 11.0 lb, Temperature 392 °F |
ISO 1133 |
Styrolution PS 124 N/L GPPS Styrolution PS 124N/L is a general purpose polystyrene grade with a good flow characteristic and an improved heat resistance.Excellent flow propertiesHigh heat resistanceUL 94 HB (Antwerp only)Infor.. |
|||
Melt Flow | 12 g/10 min @Load 10.0 kg, Temperature 220 °C |
12 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Techmer ES Plastiblend® ABS IM Availability: North AmericaForms: PelletsFeatures: High Heat ResistanceInformation provided by TP Composites, Inc. |
|||
Melt Flow | 12 g/10 min @Load 2.16 kg, Temperature 190 °C |
12 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
A. Schulman POLYBATCH™ Grey 8760 Concentrate Based In Polyethylene DescriptionPOLYBATCH® 8760 is a grey color concentrate based in polyethylene. This concentrate was designed to provide opacity and color in polyolefin film and molding applications. POLYBATCH® 8.. |
|||
Melt Flow | 12 g/10 min @Load 2.16 kg, Temperature 190 °C |
12 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 - ISO 1133 |
DuPont Elvaloy® PTW Ethylene/N-Butyl Acrylate/Glycidyl Methacrylate Copolymer Specialized copolymers deliver flexibility, toughness and weatherability to adhesives, plastics, highways and roofing.Availability: GloballyInformation provided by DuPont. |
|||
Melt Flow | 12 g/10 min | 12 g/10 min | ASTM D1238 |
A. Schulman PP 1632-01 Polypropylene Random Copolymer DescriptionPolypropylene PP 1632-01 is a polypropylene random copolymer produced utilizing unique catalyst and processing technology. It was designed for injection molding and stretch blow molding .. |
|||
Melt Flow | 12 - 16 g/10 min | 12 - 16 g/10 min | Cond L; ASTM D1238 |
Washington Penn PPH4CF2.5 Polypropylene, 25% Calcium Carbonate Filled UV Stabilized; Injection molding grade.Applications: High flow for thin wall parts requiring long-flow. Outdoor furniture.Data provided by Washington Penn Plastic Co., Inc. |
|||
Melt Flow | 12 g/10 min @Load 2.16 kg, Temperature 190 °C |
12 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
A. Schulman POLYBATCH™ Grey 8760 Concentrate Based In Polyethylene DescriptionPOLYBATCH® 8760 is a grey color concentrate based in polyethylene. This concentrate was designed to provide opacity and color in polyolefin film and molding applications. POLYBATCH® 8.. |
|||
Melt Flow | 12 g/10 min @Load 5.00 kg, Temperature 260 °C |
12 g/10 min @Load 11.0 lb, Temperature 500 °F |
ISO 1133 |
Covestro Makroblend® KU 2-7609 Polycarbonate + PBT, Mineral Filled Impact Grade ISO 7792-1-PC/PBT,MHPR,-030,MD20(PC+PBT)-blendsimpact modifiedInjection molding grade20% mineral filledPreprocessingMax. Water content |
|||
Melt Flow | 12 g/10 min @Load 1.20 kg, Temperature 300 °C |
12 g/10 min @Load 2.65 lb, Temperature 572 °F |
ISO 1133 |
Covestro Makrolon® T7855 Polycarbonate, Impact Grade ISO 7391-PC,MPR,(,,)-18-9Global gradeMVR (300 °C/1.2 kg) 12 cm3/10 minImpact modifiedMedium viscosityEasy releaseInjection molding - Melt temperature 280 - 320 °CAvailable in opaque colors onlyPre.. |
|||
Melt Flow | 12 g/10 min @Load 2.16 kg, Temperature 190 °C |
12 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil LD 202.48 Extrusion Coating Resin Product Description: LD 202.48 is an LDPE coating grade, especially designed for high speed, lightweight extrusion coating applications providing: -high speed processability – good heat sealing pro.. |
|||
Melt Flow | 12 g/10 min @Load 2.16 kg, Temperature 190 °C |
12 g/10 min @Load 4.76 lb, Temperature 374 °F |
cm³/10min; ISO 1133 |
DuPont Performance Polymers Delrin® 510GR NC000 Acetal (POM)
(Unverified Data**) 10% Glass Reinforced Medium Viscosity Acetal Homopolymer Delrin 510GR is a 10% glass reinforced acetal homopolymer for injection molding. It has high strength stiffness and high deflection temperatu.. |
|||
Melt Flow | 12 g/10 min @Load 2.16 kg, Temperature 230 °C |
12 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
ExxonMobil PP9574E6 Polypropylene Homopolymer Product Description: A highly clarified random copolymer resin designed for general purpose injection molding applications requiring resistance to build up of static electricity.Availability: North.. |
|||
Melt Flow | 12 g/10 min @Load 5.00 kg, Temperature 200 °C |
12 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Aaron Industries AAROLENE® ARPS 100-1 GPPS BLACK Polystyrene Compounded Resin AAROLENE® ARPS 100 Series Polystyrene Compounded ResinFeatures: A reprocessed, general-purpose Polystyrene resin, compounded black, specifically designed for all high speed injection molding appli.. |
|||
Melt Flow | 12 g/10 min | 12 g/10 min | ASTM D1238 |
Aclo Accutech Polypropylene Copolymer CP0436T20L Talc Reinforced |
|||
Melt Flow | 12 g/10 min @Load 2.16 kg, Temperature 190 °C |
12 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
A. Schulman POLYBATCH™ Grey 8368 Concentrate Based In Polyethylene DescriptionPOLYBATCH® 8368 is a grey color concentrate based in polyethylene. This concentrate was designed to provide opacity and color in polyolefin film and molding applications. POLYBATCH® 8.. |
|||
Melt Flow | 12 - 20 g/10 min | 12 - 20 g/10 min | ASTM D1238 |
A. Schulman POLYFORT™ FPP 1200H High Flow, Calcium Carbonate Fortified Homopolymer Polypropylene DescriptionPolyfort® FPP 1200H is a high flow 40% calcium carbonate fortified homopolymer polypropylene.Information provided by A. Schulman. |